Daxun is an experienced manufacturer of CP-1 grade titanium tubes
As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
- Titanium tube Grade:CP-1(Grade 1)- UNS R50250
- Titanium tube types: Seamless Ti tube, Ti welded tube, forged Ti tube
- Titanium tube density The density of grade 1 titanium is 4.51 g/cm3
- Standards: ASTM B861、B862、B338 / ASME SB861、SB862、SB338
- Softest Ti,High ductility, Very corrosion resistant, good cold formability
————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!
A global leader in commercially pure titanium tube fabrication services
Commercially Pure Titanium Grade 1 Tube is one of the softest and most ductile types with excellent formability. Grade 1 Titanium Tube is primarily used in the maritime and chemical industries where parts are exposed to extremely harsh conditions. The ultimate tensile strength of SB 338 Gr 1 Tube is 35 KSI min (240 MPa min), while the yield strength (0.2% variation) of Cp Grade 1 Tube is 25 – 45 KSI (170 – 310 MPa). Ti Cp Grade 1 Seamless Tube is also known as TA1, Titan Grade 1, and Gr 1. Grade 1 Titanium Tube is a non-alloyed, low-strength titanium tube product with low oxygen concentration and excellent formability; it is used in the chemical industry, heat exchangers, and desalination facilities.
Grade 1 Titanium Tube is also well suited for manufacturing exhaust systems, charge air pipes, and water pipes. We offer Titanium Tube with a thickness equivalent to 1.2 mm and diameters ranging from 51 mm to 102 mm (the most common exhaust system sizes). Therefore, these tubes are more stable and stronger even at higher exhaust gas temperatures.
Daxun certifies and tests titanium alloy tubes according to ASME SB/ASTM, B861 and B862, including hardness testing, hydrostatic testing, eddy current testing, ultrasonic defect identification, tensile testing, flattening, expansion testing, annealing, tempering, stress relief, etc.
Titanium Grade 1 Tube, Titanium UNS R50250 Tube, Titanium Alloy DIN 3.7025 Seamless Tube, Titanium Alloy Grade 1 Tube, Titanium Grade 1 Seamless Tube, Titanium UNS R50250 Seamless Tube, Titanium Alloy Grade 1 Tube, Titanium Tube Suppliers, Welded Titanium Tubes, Titanium Tubes for Sale, Titanium Seamless Tubes, Titanium Tube Suppliers, Titanium Werkstoff Nr. 3.7025 Tube, Titanium UNS R50250 Seamless Tube, Titanium Alloy R50250 Tube, Titanium R50250 Welded Tube, Titanium Gr1 Tube, Titanium Alloy DIN 3.7025 Welded Tube, Titanium Gr.1 Tube Suppliers in China.
Are you looking to purchase titanium tubes for your project or order a range of tubes? Daxun produces a wide range of titanium tubes including Grade 1 (3.7025), Grade 2 (3.7035), Grade 3 (3.7055), Grade 7 (3.7235), Grade 9 (3.7195) and Grade 12 (3.7105).
Buy titanium tubes at Daxun Alloys.
We offer a wide range of sizes starting from 1.0 mm in diameter with multiple variations, available directly from stock or custom made to your specifications through our network. We have wrought titanium tubes, seamless titanium tubes and longitudinally welded titanium tubes immediately available from stock for a wide range of applications.
We offer heat exchanger tubing in standard specifications such as ASTM B 338, ASME SB 338, DIN 17866 and VD TÜV welded titanium tubes or seamless titanium tubes. When it comes to titanium tubes, we have a large supply of titanium welded tubes and titanium seamless tubes in China in standard sizes up to 100 mm thick. We will supply welded titanium tubes for larger pipe sizes. The most common specifications used in the industry are ASTM B 861, ASFM B 862, NACE and NORSOK and VD TÜV Tube 230/2, depending on the specifications of the plant designer.
Titanium tube surface treatment options include bright annealing, pickling and grinding. Material parameters vary depending on the application and product requirements. The corrosion and mechanical properties of titanium alloy tubes vary. We are happy to assist you in evaluating your needs. If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee price and quantity for a specified period.
