Daxun is an excellent manufacturer of CP-2-grade titanium rods
As China’s leading supplier of titanium and titanium alloy rods, Daxun provides high-performance titanium rods to the world.
- Titanium Rod Grade:CP-2(Grade 2)- UNS R50400-3.7035-TA2
- Types: Hot rolled rod, forged rod, cold drawn rod, extruded rod etc
- Shape: Titanium round bar, titanium square bar、Ti hexagonal bar
- Density of Titanium Rod: Density of Grade 2 Titanium Rod is 4.51g/cm3
- Standards: ASTM B 348,ASME SB348,DIN 17862,ASTM F67,ASTM 265
- Dimensions: GB, GJB, EN, ASTM, JIS, ASME, BS, AISI, DIN, ISO, etc.
O líder mundial em serviços de fabrico de barras de titânio comercialmente puro
Grade 2 Titanium Rod is the workhorse among titanium alloy rods, offering an excellent balance of strength and weight for weight-sensitive applications. As a commercially pure (CP) titanium alloy, it achieves an ideal combination of strength and ductility, making it suitable for a wide range of demanding uses. It provides high impact strength, is easily weldable, and is extremely corrosion-resistant in oxidizing conditions, alkaline media, brine solutions, weakly reducing environments, nitric acid, and wet chlorine. Additionally, its excellent resistance to seawater and saline solutions further enhances its versatility.
The Grade 2 Titanium Rod stands out for its lightweight nature, impressive strength-to-weight ratio, and outstanding resistance to corrosion, making it highly versatile and ideal for numerous industrial uses. From general industrial uses to military and aerospace applications, this material delivers reliable performance in challenging environments.
Daxun Alloys stocks Grade 2 Titanium Rods in a variety of diameters to meet the specific requirements of different projects. Our inventory includes sizes ranging from 1 mm to 300 mm, with the ability to accommodate custom orders for larger dimensions. All rods are certified to ASTM B348 and ASTM B381 standards.
For those seeking reliable suppliers, Daxun Alloys offers a comprehensive range of Grade 2 Titanium products, including ASTM B348 Titanium Grade 2 Round Bars, UNS R50400 Bright Bars, and WERKSTOFF NR. 3.7035 Round Bars. Whether you need round, forged, or square bars, we ensure consistent quality and competitive pricing.
Feel free to contact Daxun Alloys for inquiries or to request a quote. Our team is committed to providing high-quality Grade 2 Titanium Rods and is happy to assist with any questions or project-specific needs.
Dados
- Parâmetro
- Ingrediente
- Propriedades mecânicas
- Propriedades físicas
- Pesquisas quentes
| Especificação | Detalhes |
| Material | Titanium rod and bar Grade 2 (UNS R50400) |
| Padrão | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| Dimensões | EN, ASTM, JIS, ASME, BS, AISI |
| Gama de diâmetros | 0,125″ - 14″ (3,175mm - 355,6mm), personalizado |
| Comprimento Intervalo | Até 240″ (6096mm), personalizado |
| Acabamento | Trefilado a frio (brilhante), esmerilado sem centro, laminado a quente, torneado liso, descascado, borda laminada com fenda, laminado a quente recozido, torneado em bruto, brilhante, polido, rectificado, esmerilado sem centro e preto |
| Acabamento da superfície | Estirado a frio, rectificado sem centros, polido ou torneado em bruto, preto, acabamento NO.4, acabamento BA, acabamento mate, etc. |
| Estado | Endurecido e temperado, recozido |
| Tolerância | Tolerância de diâmetro: +/- 0,005″ (0,127mm), tolerância de comprimento: +/- 0,125″ (3,175mm) |
| Formulário | Barras quadradas de titânio, lingotes de titânio, barras redondas de titânio, barras rectangulares de titânio, barras triangulares de titânio, barras forjadas de titânio, barras hexagonais de titânio, etc. |
