Daxun is an excellent manufacturer of CP Grade 3 titanium rods and bars.

  • Titanium bar grade: R50550 / CP TI50A
  • Titanium bar types: rolled bars, drawn bars, forged titanium bars
  • Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.

The global leader in commercially titanium alloy rod manufacturing services

Daxun, specializing in the production of alloy titanium rods for extreme environments

As the strongest of the CP grades, Grade 3 offers an outstanding combination of high tensile strength, excellent corrosion resistance, and good formability. This makes it an ideal material for demanding industrial applications where both durability and fabricability are paramount.This titanium grade provides superior strength compared to CP Grade 2, making it perfect for components that must withstand higher mechanical stresses. Its exceptional corrosion resistance ensures longevity in harsh environments, including seawater, chlorides, and oxidizing acids. The material features excellent weldability using standard techniques, allowing for easy fabrication and assembly, while maintaining good formability for bending and machining into complex shapes. Despite its strength, it retains titanium’s characteristic lightweight properties, contributing to overall weight reduction in final assemblies.

主な用途:

CP Grade 3 titanium bar finds extensive use across critical industries. In chemical processing, it’s trusted for heat exchangers, pressure vessels, and piping systems. The aerospace sector relies on it for airframe and jet engine components, fasteners, and brackets. Marine engineering applications include desalination plant components, propeller shafts, and offshore hardware. Power generation facilities utilize it for condenser and heat exchanger tubing, while the medical industry values it for surgical implants and instruments where high strength is essential.

Key Properties & Advantages:

  • Superior Strength: Significantly stronger than CP Grade 2, making it suitable for components that must withstand higher mechanical stresses.
  • 卓越した耐食性: Highly resistant to corrosion in a wide range of environments, including seawater, chlorides, and oxidizing acids.
  • Excellent Weldability: Can be readily welded using standard techniques, ensuring ease of fabrication and assembly.
  • Good Formability: Offers better ductility than many titanium alloys, allowing for bending, forming, and machining into complex shapes.
  • Lightweight: Retains the characteristic low density of titanium, contributing to overall weight reduction in final assemblies.
仕様 詳細
素材 CP Grade 3 Titanium Bar
スタンダード ASTM B348, AMS 4921
寸法 EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
直径範囲 0.125″ – 14″ (3.175mm – 355.6mm), custom
長さの範囲 Up to 240″ (6096mm), custom
様式 Round Bar, Square Bar, Hexagonal Bar
表面仕上げ 冷間引抜、センタレス研磨、ポリッシュ、ラフ切削、黒色、NO.4仕上げ、BA仕上げ、マット仕上げ等。.
コンディション 焼入れ、焼戻し、アニール
寛容 Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
様式 チタン角棒、チタンインゴット、チタン丸棒、チタン角棒、チタン三角棒、鍛造チタン棒、チタン六角棒など。.

大順合金 supply CP Grade 3 titanium bar sourced from premier mills, ensuring every piece meets stringent international standards for quality and consistency. Our material is fully certified and available in a wide range of sizes, with custom cutting services to meet your exact project specifications. Contact our expert team today for a competitive quote and personalized service for your titanium requirements.

続きを読む

データ

エレメント Content (%)
チタン (Ti)
Balance (~99.1%)
Oxygen (O) 0.10 – 0.27
鉄(Fe) ≤ 0.30
Carbon © ≤ 0.10
窒素(N) ≤ 0.05
Hydrogen (H) ≤ 0.015
プロパティ 価値
引張強度
~450–485 MPa
降伏強度
~380–415 MPa
伸び ~20–30%
硬度(ブリネル)
~200–240 HB
プロパティ 価値
密度 ~4.51 g/cm³
融点
~1660–1670 °C
弾性係数
~103–107 GPa
熱伝導率
~21.9 W/m·K (at 25°C)
電気抵抗率 ~420 nΩ·m

Daxunを選んで、あなたのプロジェクトを成功に導きましょう。.

今すぐDaxunに連絡する

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

今すぐDaxunに連絡する

CP Grade 3 Titanium Rod Production Method

Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
今すぐDaxunに連絡する

品質、納期、検査

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the CP Grade 3 Titanium Rod and CP Grade 3 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • 当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • 顧客テストのための無料サンプルをサポート
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

パッケージング

国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス

今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

Daxun CP Grade 3 Titanium Rods help your brand improve quickly

NOMINAL SIZE
h5
h6
h7
h8
h9
H10
H11
h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

チタン棒

最近の注目プロジェクトと製品

What is the difference between CP Grade 3 and the more common CP Grade 2? Which one should I choose?

CP Grade 3 is the strongest of the commercially pure titanium grades, offering approximately 20-30% higher tensile strength than Grade 2. You should choose Grade 3 when your application demands higher mechanical strength and pressure resistance. However, CP Grade 2 is slightly more formable, weldable, and typically more cost-effective. The simple rule is: Choose Grade 3 for strength, and Grade 2 for better formability and value.

Is CP Grade 3 titanium bar easy to machine?

Machining CP Grade 3 requires following standard practices for titanium. It demands slower cutting speeds, higher feed rates, and ample coolant compared to steel. Using sharp carbide tools and maintaining a constant cut to avoid work hardening is key. While it machines slower than steel, it can be precisely fabricated into complex shapes with the right equipment and techniques.

How good is the corrosion resistance of CP Grade 3?

Its corrosion resistance is exceptional, particularly in oxidizing environments like seawater, salt spray, and chloride solutions. It forms a stable, passive oxide film that protects it from most forms of corrosion, including pitting and crevice corrosion, making it a premier choice for the chemical processing and marine industries.

Do your titanium bars meet industry standards and come with certification?

Absolutely. All our CP Grade 3 titanium bars comply with international standards such as ASTM B348 そして AMS 4921. Every shipment is accompanied by a full Material Test Report (MTR) / mill certification, verifying its chemical composition and mechanical properties for your complete peace of mind.

早急に見積もりを取る、あるいはマーケット情報を理解するには?

お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール([email protected])は6時間以内に確認いたします。すべてのお問い合わせやメッセージに迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。

サンプルをいただけますか?

We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ
クイック見積もり