Super Austenitic 904L Stainless Steel Plate Supplier
As China’s leading stainless steel plate supplier and exporter, Daxun provides 904L stainless steel plates to the world.
- Grade: AISI 904L-N08904
- Features: Super corrosion resistance
- Manufacturing: Cold-rolled plate, hot-rolled plate, forged plate
- Normas: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type: Cold-rolled thin plate, hot-rolled thick plate
- Superfície: 2B, NO.1, NO.4, HL, BA, 8K, etc.
- Comprimento: 2438mm3048mm6000mm pode ser personalizado
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong, ATI,
Overview of 904L Stainless Steel
Alloy 904L is a superaustenitic stainless steel designed for moderate to high corrosion resistance in various process environments. This high alloy austenitic product is intended for use under severely corrosive conditions, making it a reliable choice for demanding applications. The high chromium and nickel content, along with the additions of molybdenum and copper, provide excellent corrosion resistance. With a highly alloyed chemistry that includes 25% nickel and 4.5% molybdenum, Alloy 904L is well-suited for applications requiring both high corrosion resistance and high strength. This unique composition allows it to withstand environments involving dilute sulfuric acid, hot phosphoric acid, and other inorganic acids, ensuring long-lasting performance in harsh conditions.
Dimensions and Sizes
Alloy 904L stainless steel plate is available in various dimensions and sizes to meet specific application requirements. The available thicknesses for Alloy 904L range from 3/16” through 2”, providing flexibility for different industrial needs. UNS N08904 Sheet can range up to 8mm in thickness, while 904L Plate is usually thicker than 8mm and can range up to 75mm in thickness. These dimensions can be customized to meet specific industry standards and specifications, ensuring that the material fits perfectly into any project. Additionally, 904L stainless steel plate can be easily welded and processed using standard shop fabrication practices, streamlining the manufacturing process and ensuring high-quality results.
Dados técnicos
- Parâmetro
- Composições químicas
- Propriedades mecânicas
- PROPRIEDADES FÍSICAS
- Padrão
| Stainless Steel 904L Plate, Sheet and Strip | ASTM B 168/ASME SB 168, ASTM B 906/ASME SB 906, ASME Code Cases 1827 and N-253, SAE/AMS 5540, BS 3072NA14 and 3073NA14, DIN 17750, ISO 6208, EN 10095, MIL-DTL-23228. |
| Standard Stainless Steel 904L Plate & Sheet Sizes | 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm |
| Cold rolled 904L Steel Plate 0.5-6.4 mm | |
| Hot rolled 904L Steel Plate 3.0–10.0 mm | |
| SS 904L Plate Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard Stainless Steel 904L Sheet suppliers |
| Availability of Stainless Steel 904L Foil sizes | Thickness : 8-100 microns (0.00031-0.004 in) |
| Width: Up to 500 mm (19.5 in) | |
| Weight (in rolls) : Up to 50 kg (110 lb); e.g. approxi- mately 1400 m at 8 microns and ap- proximately 112 m at 100 microns. | |
| Definição de perfis | Para fornecer um serviço completo de definição de perfis na China, utilizamos vários métodos de definição de perfis, incluindo: |
| Laser Plate Cutting | |
| Plasma Plate Cutting | |
| Oxy-propane Flame Cutting | |
| Tolerances of width and thickness | EN 10258 (formerly DIN 59381) |
| EN 10151 Stainless Steel 904L strip for springs | |
| EN 10088 Stainless Steel 904L strip (general) | |
| Stainless Steel 904L Plates standards and approvals | EN ISO 18286 |
| EN 10051 | |
| EN 10088-1 | |
| ISO 15510 | |
| EN ISO 9445 | |
| ASTM A 480 | |
| ASTM A 959 | |
| ASME IID | |
| Perfis plasmáticos | De acordo com os desenhos do cliente |
| Value added services for Stainless Steel 904L Plate | Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing. |