البيانات
- المعلمة
- المكونات
- الخواص الميكانيكية
- Hot searches
| Grade 1 Titanium pipe & Tubes Specification | ASTM B338 / ASTM B861 / ASTM B862 / ASME SB338 / ASME SB861 / ASME SB862 |
| Grade 1 Titanium pipe & Tubes Grades | Commercially pure titanium Grade 1- TA1- USN 50250 |
| Grade 1 Titanium pipe & Tubes Type | ot Rolled / Cold Drawn / Welded / ERW |
| Grade 1 Titanium pipe & Tubes Outer Diameter Size | Titanium seamless pipe – φ1.0mm to φ508.3mm |
| Titanium welded pipe – φ6.0mm to φ1219mm | |
| Grade 1 Titanium pipe & Tubes Wall Thickness | 0.3mm—50mm (customizable wall thickness) |
| Grade 1 Titanium pipe & Tubes Length | 5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size. |
| Titanium pipe Form | ‘ Hollow, U’ bent, LSAW, Hydraulic, Straight Tube, Boiler, Round, Tube Coil, Square, Rectangular Etc |
| Marking | All Titanium Tubes Tubing are marked as follows: Grade, Standard, Thickness, OD, Heat No., Length (Or according to the customer’s request.) |
| Uses of Titanium Alloy Tubes | Gas pipes, oil pipes, heat exchanger tubes, boiler tubes, fluid pipes, titanium exhaust pipes. |
| Grade 1 Titanium pipe & Tubes Pipe Ends | Plain Ends / Beveled Ends |
| Grade 1 Titanium pipe & Tubes Delivery Conditions | As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
| Grade 1 Titanium pipe & Tubes Coating | Electropolish, Mechanical Polish, Satin Finish, Passivated |
| Grade 1 Titanium pipe & Tubes Other Testing | ardness Test, Hydrostatic Test, Eddy Current test, Eddy Current, Tensile Test, Flattening, Flare Test, Annealed, Hydrostatic Test, Tempered, Stress Relieved etc. |
| Grade 1 Titanium pipe & Tubes Dimension | All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME |
| Grade 1 Titanium pipe & Tubes Value Added Services | Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
| Grade 1 Titanium pipe & Tubes Packaging | Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
| Grade 1 Titanium pipe & Tubes Shipment & Transportation | By Road – Truck / Train, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes |
| Grade 1 Titanium pipe & Tubes Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS ETC |
| العنصر | Minimum (weight %) | Maximum (weight %) | Typical (weight %) |
| في | 0.2 | ||
| O | 0.18 | ||
| C | 0.08 | ||
| N | 0.03 | ||
| H | 0.015 | ||
| تي | الرصيد |
| الخصائص الفيزيائية | Metric | English | Comments |
| الكثافة | 4.50 g/cc | 0.163 lb/in³ | |
| a Lattice Constant | 2.95 Å @Temperature 25.0 °C | 2.95 Å @Temperature 77.0 °F | alpha phase |
| 3.29 Å @Temperature 900 °C | 3.29 Å @Temperature 1650 °F | beta phase | |
| c Lattice Constant | 4.683 Å | 4.683 Å @Temperature 77.0 °F | c/a = 1.587 |
| Chemical Properties | Metric | English | Comments |
| Thermal Neutron Cross Section | 5.6 barns/atom | 5.6 barns/atom | Average for naturally occurring Ti |
| الخواص الميكانيكية | Metric | English | Comments |
| Hardness, Brinell | 120 | 120 | annealed |
| Hardness, Knoop | 132 | 132 | Estimated from Brinell. |
| Hardness, Rockwell B | 70 | 70 | annealed |
| Hardness, Vickers | 122 | 122 | Estimated from Brinell. |
| قوة الشد | 124 – 138 MPa @Temperature 427 °C | 18000 – 20000 psi @Temperature 801 °F | |
| 152 – 179 MPa @Temperature 316 °C | 22000 – 26000 psi @Temperature 601 °F | ||
| 193 – 207 MPa @Temperature 204 °C | 28000 – 30000 psi @Temperature 399 °F | ||
| Tensile Strength, Ultimate | 240 MPa | 34800 psi | |
| Tensile Strength, Yield | 170 – 310 MPa | 24700 – 45000 psi | |
| 76.0 – 90.0 MPa @Temperature 427 °C | 11000 – 13100 psi @Temperature 801 °F | 0.2% offset | |
| 83.0 – 103 MPa @Temperature 316 °C | 12000 – 14900 psi @Temperature 601 °F | 0.2% offset | |
| 110 – 124 MPa @Temperature 204 °C | 16000 – 18000 psi @Temperature 399 °F | 0.2% offset | |
| Elongation at Break | 24% | 24% | |
| 25 – 30 % @Temperature 427 °C | 25 – 30 % @Temperature 801 °F | ||
| 30 – 35 % @Temperature 316 °C | 30 – 35 % @Temperature 601 °F | ||
| 40 – 50 % @Temperature 204 °C | 40 – 50 % @Temperature 399 °F | ||
| Reduction of Area | 35% | 35% | |
| Tensile Modulus | 103 GPa | 14900 ksi | |
| Compressive Modulus | 110 GPa | 16000 ksi | |
| Poissons Ratio | 0.37 | 0.37 | |
| Shear Modulus | 45.0 GPa | 6530 ksi | |
| Charpy Impact | 310 J | 229 ft-lb | V-notch |
| Impact Test | 136 J | 100 ft-lb | Impact Strength |
| Coefficient of Friction, Dynamic | 0.68 | 0.68 | Ti sliding on Ti; 300 m/min |
| 0.8 | 0.8 | Ti sliding on Ti; 40 m/min | |
| Electrical Properties | Metric | English | Comments |
| المقاوماتية الكهربائية | 0.0000420 ohm-cm | 0.0000420 ohm-cm | |
| Magnetic Permeability | 1.00005 | 1.00005 | at 1.6 kA/m |
| Magnetic Susceptibility | 3.98E-08 | 3.98E-08 | 1/kg; Paramagnetic |
| Thermal Properties | Metric | English | Comments |
