Daxun is a 310S stainless steel sheet supplier from China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 310S stainless steel plates to the world.
- Grade: AISI 310-310S-S31008
- 製造:冷延板、熱延板、鍛造板
- 規格ASM、ASME、GB、DIN、JIS、ISO、EN、BS
- 種類:冷間圧延薄板、熱間圧延厚板
- 表面: 2B、NO.1、NO.4、HL、BA、8K、等。.
- 長さ: 2438mm3048mm6000mm はカスタマイズすることができます
- Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong
The global leader in stainless steel sheet fabrication services
S31008 (310S) Sheet and Plate, Austenitic stainless steel alloy 310S (UNS S31008) is designed for applications requiring high-temperature corrosion resistance. The alloy resists oxidation up to 2010°F (1100°C) with room temperature cycling. Alloy 310 can be used in moderate carburizing environments and is resistant to sulfidation due to its high chromium content and moderate nickel content. More severe carburizing environments in heat-treating equipment typically require a nickel alloy such as 330 (UNS N08330). Alloy 310S can be used in bonding, nitriding, mild oxidation, and thermal cycling processes; however, a reduced maximum service temperature is required. Alloy 310 can also be used in cryogenic applications because it has low magnetic permeability and remains strong down to -450°F (-268°C). When heated to 1202–1742, the alloy precipitates the sigma phase (650–950°C). Hardness is partially restored by solution annealing at 2012–2102°F (1100–1150°C). This alloy is also available as a low-carbon alloy, 310S (UNS S31008). It is easily fabricated. A high carbon modification, 310H (UNS S31009), is designed to improve creep resistance. In most cases, the grain size and carbon content of the plate can meet both 310S and 310H standards. Standard shop fabrication procedures can be used to easily weld and process alloy 310.
Stainless Steel 310S Plate has trace amounts of silicon, sulfur, phosphorus, manganese, and up to 24% chromium, 19% nickel, and up to 0.08% carbon. Heat resistance, corrosion resistance, strength, and even high-temperature oxidation resistance are just a few of the many benefits of this popular stainless steel alloy. It can be utilized in many different applications, including burners, oil burners, and evaporator pipes and tubes. Because of its affordability, it’s perfect for a range of applications requiring low-cost maintenance supplies.
Because of its exceptional resilience to high temperatures, the 310S stainless steel plate is a great option for a wide range of industries, including petrochemical and chemical production, food processing, power plants, dairy farms, sugar mills, breweries, and energy generation. 310S Stainless Steel Plate is capable of withstanding oxidizing environments up to 2100°F (1149°C) due to its high chromium concentration. Its ductility, toughness, and weldability are all excellent. Its exceptional low-temperature performance, even down to -20°F (-29°C), combined with its resistance to heat and corrosion make it the perfect material for cryogenic applications. In conclusion, it is an excellent option for high-temperature industrial applications due to its strong resistance to oxidation and ability to prevent scaling at temperatures as high as 2000°F (1093°C).
技術データ
- パラメータ
- エレメント
- 機械的性質
- スタンダード
| Product Parameters: 310(UNS S31008) Stainless Steel Sheet/Plate | |||
| 幅 | 10mm~2500mm | ||
| 厚さ | 0.2mm~100mm | 厚さ公差 | ±0.03mm |
| スタンダード | ASM/ASM240/480、JIS4305、DIN EN 10088-2 | ||
| 表面 | 2B、BA、8K、NO.1、NO.4、NO.3、ヘアライン、チェック、ゴールド、ブラック、ローズゴールドなど | ||
| スペック | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| ミル・オリジン | TISCO、ZPSS、BAOSTEEL、JISCO、ZSESS、ATI、SMC、HAYNES、VDM、ArcelorMittal、Outokumpuなど。. | ||
| 認証 | ISO、SGS、BV、TUV、CE など | ||
| エレメント | % Present (in product form) | |
| C, H, P, L | TW* / TS* | |
| カーボン(C) | ≤0.10 | ≤0.15 |
| ケイ素 (Si) | ≤1.50 | ≤0.75 |
| マンガン (Mn) | ≤2.00 | ≤2.00 |
| リン (P) | ≤0.045 | ≤0.045 |
| Sulfur (S) | ≤0.015 | ≤0.030 |
| クロム(Cr) | 24.00 – 26.00 | 24.00 – 26.00 |
| ニッケル(Ni) | 19.00 – 22.00 | 19.00 – 22.00 |
| 窒素(N) | ≤0.11 | – |
| 鉄(Fe) | バランス | バランス |
| Product Form | |||||
| C, H, P | L | TW* / TS* | |||
| Thickness a or diamter d (mm) | a ≤ 12 | d ≤ 25 | – | ||
| Hardness HB max. 1) 2) 3) | 192 | 192 | – | ||
| Proof Strength3) | Rp0.2 N/mm2 | 210 | 210 | 230 | |
| Rp1.0 N/mm2 | 230 | 230 | 270 | ||
| 引張強度 | Rm N/mm2 | 500 – 700 | 500 – 700 | min. 500 | |
| Elongation min. in % | Long Products | 351) | 351) | 334) / 355) | |
| Flat Products | 0.5 ≤ a/d < 3 | 334)5) | 334)5) | 354)5)6) | |
| 3 ≤ a/d | 354)5) | 354)5) | 354)5)6) | ||
| 310 | 310S | 310H |
|---|---|---|
| UNS S31000 | UNS S31008 | UNS S31009 |
| ASTM A240 | ASTM A240 | ASTM A240 |
| ASTM A480 | ASTM A480 | ASTM A480 |
| ASME SA240 | ASME SA240 | ASME SA240 |
| AMS 5521 | AMS 5521 | AMS 5521 |
Daxunを選択し、顧客を満足させる。.