| Value added services for Stainless Steel 904L Coil | Corte no comprimento |
| Corte longitudinal | |
| Polimento | |
| Blanking | |
| SS 904L Plate Origin | China Origin, European Origin, Japanese Origin |
| Packing of 904L Steel Sheet | Bundles with waterproof cloth outside or plywood box |
| Test | UT, SGS testing, TUV etc |
| Elemento | % Present (in product form) |
| Carbono (C) | 0.02 |
| Silício (Si) | 0.7 |
| Manganês (Mn) | 2 |
| Fósforo (P) | 0.03 |
| Enxofre (S) | 0.01 |
| Crómio (Cr) | 19.00 – 21.00 |
| Níquel (Ni) | 24.00 – 26.00 |
| Azoto (N) | 0.15 |
| Molibdénio (Mo) | 4.00 – 5.00 |
| Copper (Cu) | 1.20 – 2.00 |
| Ferro (Fe) | Equilíbrio |
| Product Form | ||||||||
| C | H | P | L | L | TW/TS | |||
| Thickness (mm) Max. | 8 | 13.5 | 75 | 160 | 2502) | 60 | ||
| Yield Strength | Rp0.2聽N/mm2 | 2403) | 2203) | 2203) | 2304) | 2305) | 2306) | |
| Rp1.0聽N/mm2 | 2703) | 2603) | 2603) | 2603) | 2603) | 2503) | ||
| Resistência à tração | Rm聽N/mm2 | 530 – 7303) | 530 – 7303) | 520 – 7203) | 530 – 7304) | 530 – 7305) | 520 – 7206) | |
| Elongation min. in % | Jmin聽(Longitudinal) | - | 100 | 100 | 100 | - | 120 | |
| Jmin聽(Transverse) | - | 60 | 60 | - | 60 | 90 | ||
| Density at 20°C kg/m3 | 8 | |
| Thermal Conductivity W/m K at | 20°C | 12 |
| Modulus of Elasticity kN/mm2 at | 20°C | 195 |
| 200°C | 182 | |
| 400°C | 166 | |
| 500°C | 158 | |
| Specific Thermal Capacity at 20°C J/kg K | 450 | |
| Electrical Resistivity at 20°C Ω mm2/m | 1 | |
| UNS S904L | 1.4539 | UNS N08904 |
| ASTM A240 | ASTM A240 | ASTM A240 |
| ASTM A480 | ASTM A480 | ASTM A480 |
| ASME SA240 | ASME SA240 | ASME SA240 |
| AMS 5521 | AMS 5521 | AMS 5521 |
Escolha a Daxun e deixe os seus clientes satisfeitos.

Entrega rápida
We provide timely and fast delivery of 904L stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
904L plate features
Type 904L is a high alloy austenitic stainless steel that is known for its corrosion properties.
- Não magnético
- Stronger corrosion properties than Type 316L an 317L
- Good resistance to sulphuric, phosphoric and acetic acids
- High resistance to crevice and stress corrosion cracking
- Excellent formability and weldability

Stainless Steel 904L Applications
Application of using Type 904L stainless steel:
- Cooling equipment for seawater
- Chemical processing of sulphuric, phosphoric and acetic acids
- Permutadores de calor
- Condenser tubes
- Gas washing
- Control and instrumentation
- Oil and gas industry
- Pharmaceutical production
- Wiring in electrostatic precipitators
Qualidade, entrega, inspeção
-
Daxun Alloy is committed to quality assurance. The company conducts various tests to ensure material suitability. These tests include flattening, pitting, and resistance tests. Mechanical, hardness, and expansion tests are also performed. Material positive identification is another key quality assurance measure. All these tests guarantee that the materials meet application requirements. Customers can trust Daxun Alloy for high-quality, suitable products.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
O nosso prazo de entrega está estritamente de acordo com o contrato. - Apoio a agências terceiras do cliente para se deslocarem à fábrica para inspeção
- Apoio a amostras gratuitas aos clientes para testes
- Apoio à inspeção de fábrica no local ou por vídeo

Technical Services
Se necessitar de qualquer assistência técnica adicional, o nosso metalúrgico residente e a nossa equipa experiente terão todo o prazer em ajudar. Além disso, a Daxun possui um laboratório de testes certificado - o primeiro na indústria de inventário de multi-metal e plástico. Isto, na nossa opinião, demonstra a nossa dedicação inabalável à qualidade e a nossa filosofia como um fornecedor de serviço completo.