| Heat of Fusion | 325 J/g | 140 BTU/lb | High Purity Ti. |
| CTE, linear | 8.35 µm/m-°C @Temperature 15.0 °C | 4.64 µin/in-°F @Temperature 59.0 °F | |
| 8.70 µm/m-°C @Temperature 100 °C | 4.83 µin/in-°F @Temperature 212 °F | ||
| 9.50 µm/m-°C @Temperature 300 °C | 5.28 µin/in-°F @Temperature 572 °F | ||
| 9.70 µm/m-°C @Temperature 0.000 – 540 °C | 5.39 µin/in-°F @Temperature 32.0 – 1000 °F | perpendicular to the c-axis | |
| Specific Heat Capacity | 0.520 J/g-°C | 0.124 BTU/lb-°F | |
| 0.560 J/g-°C @Temperature 200 °C | 0.134 BTU/lb-°F @Temperature 392 °F | ||
| 0.620 J/g-°C @Temperature 400 °C | 0.148 BTU/lb-°F @Temperature 752 °F | ||
| 0.690 J/g-°C @Temperature 600 °C | 0.165 BTU/lb-°F @Temperature 1110 °F | ||
| التوصيل الحراري | 16.0 W/m-K | 111 BTU-in/hr-ft²-°F | annealed |
| نقطة الانصهار | <= 1670 °C | <= 3040 °F | |
| Liquidus | 1670 °C | 3040 °F | |
| Beta Transus | 882 °C | 1620 °F | |
| Optical Properties | Metric | English | Comments |
| Emissivity (0-1) | 0.3 @Temperature 710 °C | 0.3 @Temperature 1310 °F | High purity Ti |
| Reflection Coefficient, Visible (0-1) | 0.56 | 0.56 | High purity Ti; visible light. |
| Component Elements Properties | Metric | English | Comments |
| Carbon, C | <= 0.10 % | <= 0.10 % | |
| Hydrogen, H | <= 0.015 % | <= 0.015 % | |
| Iron, Fe | <= 0.20 % | <= 0.20 % | |
| Nitrogen, N | <= 0.030 % | <= 0.030 % | |
| Other, total | <= 0.30 % | <= 0.30 % | |
| Oxygen, O | <= 0.18 % | <= 0.18 % | |
| Titanium, Ti | >= 99.175 % | >= 99.175 % | |
| Descriptive Properties | |||
| Alpha Phase Crystal Structure | cph, below 882°C | ||
| Beta Phase Crystal Structure | bcc, above 882°C | ||
| Ti. Alloy Grade Titanium Alloy Grade 1 Round Tubes | Titanium Grade 1 Oil and gas tubes distributor |
| Titanium Alloy Grade 1 Round Tubing | ASME Titanium Grade 1 Seamless Tube |
| Titanium Grade 1 Round Tube suppliers | Seamless Titanium Grade 1 Tubing |
| UNS R50250 Round Tubes distributor | 1 Nickel Chromium Tubing |
| Titanium Alloy Grade 1 Round Tube suppliers | Titanium Grade 1 Nuclear tubes suppliers |
| Titanium Alloy Grade 1 Welded Tube suppliers | Titanium Grade 1 Chemical process tubes traders |
| Titanium Alloy Grade 1 Round Tubes stockist | Titanium Grade 1 Medical tubes manufacturers |
| Titanium Grade 1 Seamless Tube | Titanium Grade 1 Heat exchanger tubes stockist |
| Grade 1 Titanium Welded Tube | Titanium Grade 1 Control lines manufacturers |
| Titanium Alloy Grade 1 Coil Tubes | Titanium Grade 1 Umbilicals suppliers |
| Alloy WERKSTOFF NR. 3.7025 Welded Tubes | Titanium Grade 1 Hydraulic tubes traders |
| Titanium Grade 1 Triangle Tube exporter in CHINA | Titanium Grade 1 Electropolished Tubes |
| Titanium Grade 1 Hexagonal Tube distributor | Titanium Grade 1 SCH 40 Tube exporter in CHINA |
| Titanium Grade 1 Hollow Tubes Suppliers | Titanium Grade 1 SCH 80 Tube distributor |
| exporter of Titanium Grade 1 thermocouple Tube | Titanium Grade 1 Oil & Gas Tubing distributor |
| Trader of ASTM Titanium Grade 1 Polish Tube | Titanium Grade 1 SCH 40 Tube distributor |
| Titanium Grade 1 Cold Drawn Tube stockist | Titanium Grade 1 SCH 80 Tube manufacturers |
| Titanium Grade 1 ERW Tube manufacturers | Titanium Grade 1 Seamless Hollow Tubes |
| High Quality Titanium Grade 1 Seamless Tube | Stockist of Titanium Grade 1 Electropolished Tubes |
| Titanium Grade 1 Square Tube manufacturers | ASTM/ASME Titanium Grade 1 Capillary Tubes |
| Titanium Grade 1 Round Tube exporter in CHINA | Titanium Grade 1 U Shaped Tube distributor |
| Titanium Grade 1 Rectangular Tube traders | Titanium Grade Titanium Alloy Grade 1 Tube suppliers |
| ASTM Titanium Grade 1 Round Tubes stockist | ASTM Titanium Grade 1 Decorative Tubes |
| exporter of Titanium Grade 1 Colour Coated Tube | Titanium Grade 1 Tubing exporter in CHINA |
| Titanium Grade 1 Welded Tube stockist | Titanium Grade 1 Oil Tube suppliers |
| Titanium Grade 1 Secondary & Surplus Tube | ASTM Titanium Grade 1 Instrumentation Tubes |
| Titanium Grade 1 Outside Polished Tube | Titanium Grade 1 Triangle Tube distributor |
| ASTM/ASME Titanium Grade 1 Capillary Tubes | Titanium Grade 1 High-strength capillary tubing |
| Titanium Grade 1 EFW Tube suppliers | Titanium Grade 1 Bellows Tubes exporter in CHINA |
| Titanium Grade 1 Boiler Tubes distributor | Titanium Grade 1 precision tubes stockist |
| Titanium Grade 1 Cold Drawn Tube wholesaler | Titanium Grade 1 Transmission tubes importers |
| Titanium Grade 1 U Shaped Tube suppliers | Titanium Grade 1 Pitot tubes exporter in CHINA |
| Titanium Grade 1 exhaust tubing manufacturers | Titanium Grade 1 encapsulated coiled tubing |
| Titanium Grade 1 Condensers tubes stockholder | Titanium Grade 1 High pressure tubes stockist |