| Propriedades físicas | Densidade: 0,163 lb/in³ (4,51 g/cm³), Ponto de fusão: 3.020°F (1.660°C), Alongamento: 20-30%, Módulo de elasticidade: 16,5 x 10⁶ psi (114 GPa) |
| Composição química | Titânio (min): 99.2%, Oxigénio (máx): 0.25%, Carbono (máx.): 0,08%, Ferro (máx.): 0.30%, Azoto (máx): 0,03%, Hidrogénio (máx.): 0.015% |
| Elemento | Weight % |
| C | ≤0.08 |
| O | ≤0.25 |
| N | ≤0.03 |
| H | ≤0.015 |
| Fe | ≤0.30 |
| *OEE | ≤0.10 |
| *OET | ≤0.40 |
| Ti | Remaining |
| Dureza, Knoop | 170 | 170 | |
| Hardness, Rockwell B | 80 | 80 | |
| Dureza, Vickers | 145 | 145 | |
| Tensile Strength, Ultimate | 344 MPa | 49900 psi | |
| Tensile Strength, Yield | 275 – 410 MPa | 39900 – 59500 psi | |
| Alongamento na rutura | 20 % | 20 % | |
| Redução da área | 35 % | 35 % | |
| Módulo de elasticidade | 105 GPa | 15200 ksi | In Tension |
| Compressive Modulus | 110 GPa | 16000 ksi | |
| Poisson’s Ratio | 0.37 | 0.37 | |
| Izod Impact | 114 – 171 J | 84.1 – 126 ft-lb | |
| Resistência à fadiga | 300 MPa | 43500 psi | 1E+7 cycles, Unnotched |
| Resistência à fadiga | 425 MPa | 61600 psi | 30,000 cycles, Unnotched |
| Resistência à fratura | 66 MPa-m½ | 60.1 ksi-in½ | K(Q); annealed |
| Módulo de cisalhamento | 45 GPa | 6530 ksi |
| Densidade | Melting Range | Modulus of Elasticity (Tension) | Specific Heat | Mean Coefficient of Expansion | Condutividade térmica | Resistividade eléctrica |
| kg/m3 | °C | GPa | J/kg. °C | x10 -6 / °C | W / m. °C | micro-ohm.m |
| 4,507 | 1668± 10 | 103 | 519 | 8.41 | 11.4 | 0.42 |
| ASTM B348 Alloy Gr 2 Hex Bar Polished | grade 2 titanium Hexagonal Bar |
| ASTM B348 Alloy Gr 2 Rectangular Bar | Titanium WERKSTOFF NR. 3.7035 Threaded Bar Black |
| Titanium UNS R50400 Round Bar | grade 2 titanium Din 3.7035 Flat Bar |
| Titanium Grade 2 Bar | Alloy grade 2 titanium Flat Bar Black |
| Alloy Gr 2 Rounds | ASME SB 338 gr 2 Flat Bar Bright |
| Titanium Alloy Grade 2 Bright Bar | Alloy Gr 2 Flat Bar Polished |
| Alloy grade 2 titanium Hex Bar Annealed | Titanium WERKSTOFF NR. 3.7035 Cold Drawn Round Bar |
| ASTM B348 grade 2 titanium Round Bars | Titanium Grade 2 Flat Bar stock |
| Titanium WERKSTOFF NR. 3.7035 Hex Bar | Alloy Gr 2 Threaded Bar |
| Titanium Grade 2 Square Bar Polished | Titanium UNS R50400 Bright Bar Hot Rolled |
| 3.7035 grade 2 titanium Hex Bar Bright | Alloy Gr 2 Alloy Hollow Bar |
| Gr 2 Titanium Rectangular Bar Annealed | Alloy grade 2 titanium Polished Hex Bar |
| ASME SB 338 gr 2 Forged Bar | Gr 2 Titanium Polished Bar |
| Alloy Gr 2 Alloy Rods | UNS R50400 Titanium Flat Bar Cold Drawn |
| Alloy Gr 2 Square Bar Cold Drawn | Titanium Grade 2 Bright Bar material |
| grade 2 titanium Rod | Titanium UNS R50400 Flat Bar Annealed |
Escolha a Daxun para ajudar o seu projeto a arrancar.
DAXUN® Grade 2 Titanium Rod Features
DAXUN® Ti Grade 2 is a commercially pure (CP) titanium bar known for its standout features:
- Excellent general corrosion resistance in seawater
- Resistant to stress corrosion cracking in chloride and sour gas environments
- Excellent resistance to pitting, crevice, and erosion-corrosion
- High heat transfer efficiency
- Good formability and weldability
- Extremely low thermal expansion
- Moderate strength
Vantagens da fábrica Daxun
Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.
Grade 2 Titanium Rod Production Method
Daxun specializes in producing high-quality titanium bars known for their exceptional performance. Additionally, we offer customized manufacturing services to meet specific requirements as outlined in the customer’s agreement.
- Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Relatórios de ensaio
Os relatórios de teste que fornecemos incluem: Haste de titânio de grau 2 e barra redonda de titânio de grau 2 Certificado de teste de fábrica, EN 10204 3.1, relatório químico, relatório mecânico, relatório de teste PMI, relatório de inspeção visual, relatório de inspeção de terceiros, relatório de laboratório aprovado pela NABL, relatório de teste destrutivo, relatório de teste não destrutivo. (Daxun fornecerá de acordo com os requisitos do cliente)
Grade 2 Rods Applications and Standards
Grade 2 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Aerospace, military, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
- Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
- Normas: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Qualidade, entrega, inspeção
Daxun ensures the reliability of Grade 2 Titanium Rods and Round Bars through rigorous quality assurance tests. These include tensile testing, chemical analysis, PMI for material consistency, micro and macro testing, IGC testing for corrosion resistance, ultrasonic flaw detection, and hardness and expansion evaluations.
Throughout production, Daxun carefully measures diameter, thickness, and surface quality, guaranteeing materials meet the highest standards and application requirements.
- O nosso prazo de entrega está estritamente de acordo com o contrato.
- Apoio a agências terceiras do cliente para se deslocarem à fábrica para inspeção
- Apoio a amostras gratuitas para teste do cliente
- Apoio à inspeção de fábrica no local ou por vídeo
Embalagem
A Daxun Alloy assegura a melhor qualidade de embalagem, uma vez que esta desempenha um papel importante no transporte internacional de mercadorias, onde as mercadorias passam por vários canais para chegar ao destino final, pelo que prestamos especial atenção à embalagem. Embalamos os nossos produtos de várias formas, consoante o produto. Embalamos os nossos produtos de várias formas, tais como:
- Caixas e caixotes
- Embalagem retrátil
- Paletes de madeira
- Caixas de madeira
Apoio técnico
If you require additional technical assistance, our resident metallurgist and knowledgeable staff are ready to support you. At Daxun, we take pride in our certified testing laboratory, a first in the multi-metal and plastic inventory industry. This reflects our unwavering commitment to quality and reinforces our philosophy as a full-service supplier dedicated to meeting your needs.
Grade 2 bar and rod features
Daxun Grade 2 Titanium Rods help your brand improve quickly
- Titanium rod/bar
- Types of Grade 2 Titanium Rods
- Tolerances for Grade 2 Titanium Round Bars (BS EN ISO 286-2)
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of rod/bar, Bar and Tube. | |
| Norma de produtos/transformação | Grau/tamanho |
| Titanium rod/bar— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Espessura: (0,0197”-6”)Largura máxima: 12 pés,Comprimento máximo: 50 pés) |
| AMS-T-9046 | |
| Titanium and Titanium alloy rod/bar | |
| Titânio comercialmente puro (CP) | |
| Designação do código | Resistência ao escoamento |
| mínimo, ksi 1 / | |
| CP-1 | 70 |
| CP-2 | 55 |
| CP-3 | 40 |
| CP-4 | 25 |
| Ligas alfa de titânio(A) | |
| Designação do código | Composição |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| Ligas de titânio alfa-beta (AB) | |
| Designação do código | Composição |
| AB-1 | 6A1-4V |
| AB-2 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2,5V |
| AB-6 | 8Mn |
| Ligas de titânio beta(B) | |
| Designação do código | Composição |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| Processamento: | |
| Laminagem a quente | Laminagem a frio |
| Graus disponíveis: | |
| PC Grau 1 | Grau 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| PC Grau 2 | Grau 6Al-4V ELI (antigo Grau 23) |
| Grau 7 | Grau 6Al-6V-2Sn (6-62) |
| Grau 19 | Grau 8Al-1Mo-1V (8-1-1) |
| Grau 5 (6Al-4V) | Grau 9 (3Al-2,5V) |
| Grau 6 (5Al-2.5Sn) | PC Grau 3 |
| Aplicação | |
| Indústria química | Dessalinização da água do mar |
| Indústria petroquímica | Aeroespacial |
| Domínio da maquinagem, domínio automóvel | Componente de telemóvel Campo. |
| Titanium Grade 2 Hex Bar | Titanium Gr 2 Hex Bar |