Maquinação avançada
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of the variety, specification, and origin of each stainless steel plate, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.
904L plate stainless steel Features
Daxun Deixe a sua marca melhorar rapidamente
- Galeria
- Tolerância
- Estado de entrega
- Outras séries de produtos
| Tolerância para chapa 2B | |||
| Tamanho | Classificação de tolerância | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Tolerância para chapa laminada a quente n.º 1 | |||
| Tamanho | Classificação de tolerância | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Entrega Estado Escolha | Estado da superfície |
| Laminados a frio | 2B |
| 2D | |
| BA | |
| Fio de cabelo | |
| N.º 3 | |
| N.º 4 | |
| 6K | |
| 8K | |
| Nota: | |
| 1. Se necessitar de um estado de entrega diferente do acima indicado, por favor confirme connosco. | |
| 2. Em caso de pedido de informação ou de encomenda, agradecemos que nos informe de qualquer requisito adicional não indicado aqui. | |
| Estado de entrega | |
| Entrega Estado Escolha | Estado da superfície |
| Laminados a quente | N.º 1 |
| N.º 3 | |
| N.º 4 | |
| 6K | |
| 8K | |
| Em conserva | |
| Nota: | |
| 1. Se necessitar de um estado de entrega diferente do acima indicado, por favor confirme connosco. | |
| 2. Em caso de pedido de informação ou de encomenda, agradecemos que nos informe de qualquer requisito adicional não indicado aqui. | |
| Grau | Tipo | Espessura | Superfície |
| Austenítico | 304/304H/304L/304J1 | 0,25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrite ultra-puro | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Grau | Tipo | Espessura | Original |
| Aço resistente ao calor | 309S | 0,5-40mm | CHN |
| 310S | 0,5-40mm | CHN | |
| Aço duplex | 2101 | 1,5-50 mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0,5-60mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Aço superaustenítico | N08904 | 0,6-50mm | SWE / JPN / CHN |
| S31254 | 0,5-50mm | SWE / JPN / CHN | |
| N08926 | 0,5-50mm | SWE / JPN / CHN | |
| N08367 | 0,5-50mm | SWE / JPN / CHN | |
| Liga à base de níquel | N08031 | 1.0-50mm | EUA / JPN / GER |
| N08810/N08800 | 0,8-50mm | EUA / JPN / CHN | |
| N08028 | 1,0-20mm | EUA / GER / JPN | |
| N08020 | 1,0-20mm | EUA / GER / JPN | |
| N08825 | 0,8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50mm | EUA / GER / JPN | |
| N06022 | 1.0-50mm | EUA / GER / JPN | |
| N06625 | 0,8-20mm | EUA / GER / CHN | |
| N04400 | 1,0-20mm | EUA / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20mm | EUA / JPN | |
| Titânio | TA1/Gr1 | 0,5-50mm | JPN / CHN |
| TA2/Gr2 | 0,5-50mm | JPN / CHN | |
| Material de soldadura | ERNiCrMo-13 | 1.2、2.4mm | ALEMANHA |
| ERNiCrMo-3 | 2,4 mm | ALEMANHA | |
| ERNiCrMo-4 | 2,4 mm | EUA |
The surface and shape of 904L stainless steel plate (7)
Informações disponíveis para consulta e descarregamento
Daxun é um fabricante confiável de chapa de aço inoxidável
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Produtos e projectos recentes de casos quentes
Produtos relacionados (13)
Podemos fornecer amostras de chapas de aço inoxidável para que possa verificar a qualidade. A amostra é grátis e o cliente só paga o frete.
Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.
O nosso MOQ é de 1 tonelada para chapas de aço inoxidável.
As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.