| Titanium Grade 1 Super Heaters exporter in CHINA | Titanium Grade 1 Nuclear Fuel tubes manufacturers |
| distributor of Titanium Grade 1 Tubes for Heat Exchangers | Titanium Grade 1 EFW Tubes Suppliers |
| Titanium Grade 1 redrawn tubing suppliers | distributor of Titanium Grade 1 Instrumentation tubes |
| Titanium Grade 1 seam-welded tubing stockist | exporter of Titanium Grade 1 high precision tubes |
| supplier of Titanium Grade 1 cold-drawn coiled tubing | Titanium Grade 1 Nuclear Control Rod Tubes |
| Titanium Grade 1 Chemical Process Tubes stockist | Titanium Grade 1 Seamless Tubing stockist |
| Titanium Grade 1 Welded coiled tubing distributor | Stockholder of Titanium Grade 1 Gas Tube Ar 15 |
| Titanium Alloy Grade 1 heat resistant tubing | Titanium Grade 1 Bourdon Tube importers |
| custom Titanium Grade 1 tubing | Distributor of Titanium Grade 1 Capillary Tubing |
| Titanium Grade 1 header tubing | Supplier of Titanium Grade 1 Furnace Tube |
| Titanium Grade 1 rectangular tubing | Titanium Grade 1 Gas Tubing manufacturers |
| Titanium Grade 1 Cold Rolled Coiled Tubing | Titanium Grade 1 seamless coil tubing wholesaler |
| Titanium Grade 1 Heat-resistant capillary Tube | Titanium Grade 1 seamless straight tubing |
| Titanium Grade 1 Square Tubing manufacturers | Titanium Grade 1 cold drawn seamless tubes |
| ASTM Titanium Grade 1 Heat Exchager Tubes | Titanium Grade 1 Aerospace Engine Tubes stockist |
| Titanium Grade 1 Tubing | Titanium Grade 1 Furnace Tubes manufacturers |
| Grade 1 Titanium Instrumentation Tubes | Titanium Grade 1 Precision Tubing exporter in CHINA |
| Titanium Alloy Grade 1 coiled tubing | Titanium Grade 1 Hot finished seamless tubing (HFS) |
| Titanium Alloy Grade 1 straight tube heat exchanger | Titanium Grade 1 Cold drawn seamless tubing (CDS) |
| Titanium Grade 1 umbilical tubing | Titanium Grade 1 Drawn over mandrel (DOM) |
| Titanium Grade 1 extreme environment gas tube | supplier of Grade 1 Titanium Finned Tube |
| Titanium Grade 1 tube stock | Titanium Grade 1 Tubes for Precision Components |
| Titanium Grade 1 welded tubing stockist | Titanium Alloy Grade 1 Seamless Tube |
| Titanium Grade 1 tubing bends | Grade 1 Titanium Seamless Tubes |
| Titanium Grade 1 thin wall tubing | UNS R50250 Seamless Tube |
| custom Titanium Grade 1 tubing | Grade 1 Titanium Welded Tubes |
| Titanium Grade 1 tube sizes | Titanium Alloy UNS R50250 Welded Tube |
| Titanium Grade 1 cannula Tubes | Ti. Alloy Grade 1 Welded Tubes |
| Titanium Grade 1 pyrometer tubes | WERKSTOFF NR. 3.7025 Seamless Tubes |
| Titanium Grade 1 protective tubes | ASME SB338 Ti. Alloy Grade 1 Seamless Tube |
| Titanium Grade 1 hypodermic tubing | ASME SB338 Ti. Alloy Grade 1 Round Tubes |
| Titanium Grade 1 capillary tube | Titanium Grade 1 Mortar Tube stockholder |
اختر Daxun لمساعدة مشروعك على الانطلاق.

Advanced Production:Titanium seamless pipe
- Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
- (The above is agreed upon by the manufacturer and the customer based on the specific situation)
Grade 1 Titanium Tube Features
Grade 1 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.
- Softest Titanium
- Highest Ductility
- Excellent Corrosion Resistance
- Good Cold Formability


Advanced Production: Titanium Welded Tube
Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.
تقارير الاختبار
The test reports we provide include: Factory test certificate for Grade 1 titanium welded pipe and Grade 1 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)


Applications and standards
Titanium Grade 1 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:
- Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
- Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
Standard : ASTM, ASME and API
الجودة والتسليم والتفتيش
Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 1 Titanium Welded Pipe and Grade 1 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.
- وقت التسليم لدينا يتوافق تمامًا مع العقد.
- دعم الوكالات الخارجية للعملاء للذهاب إلى المصنع للفحص
- دعم العينات المجانية لاختبار العملاء
- دعم الفحص الموقعي أو فحص المصنع بالفيديو


التعبئة والتغليف
تضمن شركة Daxun Alloy أفضل جودة للتغليف لأنها تلعب دورًا مهمًا في الشحن الدولي حيث تمر البضائع عبر قنوات مختلفة للوصول إلى الوجهة النهائية، لذلك نولي اهتمامًا خاصًا بالتغليف. نقوم بتغليف بضائعنا بعدة طرق حسب المنتج. نقوم بتغليف منتجاتنا بعدة طرق مثل:
- الصناديق والصناديق
- الغلاف المنكمش
- منصات خشبية
- صناديق خشبية
الدعم الفني
إذا كنت بحاجة إلى أي مساعدة فنية إضافية، فسيكون من دواعي سرور أخصائي المعادن المقيم لدينا وموظفينا المطلعين تقديم المساعدة. بالإضافة إلى ذلك، تفتخر Daxun بوجود مختبر اختبار معتمد - وهو الأول من نوعه في صناعة مخزون المعادن المتعددة والبلاستيك. وهذا، في رأينا، يدل على تفانينا الثابت للجودة وفلسفتنا كمورد متكامل الخدمات.