迅速な配達
We provide timely and fast delivery of 310S stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Benefits of Stainless Steel 310S Plates :
- Corrosion resistance: The main benefit of 310S stainless steel plates is their excellent corrosion resistance. They resist corrosion from a wide range of environments, including acidic and alkaline solutions, making them suitable for a wide range of applications.
- High-temperature strength: 310S stainless steel plates exhibit excellent strength at elevated temperatures. This property is critical in applications that are frequently exposed to high temperatures, ensuring structural integrity and performance in demanding conditions.
- Durability and lifespan: The durability of 310S stainless steel plates gives them a long service life, making them an affordable choice for many applications. The material is resistant to wear and tear, minimizing the need for frequent replacement.

Benefits of Stainless Steel 310S Plates :
310S/2520 Plate Features:
- High-temperature resistance
- 優れた耐酸化性
- Improved creep/rupture properties
- 優れた耐食性
- Not susceptible to thermal fatigue and cyclic heating
- Good strength at temperatures up to 2100°F
品質、納期、検査
- Daxunは厳格に製品の品質を管理しています。ご注文の前に、製品保証書をお送りします。また、テスト用のサンプルが必要な場合は、無料でサンプルをお送りすることもできます。.
- During the production process, we carefully measure the diameter, thickness, and surface quality of each product to ensure it meets exacting standards. Our standard delivery time is typically 7 to 15 days. However, for special-sized products, the delivery time may be extended to 20 days to accommodate the additional customization and processing required.
当社の納期は、契約に厳密に従います。. - 顧客の第三者機関が工場に検査に行くのをサポートする。
- テスト用の無料サンプルを顧客に提供
- 現場検査またはビデオ工場検査をサポート

アプリケーション
- Cryogenic Components: Designed to withstand extremely low temperatures, ensuring optimal performance in critical applications.
- Food Processing: Reliable materials and components tailored for hygienic and efficient food production systems.
- Furnaces: Durable solutions for burners, doors, fans, ducting, and liners, supporting high-temperature industrial processes.
- Fluidized Bed Furnaces: Robust components including coal burners, grates, ducting, and bellows for enhanced operational efficiency.
- Ore Processing and Steel Mills: High-performance equipment for smelting, steelmaking, and continuous casting operations.
- Petroleum Refining: Specialized systems such as catalytic recovery units, flares, heat exchangers, and tube hangers for maximum efficiency in refining processes.
- Power Generation: Precision-engineered components like gas furnace internals, pulverized coal burners, and tube hangers to support energy production.
- Sintering and Cement Plants: Reliable burners, burner hoods, feed and discharge systems, and bellows for seamless operation in harsh environments.
- Heat Treating: Advanced solutions, including annealing covers and boxes, burner grates, doors, fans, muffle furnaces, retorts, heat exchangers, and walking beams for consistent performance in thermal processing.
SS 310S Plate Surface Treatment
1D: The surface is matte with a discontinuous particle shape.
2D:シルバーがかった白。.
2B: Silver gray with better gloss and flatness than the 2D surface.
バ:鏡面に近く、光沢と反射性に優れる。.
No.3:光沢が良く、表面が粗い。.
No.4:表面に細かい線があり、光沢がある。.
HL:シルバーグレーに金色の髪。.