| Grade 2 Titanium Hexagonal Bar | |
| Gr 2 Titanium Alloy Hex Bar | |
| UNS R50400 Titanium Hexagonal Bar | |
| ASTM B348 Grade 2 Titanium Hex Bar | |
| Titanium Alloy Grade 2 Square Bar | Titanium Grade 2 Square Bar |
| Grade 2 Titanium Square Bars | |
| Gr 2Titanium Alloy Square Bar | |
| UNS R50400 Titanium Square Bar | |
| WERKSTOFF NR. 3.7035 Barra Quadrada | |
| ASTM B348 Gr 2 Titanium Square Bars | |
| Titanium Grade 2 Rectangular Bar | Titanium Grade 2 Rectangular Bar |
| Ti. Barras rectangulares de liga Gr2 | |
| Gr 2 Titanium Alloy Rectangular Bar | |
| UNS R50400 Titanium Rectangular Bars | |
| WERKSTOFF NR. 3.7035 Barra retangular | |
| ASTM B348 Gr 2 Titanium Rectangular Bar | |
| Titanium Grade 2 Flat Bars | Titanium Grade 2 Flat Bar |
| Gr 2Titanium Alloy Flat Bars | |
| Titanium Gr 2Flat Bars | |
| UNS R50400 Titanium Flat Bars | |
| WERKSTOFF NR. 3.7035 Barras planas | |
| ASTM B348 Gr 2 Titanium Flat Bars | |
| Titanium Grade 2 Polished Bar | Titanium Grade 2 Polished Bar |
| Grade 2Titanium Polished Bars | |
| Gr 2Titanium Alloy Polished Bar | |
| UNS R50400 Titanium Polished Bars | |
| WERKSTOFF NR. 3.7035 Barra Polida | |
| ASTM B348 Gr 2 Titanium Polished Bar | |
| Titanium Grade 2 Threaded Bar | Titanium Gr 2 Threaded Bar |
| Grade 2Titanium Threaded Bars | |
| Ti. Alloy Grade 2 Threaded Bar | |
| UNS R50400 Titanium Threaded Bar | |
| WERKSTOFF NR. 3.7035 Barra roscada | |
| ASTM B348 Gr 2 Titanium Threaded Bar |
| TAMANHO NOMINAL | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| DIÂMETRO mm | ||||||||
| ~ a 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| de 3 a 6 anos | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| mais de 6 a 10 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| mais de 10 a 18 anos | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| mais de 18 a 30 anos | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| mais de 30 a 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| mais de 50 a 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| mais de 80 a 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| mais de 120 a 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| mais de 180 a 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
2nd grade bar type (3)
Informações disponíveis para consulta e descarregamento
Haste de titânio
Daxun is a trustworthy titanium rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the Titanium rod have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Produtos e projectos recentes de casos quentes
Produtos relacionados (8)
What are Grade 2 Titanium rods?
Ti CP Grade 2 has greater tolerated levels of iron and oxygen and is frequently utilized due to its outstanding formability, moderate strength, and superior corrosion resistance. It has a minimum yield strength of 275 Mpa (40 ksi) and relatively low amounts of impurity elements, placing it in the strength range of Grades 1 to 3.
Grade 2 Titanium Rod Equivalent Grade
| nation | name | usually |
| Russia | VT1-0 (VT1-0) | Gorst 19807-91 |
| Germany | 3.7035 | Job Number (3.7035) |
| Europe | Titanium Grade 2 | ZH-10204 3.1 |
| Japan | Titanium Grade 2 | JIS H 4600 |
| People’s Republic of China | TA2 | GB/T 3621-2007 / GB/T 13810-2007 |
| USA | Titanium Grade 2 | ASTM B348 / B265 / B337,UNS R50400 |
Resistência à corrosão
Commercially pure (CP) titanium offers remarkable resistance to crevice corrosion in salt solutions, outperforming stainless steel. It retains its integrity against crevice corrosion at temperatures under 80 °C (176 °F), regardless of pH levels, even in environments with high chlorine concentrations.
Stress Corrosion Cracking (SCC)
Grade 2 titanium exhibits remarkable resistance to stress corrosion cracking. It performs exceptionally well in hot chloride solutions and is entirely immune to SCC in seawater, making it a dependable material for harsh environments.
Erosion Corrosion
Titanium exhibits exceptional durability in flowing seawater, withstanding velocities as high as 130 ft/sec (40 m/sec) without significant degradation. Even in the presence of abrasive particles like sand, its corrosion resistance remains largely unaffected, highlighting its reliability in demanding environments.