Grade 1 Titanium TUBE Features
Daxun Grade 1 Titanium TUBE Let your brand improve rapidly
- معرض الصور
- Titanium tube/pipe:
- السطح
- Types of
- Weight
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube. | |
| Products/Processing Standard | Grade/Size |
| Titanium pipe, tube, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet) |
| AMS-T-9046 | |
| Titanium and Titanium alloy tube | |
| Commercially pure titanium (CP) | |
| Code designation | Yield strength |
| minimum, ksi 1 / | |
| CP-1 | 70 |
| CP-2 | 55 |
| CP-3 | 40 |
| CP-4 | 25 |
| Alpha titanium alloys(A) | |
| Code designation | Composition |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| Alpha-beta titanium alloys(AB) | |
| Code designation | Composition |
| AB-1 | 6A1-4V |
| AB-2 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| Beta titanium alloys(B) | |
| Code designation | Composition |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| Processing: | |
| الدرفلة على الساخن | الدرفلة على البارد |
| Available Grades: | |
| الصف الأول الابتدائي | Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| الصف الثاني الابتدائي | Grade 6Al-4V ELI (Formerly Grade 23) |
| Grade 7 | Grade 6Al-6V-2Sn (6-62) |
| Grade 19 | Grade 8Al-1Mo-1V (8-1-1) |
| Grade 5 (6Al-4V) | Grade 9 (3Al-2.5V) |
| Grade 6 (5Al-2.5Sn) | الصف الثالث الابتدائي |
| Application | |
| الصناعة الكيميائية | Desalination Of Sea Water |
| Petrochemical Industry | الطيران والفضاء |
| Machining Field, Automobile Field | Mobile Phone Component Field. |
| urface Finish | Internal Surface(ID) | Exterbal Surface(OD) | |||
| Roughness Average(RA) | Roughness Average(RA) | ||||
| μ inch | μm | μ inch | μm | ||
| بكالوريوس | Beight Annealed | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| EP | Electro Polish | 15,10,7,5 | 0.38,0.25,0.20;0.13 | 32 | 0.8 |
| MP | Mechanical Polish | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| AP | Annealed & Pickled | Not defined | Not defined | 40 or Not defined | 1.0 or Not defined |
| Titanium Grade 1 Seamless Pipe | Titanium DIN 3.7025 Seamless Pipe |
| Titanium UNS R50250 Seamless Pipe | |
| Titanium Grade 1 Seamless Pipes | |
| Titanium Alloy Gr.1 Seamless Pipe | |
| ASTM B337 Titanium Grade 1 Seamless Pipe | |
| ASME SB337 Ti Alloy Gr.1 Seamless Pipes | |
| Titanium Grade 1 Welded Pipe | Titanium DIN 3.7025 Welded Pipe |
| Titanium UNS R50250 Welded Pipe | |
| Titanium Grade 1 Welded Pipes | |
| Titanium Alloy Gr.1 Welded Pipe | |
| ASTM B337 Titanium Grade 1 Welded Pipes | |
| ASME SB337 Ti Alloy Gr.1 Welded Pipes | |
| Titanium Grade 1 Round Pipe | Titanium DIN 3.7025 Round Pipe |
| Titanium UNS R50250 Round Pipes | |
| Titanium Grade 1 Round Pipes | |
| Titanium Alloy Gr.1 Round Pipe | |
| Titanium Grade 1 Round Pipe | |
| Ti Alloy Gr.1 Round Pipes | |
| Titanium Gr.1 Seamless Tubes | Titanium DIN 3.7025 Seamless Tubes |
| Titanium UNS R50250 Seamless Tubes | |
| Titanium Grade 1 Seamless Tubing | |
| Titanium Alloy Gr.1 Seamless Tubes | |
| ASTM B338 Titanium Gr.1 Seamless Tubing | |
| ASME SB338 Ti Alloy Grade 1 Seamless Tubes | |
| Titanium Grade 1 Welded Tubes | Titanium DIN 3.7025 Welded Tubes |
| Titanium UNS R50250 Welded Tubes | |
| Titanium Grade 1 Welded Tubing | |
| Titanium Alloy Gr.1 Welded Tubes | |
| ASTM B338 Titanium Grade 1 Welded Tubing | |
| ASME SB338 Ti Alloy Gr.1 Welded Tubes | |
| Titanium Grade 1 Round Tubes | Titanium DIN 3.7025 Round Tubes |
| Titanium UNS R50250 Round Tubes | |
| Titanium Grade 1 Round Tubing | |
| Titanium Alloy Gr.1 Round Tubes | |