8K:鏡面。.
310 plate stainless steel Features
Daxun ブランドを急速に向上させる
- ギャラリー
- 寛容
- 配送状態
- その他の製品シリーズ
| 2Bシートの公差 | |||
| サイズ | 寛容度ランク | ||
| グループ1 | グループ2 | グループ3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| No.1熱延板の公差 | |||
| サイズ | 寛容度ランク | ||
| グループ1 | グループ2 | グループ3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| デリバリー・ステートの選択 | 表面状態 |
| 冷間圧延 | 2B |
| 2D | |
| 文学士 | |
| ヘアライン | |
| 第3位 | |
| 第4位 | |
| 6K | |
| 8K | |
| 注: | |
| 1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。. | |
| 2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。. | |
| 配信状態 | |
| デリバリー・ステートの選択 | 表面状態 |
| 熱間圧延 | 第1位 |
| 第3位 | |
| 第4位 | |
| 6K | |
| 8K | |
| ピクルス | |
| 注: | |
| 1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。. | |
| 2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。. | |
| グレード | タイプ | 厚さ | 表面 |
| オーステナイト系 | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/4番/8K/SB/HL/1番 |
| 321 | 0.4-80mm | 2B/BA/4番/8K/SB/HL/1番 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/4番/8K/SB/HL/1番 | |
| フェライト | 430 | 0.4-3.0mm | 2b/ba/no.4/8k/sb/hl |
| 超高純度フェライト | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
| 409L | 0.4-2.5mm | 2B、2D | |
| グレード | タイプ | 厚さ | オリジナル |
| 耐熱鋼 | 309S | 0.5-40mm | 中国 |
| 310S | 0.5-40mm | 中国 | |
| 二相鋼 | 2101 | 1.5-50mm | 中国 |
| 2304 | 3.0-50mm | 中国 | |
| 2205 | 0.5-60mm | 中国 | |
| 2507 | 1.0-60mm | スイス/日本/中国 | |
| スーパーオーステナイト鋼 | N08904 | 0.6-50mm | スイス/日本/中国 |
| S31254 | 0.5-50mm | スイス/日本/中国 | |
| N08926 | 0.5-50mm | スイス/日本/中国 | |
| N08367 | 0.5-50mm | スイス/日本/中国 | |
| ニッケル基合金 | N08031 | 1.0-50mm | アメリカ / 日本 / ドイツ |
| N08810/N08800 | 0.8-50mm | アメリカ / 日本 / 中国 | |
| N08028 | 1.0-20mm | アメリカ / ドイツ / 日本 | |
| N08020 | 1.0-20mm | アメリカ / ドイツ / 日本 | |
| N08825 | 0.8-40mm | アメリカ / ドイツ / スイス / 日本 / 中国 | |
| N10276 | 0.5-50mm | アメリカ / ドイツ / 日本 | |
| N06022 | 1.0-50mm | アメリカ / ドイツ / 日本 | |
| N06625 | 0.8-20mm | アメリカ / ドイツ / 中国 | |
| N04400 | 1.0-20mm | アメリカ / ドイツ / 日本 | |
| N06600 | 1.0-50mm | アメリカ / ドイツ / 日本 / 中国 | |
| N02201 | 0.5-20mm | アメリカ / 日本 | |
| チタン | TA1/Gr1 | 0.5-50mm | 日本 / 中国 |
| TA2/Gr2 | 0.5-50mm | 日本 / 中国 | |
| 溶接材料 | ERNiCrMo-13 | 1.2、2.4mm | ドイツ |
| ERNiCrMo-3 | 2.4mm | ドイツ | |
| ERNiCrMo-4 | 2.4mm | 米国 |
The surface and shape of 310S stainless steel plate (7)
参照およびダウンロード可能な情報
Daxunは信頼できるステンレス鋼板メーカーです。
Daxunは専門メーカーとして、生産するすべての製品が高品質であることを保証します。そのため、すべてのステンレス鋼板はISO9001、SGS、CE、OQCなどの国際品質規格の認証を取得しています。また、ステンレス鋼板の欠陥が少ないことを保証するために、厳格な品質管理を行っています。Daxunでは、すべての製品は、耐久性、高品質、高性能であることをご安心ください。.
最近の注目プロジェクトと製品
関連商品 (13)
私達は質を点検するためにあなたのためのステンレス鋼板のサンプルを提供してもいいです。サンプルは無料で、お客様は運賃を支払うだけです。.
カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.
私達の MOQ はステンレス鋼シートのための 1 トンです。.
トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.