Hydrogen Embrittlement
When exposed to seawater, titanium absorbs minimal hydrogen, even at higher temperatures. However, absorption typically takes place only under certain specific conditions:
- pH levels below 3 or above 12
- Temperatures exceeding 80 °C (176 °F)
- A mechanism for hydrogen generation, such as galvanic coupling or an impressed current.
Bio-Corrosion
Titanium alloys exhibit complete immunity to microbiologically influenced corrosion. However, because they are non-toxic to marine organisms, biofouling can develop in seawater. This can be effectively managed through chlorination or by increasing the flow rate of water through heat exchangers.
Corrosion Fatigue
Unlike many materials, titanium maintains its fatigue performance in seawater. Fatigue endurance limits and crack growth rates are consistent, whether tested in air or seawater, making it a reliable choice for marine applications.
Galvanic Corrosion
Titanium ranks among the noble materials in the galvanic series, positioned near stainless steels, and generally serves as the cathode when paired with other metals. As a result, titanium remains resistant to galvanic corrosion but can increase corrosion in less noble metals. When paired with more noble substances, such as graphite, its passive properties become even stronger.
Fatigue Properties
Grade 2 Titanium Rod maintains its exceptional fatigue properties even in seawater. Its fatigue endurance limits and crack growth rates remain unchanged regardless of whether testing occurs in air or seawater, highlighting its consistent performance under varied conditions.
Soldabilidade
CP2 Grade Titanium Rod is highly weldable when appropriate precautions are observed. Given its reactive nature, an inert gas shield must protect both the outer diameter (OD) and inner diameter (ID) during welding. Additionally, the rod should be completely free of grease or oil to ensure optimal weld integrity.
Grade 2 Titanium Rod is most often welded using either manual or automatic TIG methods, with or without filler wire. A low heat input is advised to limit the size of the heat-affected zone. Post-weld heat treatment is generally not required, simplifying the process while maintaining the rod’s key properties.
This revised version maintains the technical depth and original structure while improving clarity, readability, and flow. Let me know if you’d like further refinements!
| Working material: | 3.7035 / UNS R50400 |
| Diameter: | 3 – 400 mm |
| Lengths: | 2.000 – 4.000 mm |
| Versions: | Rolled, forged, annealed |
| Surfaces: | Turned, peeled, polished |
| Standards: | ASTM B 348, ASME SB 348, DIN 17862, ASTM F 67, NACE MR 0175, ISO 1515156-3, ISO 5832-2 |
Buy Grade 2 Titanium Rods/Rounds at Daxun
Are you in need of round rod material made from Grade 2 Titanium Alloy Rod-3.7035? At Daxun, we specialize in providing customized titanium rods tailored to your project’s specifications. As an experienced supplier, we are committed to supporting your needs with precision and reliability.
Our Grade 2 Titanium bars are available in diameters ranging from 2.0 mm to 400 mm. Tolerances and execution may vary based on the size of the bar. Smaller diameters are provided centerless ground with h7 tolerances, while larger sizes come with h9 or h11 tolerances. Contact Daxun to discuss your requirements or to request a customized project quote.
Buy Grade 2 Titanium Bars: Features and Specifications.
- Forged bars can be peeled or pre-machined. The material is available in a variety of specifications depending on the application and market needs.
- Our titanium bars typically meet various requirements and certifications, including ASTM B348 and ASTM F 67, DIN 17860, VD TÜV Table 230-3, and Nace MR 0175.
- Titanium round bars are often used where they have excellent corrosion resistance and good mechanical properties.
- Grade 2 titanium bars (3,7035) are therefore suitable for use as a construction material for equipment and devices, as they are easy to process.
Os nossos serviços de material de barras de titânio
- Como um centro de serviços experiente, podemos adaptar o seu material em barra de titânio às suas especificações, trabalhar com vários organismos de certificação, como a TÜV Rheinland ou a DNV, para aprovar as especificações e iniciar a atualização de produtos semi-acabados de titânio para satisfazer as aplicações adequadas.
- Teremos todo o gosto em fornecer-lhe uma consulta e explicar-lhe tudo o que precisa de saber sobre a obtenção de material de barras de titânio, incluindo quais as normas que requerem maior atenção para os componentes a fabricar.