| Titanium Grade 1 Round Tubing | |
| Ti Alloy Gr.1 Round Tubes | |
| Titanium Grade 1 Pipe | Titanium DIN 3.7025 Pipe |
| Titanium UNS R50250 Pipes | |
| Titanium Grade 1 Pipe | |
| Titanium Alloy Gr.1 Pipes | |
| Titanium Grade 1 Pipes | |
| Ti Alloy Gr.1 Pipe | |
| Titanium Grade 1 Tube | Titanium DIN 3.7025 Tubes |
| Titanium UNS R50250 Tube | |
| Titanium Grade 1 Tubing | |
| Titanium Alloy Gr.1 Tubes | |
| Titanium Grade 1 Tubes | |
| Ti Alloy Gr.1 Tubes |
| NPS | Outside Diameter | Wall Thickness | Weight | Weight | |||
| in | mm | in | mm | Sched | kg/Mtr | Lb/ft | |
| 1/2″ | 0.84 | 21 | 0.109 | 2.769 | 40 STD | 1.268 | 0.851 |
| 0.147 | 3.734 | 80 STD | 1.621 | 1.088 | |||
| 3/4″ | 1.05 | 27 | 0.113 | 2.87 | 40 STD | 1.684 | 1.131 |
| 0.154 | 3.912 | 80 STD | 2.195 | 1.474 | |||
| 1″ | 1.315 | 33 | 0.133 | 3.378 | 40 STD | 2.501 | 1.679 |
| 0.179 | 4.547 | 80 STD | 3.325 | 2.172 | |||
| 1 1/4″ | 1.66 | 42 | 0.14 | 3.556 | 40 STD | 3.385 | 2.273 |
| 0.191 | 4.851 | 80 STD | 4.464 | 2.997 | |||
| 1 1/2″ | 1.9 | 48 | 0.145 | 3.683 | 40 STD | 4.048 | 2.718 |
| 0.2 | 5.08 | 80 STD | 5.409 | 3.361 | |||
| 2″ | 2.375 | 60 | 0.154 | 3.912 | 40 STD | 5.441 | 3.653 |
| 0.218 | 5.537 | 80 STD | 7.48 | 5.022 | |||
| 2 1/2″ | 2.875 | 73 | 0.203 | 5.516 | 40 STD | 8.629 | 5.793 |
| 0.276 | 7.01 | 80 STD | 11.411 | 7.661 | |||
| 3″ | 3.5 | 89 | 0.216 | 5.486 | 40 STD | 11.284 | 7.576 |
| 0.3 | 7.62 | 80 STD | 15.272 | 10.253 | |||
| 4″ | 4.5 | 114 | 0.237 | 6.02 | 16.073 | 10.79 | |
| 0.337 | 8.56 | 22.318 | 14.983 | ||||
| 6″ | 6.625 | 168 | 0.188 | 4.775 | 19.252 | 12.924 | |
| 0.203 | 5.516 | 20.739 | 13.923 | ||||
| 0.219 | 5.563 | 22.318 | 14.983 | ||||
| 0.25 | 6.35 | 25.354 | 17.021 | ||||
| 0.28 | 7.112 | 40 STD | 58.263 | 18.974 | |||
| 0.312 | 7.925 | 31.334 | 21.036 | ||||
| 0.375 | 9.525 | 37.285 | 25.031 | ||||
| 0.432 | 10.973 | 80 XHY | 42.561 | 28.573 | |||
| 0.5 | 12.7 | 48.719 | 32.708 | ||||
| 8″ | 8.625 | 219 | 0.188 | 4.775 | 25.233 | 16.94 | |
| 0.203 | 5.156 | 27.198 | 18.259 | ||||
| 0.219 | 5.563 | 29.286 | 19.661 | ||||
| 0.25 | 6.35 | 20 | 33.308 | 22.361 | |||
| 0.277 | 7.036 | 30 | 36.786 | 24.696 | |||
| 0.322 | 8.179 | 40 | 42.352 | 28.554 | |||
| 0.375 | 9.525 | 49.216 | 33.041 | ||||
| 0.406 | 10.312 | 60 | 53.085 | 35.638 | |||
| 0.5 | 12.7 | 80 XHY | 64.627 | 43.388 | |||
| 10″ | 10.75 | 273 | 0.188 | 4.775 | 31.588 | 21.207 | |
| 0.219 | 5.563 | 36.689 | 24.631 | ||||
| 0.25 | 6.35 | 20 | 41.759 | 28.035 | |||
| 0.307 | 7.798 | 30 | 51.002 | 34.24 | |||
| 0.344 | 8.738 | 56.946 | 38.231 | ||||
| 0.365 | 9.271 | 40 STD | 63.301 | 40.483 | |||
| 0.438 | 11.125 | 71.852 | 48.238 | ||||
| 0.5 | 12.7 | 60 XHY | 81.53 | 54.735 | |||
| 0.594 | 15.088 | 80 | 95.969 | 64.429 | |||
| 12″ | 12.75 | 324 | 0.188 | 4.775 | 37.57 | 25.222 | |
| 0.219 | 5.563 | 43.657 | 29.309 | ||||
| 0.25 | 6.35 | 49.713 | 33.375 | ||||
| 0.281 | 7.137 | 55.739 | 37.42 | ||||
| 0.312 | 7.925 | 61.735 | 41.445 | ||||
| 0.375 | 9.525 | 73.824 | 49.562 | ||||
| 0.406 | 10.312 | 79.727 | 53.525 | ||||
| 0.5 | 12.7 | 97.438 | 65.415 | ||||
| 0.562 | 14.275 | 108.966 | 73.154 | ||||
| 14″ | 14 | 356 | 0.188 | 4.775 | 41.308 | 27.732 | |
| 0.219 | 5.563 | 48.012 | 32.233 | ||||
| 0.25 | 6.35 | 20 | 54.685 | 36.713 | |||
| 0.281 | 7.137 | 61.327 | 41.172 | ||||
| 0.312 | 7.925 | 67.939 | 45.611 | ||||
| 0.375 | 9.525 | STD | 81.281 | 54.568 | |||
| 0.438 | 11.125 | 40 | 94.498 | 63.441 | |||
| 0.5 | 12.7 | XHY | 107.381 | 72.09 | |||
| 0.625 | 15.875 | 132.983 | 89.278 | ||||