- Se tiver um compromisso de fornecimento a longo prazo, pode estabelecer um acordo-quadro com a Daxun. Garantimos preços e quantidades durante um determinado período.
- Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about the Grade 2 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
Informações para encomenda
When placing a purchase order, make sure to include the quantity, grade, type or category, API5L reference, as well as the thickness, width, and length of the product. If you have any specific requirements, like chemical composition, mechanical properties, heat treatment, additional testing, manufacturing methods, surface coatings, or end finishes, let us know so we can meet your needs.
Feel free to contact Daxun with your order details. We are committed to responding to your inquiry promptly.
O tipo de liga de titânio de que necessita depende do projeto em que está a trabalhar, uma vez que cada tipo tem benefícios diferentes.
Todos os graus de liga de titânio são extremamente fortes e resistentes à corrosão, o que significa que continuarão a funcionar bem nas condições mais adversas.
Os graus mais elevados de liga de titânio (5-12) são ligas concebidas para benefícios específicos. Por exemplo, a liga de titânio de grau 12 tem uma excelente resistência ao calor, o que a torna uma escolha perfeita para permutadores de calor de casco e tubo, tubagens hidráulicas e equipamento da indústria química.
Os graus 1-4 são ligas de titânio puro e são a escolha perfeita se precisar de um material soldável e dúctil para sistemas de tubagem e tubos. Encontrará graus inferiores utilizados nas indústrias marinha e industrial.
Se está a iniciar um projeto e não tem a certeza de qual o melhor tipo de liga de titânio para si, contacte-nos hoje mesmo; teremos todo o gosto em ajudá-lo.
Na DAXUN, oferecemos uma vasta gama de graus de liga de titânio, do grau 1 ao grau 12.
Os graus 1-4 são titânio puro, enquanto os graus superiores são ligas.
Os tipos de liga são populares pela sua elevada relação resistência/peso.
O grau de liga de titânio mais utilizado que encontramos é o grau 5. Embora continue a ser rica em titânio, esta classe é uma das mais fiáveis porque pode suportar temperaturas até 600°F e resistir a condições extremas.
As qualidades superiores são preferidas por indústrias como a aeroespacial e a marítima devido à sua resistência ao desgaste e à corrosão.
Por outro lado, os graus inferiores são utilizados principalmente para soldadura devido à sua menor resistência.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
Embora o grau de titânio aumente ligeiramente o custo, o custo total é determinado principalmente pela forma e pelo formato do titânio que pretende.
At DAXUN, we offer a wide range of titanium products, including rod/bars, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
Infelizmente, é difícil apresentar um preço online sem saber muito sobre o seu projeto e para que será utilizado o titânio.
Felizmente, a nossa equipa de especialistas está sempre aqui para o ajudar e aconselhar nas suas necessidades de titânio. Ao enviar um e-mail para [email protected], poderemos responder-lhe com alguns conselhos e um orçamento exato.
Certifique-se de que inclui o máximo de informação possível sobre o grau, a forma e a quantidade de titânio de que necessita para compreender melhor as suas necessidades.
A equipa da DAXUN é experiente, conhecedora e simpática. Com anos de experiência no sector, sabem tudo sobre o titânio, incluindo as suas utilizações, benefícios e graus.
Para obter actualizações regulares sobre o titânio, as suas utilizações e as suas aplicações em todas as indústrias, não deixe de consultar o nosso blogue. Os nossos especialistas escreveram guias fáceis de seguir que pode consultar sempre que tiver dúvidas.
Se continuar a ter problemas, não hesite em contactar-nos; teremos todo o gosto em ajudar.
Ao enviar uma mensagem de correio eletrónico para [email protected], receberá uma resposta rápida. Certifique-se de que inclui o máximo de pormenores possível na sua pergunta para que possamos recomendar uma solução adequada.
Preencha o formulário na página “Contacte-nos” ou ligue para o nosso gestor de vendas através do número “+86 13382898899” e entraremos em contacto consigo o mais rapidamente possível. O nosso WhatsApp está online e o e-mail ([email protected]) será verificado no prazo de 6 horas. Todas as perguntas ou mensagens serão respondidas prontamente. Além disso, todas as semanas partilhamos informações de mercado com os nossos clientes
We can provide Titanium rod. samples for you to check the quality. Sample is free and you just pay the freight.
Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.
Our MOQ is 1 ton for Titanium rod.
As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.