| 16” | 16 | 406 | 0.188 | 4.775 | 47.29 | 21.748 | |
| 0.219 | 5.563 | 54.98 | 36.91 | ||||
| 0.25 | 6.35 | 10 | 62.639 | 42.053 | |||
| 0.281 | 7.137 | 70.268 | 47.174 | ||||
| 0.312 | 7.925 | 20 | 77.866 | 52.275 | |||
| 0.344 | 8.738 | 85.677 | 57.519 | ||||
| 0.375 | 9.525 | 30 | 93.213 | 62.578 | |||
| STD | |||||||
| 0.438 | 11.125 | 108.433 | 72.797 | ||||
| 0.5 | 12.7 | 40 | 123.289 | 82.77 | |||
| XHY | |||||||
| 18″ | 18 | 457 | 0.219 | 5.563 | 61.948 | 41.588 | |
| 0.25 | 6.35 | 70.593 | 47.393 | ||||
| 0.281 | 7.137 | 79.208 | 53.176 | ||||
| 0.312 | 7.925 | 20 | 87.792 | 58.939 | |||
| 0.375 | 9.525 | STD | 105.144 | 70.588 | |||
| 0.438 | 11.125 | 30 | 122.369 | 82.152 | |||
| 0.5 | 12.7 | XHY | 139.198 | 93.45 | |||
| 0.562 | 14.275 | 40 | 155.904 | 104.666 | |||
| 0.625 | 15.875 | 172.754 | 115.978 | ||||
| 20″ | 20 | 508 | 0.25 | 6.35 | 78.547 | 52.733 | |
| 0.282 | 7.163 | 88.458 | 59.386 | ||||
| 0.312 | 7.925 | 97.719 | 65.604 | ||||
| 0.375 | 9.525 | 20 STD | 117.075 | 78.598 | |||
| 0.438 | 11.125 | 136.305 | 91.508 | ||||
| 0.5 | 12.7 | 30 XHY | 155.106 | 104.13 | |||
| 0.594 | 15.088 | 40 | 183.378 | 123.11 | |||
| 0.625 | 15.875 | 192.64 | 129.328 | ||||
| 0.688 | 17.475 | 211.368 | 141.901 | ||||
| 24″ | 24 | 610 | 0.25 | 6.35 | 94.456 | 63.413 | |
| 0.281 | 7.137 | 106.029 | 71.183 | ||||
| 0.312 | 7.925 | 117.573 | 18.932 | ||||
| 0.375 | 9.525 | 20 STD | 140.938 | 64.618 | |||
| 0.438 | 11.125 | 164.176 | 110.219 | ||||
| 0.5 | 12.7 | XHY | 186.923 | 125.49 | |||
| 0.625 | 15.875 | 232.41 | 156.028 | ||||
| 0.688 | 17.475 | 40 | 255.148 | 171.293 | |||
| 0.75 | 19.05 | 277.401 | 186.233 | ||||
| 30″ | 30 | 762 | 0.25 | 6.35 | 118.318 | 79.433 | |
| 0.281 | 7.137 | 132.851 | 89.189 | ||||
| 0.312 | 7.925 | 10 | 147.353 | 98.925 | |||
| 0.375 | 9.525 | STD | 176.731 | 118.648 | |||
| 0.438 | 11.125 | 205.983 | 138.286 | ||||
| 0.5 | 12.7 | 20 XHY | 234.647 | 157.53 | |||
| 0.625 | 15.875 | 30 | 292.066 | 196.078 | |||
| 0.688 | 17.475 | 320.817 | 215.38 | ||||
| 0.75 | 19.05 | 348.988 | 234.293 | ||||
| 36″ | 36 | 914 | 0.25 | 6.35 | 142.18 | 95.453 | |
| 0.281 | 7.137 | 159.672 | 107.196 | ||||
| 0.312 | 7.925 | 10 | 177.133 | 118.918 | |||
| 0.375 | 9.525 | STD | 215.525 | 142.678 | |||
| 0.438 | 11.125 | 247.79 | 166.353 | ||||
| 0.5 | 12.7 | 20 XHY | 282.372 | 198.57 | |||
| 0.625 | 15.875 | 351.723 | 236.128 | ||||
| 0.688 | 17.475 | 386.487 | 259.467 | ||||
| 0.75 | 19.05 | 420.576 | 282.353 | ||||
| 42″ | 42 | 1067 | 0.312 | 7.925 | 206.914 | 138.911 | |
| 0.375 | 9.525 | STD | 248.319 | 166.708 | |||
| 0.5 | 12.7 | XHY | 33.097 | 221.61 | |||
| 0.75 | 19.05 | 492.163 | 330.413 | ||||
| 48″ | 48 | 1219 | 0.375 | 9.525 | STD | 284.112 | 190.738 |
| 0.438 | 11.125 | 331.404 | 222.487 | ||||
| 0.5 | 12.7 | XHY | 377.822 | 253.65 | |||
| 0.75 | 19.05 | 563.75 | 378.473 | ||||
| 0.875 | 22.225 | 655.969 | 440.383 | ||||
Grade 1 titanium tube form (4)
المعلومات المتاحة للرجوع إليها وتنزيلها
Daxun is a trustworthy stainless steel tube manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
أحدث مشاريع ومنتجات الحالة الساخنة
المنتجات ذات الصلة (8)
ASTM B338 | ASTM B265 | ASME SB265 | ASTM F67 | ISO 5832-2 | 3.7025 | UNS R50250
- Pure titanium Grade 1 has excellent ductility and cold formability, making it ideal for deep drawing. Titanium Grade 1 is well-known for its good general and seawater corrosion resistance, as well as its great resistance to oxidising, neutral, and mildly reducing media (solutions), including chlorides.
- Titanium’s low density (approximately half that of nickel-based alloys), high strength-to-weight ratio, and corrosion resistance make it an excellent choice for a variety of harsh chemical conditions.
تعتمد درجة سبيكة التيتانيوم التي تحتاجها على المشروع الذي تعمل عليه، حيث أن لكل درجة فوائد مختلفة.
إنّ جميع درجات سبائك التيتانيوم قوية للغاية ومقاومة للتآكل، مما يعني أنها ستستمر في العمل بشكل جيد في أقسى الظروف.
إن الدرجات الأعلى من سبائك التيتانيوم (5-12) هي سبائك مصممة لفوائد محددة. على سبيل المثال، تتميز سبائك التيتانيوم من الدرجة 12 بمقاومة ممتازة للحرارة، مما يجعلها خياراً مثالياً للمبادلات الحرارية الصدفية والأنبوبية والأنابيب الهيدروليكية ومعدات الصناعة الكيميائية.
الدرجات من 1-4 هي سبائك التيتانيوم النقي، وهي خيار مثالي إذا كنت بحاجة إلى مادة قابلة للحام وقابلة للسحب لأنظمة الأنابيب والأنابيب. ستجد درجات أقل تستخدم في الصناعات البحرية والصناعية.
إذا كنت تبدأ مشروعاً ولست متأكداً من درجة سبيكة التيتانيوم الأفضل لك، اتصل بنا اليوم؛ فنحن سعداء للغاية بمساعدتك.
نقدم في DAXUN مجموعة واسعة من درجات سبائك التيتانيوم من الدرجة 1 إلى الدرجة 12.
الدرجات من 1 إلى 4 هي التيتانيوم النقي، بينما الدرجات الأعلى هي السبائك.
تحظى درجات السبائك بشعبية كبيرة بسبب نسبة قوتها إلى وزنها العالية.
درجة سبائك التيتانيوم الأكثر استخداماً لدينا هي الدرجة 5. وعلى الرغم من أنها لا تزال تحتوي على نسبة عالية من التيتانيوم، إلا أن هذه الدرجة هي الأكثر موثوقية لأنها تتحمل درجات حرارة تصل إلى 600 درجة فهرنهايت وتتحمل الظروف القاسية.
وتفضل الصناعات مثل صناعات الطيران والصناعات البحرية الدرجات الأعلى لمقاومتها للتآكل والتآكل.
وعلى العكس من ذلك، تُستخدم الدرجات الأقل في المقام الأول في اللحام نظرًا لانخفاض قوتها.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
على الرغم من أن درجة التيتانيوم تزيد من التكلفة قليلاً، إلا أن التكلفة الإجمالية تتحدد في المقام الأول حسب شكل وشكل التيتانيوم الذي تحتاجه.
At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
لسوء الحظ، من الصعب التوصل إلى سعر عبر الإنترنت دون معرفة الكثير عن مشروعك وما سيُستخدم التيتانيوم من أجله.
لحسن الحظ، فريق خبرائنا موجود دائماً لمساعدتك وتقديم المشورة لك بشأن احتياجاتك من التيتانيوم. من خلال إرسال بريد إلكتروني إلى [email protected]، سنكون قادرين على الرد عليك ببعض النصائح وعرض أسعار دقيق.
احرص على تضمين أكبر قدر ممكن من المعلومات حول درجة وشكل وكمية التيتانيوم التي تحتاجها للحصول على فهم أفضل لاحتياجاتك.
يتمتع فريق العمل في DAXUN بالخبرة والمعرفة والود. وبفضل سنوات خبرتهم الطويلة في هذا المجال، فهم يعرفون كل شيء عن التيتانيوم، بما في ذلك استخداماته وفوائده ودرجاته.
للحصول على تحديثات منتظمة عن التيتانيوم واستخداماته وتطبيقاته في مختلف الصناعات، احرص على الاطلاع على مدونتنا. لقد كتب خبراؤنا أدلة سهلة المتابعة يمكنك الرجوع إليها دائماً عندما تكون لديك أسئلة.
إذا كنت لا تزال تواجه مشكلة، فلا تتردد في الاتصال بنا؛ يسعدنا تقديم المساعدة.
من خلال إرسال بريد إلكتروني إلى [email protected]، ستتلقى رداً سريعاً. تأكد من تضمين أكبر قدر ممكن من التفاصيل في سؤالك حتى نتمكن من التوصية بالحل المناسب.
يُرجى ملء النموذج الموجود في صفحة “اتصل بنا”، أو الاتصال بمدير المبيعات لدينا على “+86 13382898899”، وسوف نتصل بك في أقرب وقت ممكن. واتسابنا على الإنترنت، وسيتم التحقق من البريد الإلكتروني ([email protected]) في غضون 6 ساعات. سيتم الرد على كل استفسار أو رسالة على الفور. بالإضافة إلى ذلك، نشارك معلومات السوق مع عملائنا كل أسبوع
يمكننا تقديم عينات من صفائح الفولاذ المقاوم للصدأ لك للتحقق من الجودة. العينة مجانية وما عليك سوى دفع أجرة الشحن.
لقد قمنا بالتصدير إلى أكثر من 42 دولة، مثل كندا، وتشيلي، والكويت، وألمانيا، وكوريا الجنوبية، والمملكة العربية السعودية، وسنغافورة، وغيرها.
موك لدينا هو 1 طن لصفائح الفولاذ المقاوم للصدأ.
يمكن تسليم الطلبات التجريبية في غضون أسبوع. بالنسبة للطلبات العادية، يستغرق الأمر أسبوعين تقريباً.