x
お問い合わせ
クイック見積もり

Daxun 310-310S-S31008 stainless steel PIPE and TUBE China supplier

As China’s leading Stainless Steel pipe and tube supplier and exporter, Daxun provides stainless steel PIPEs to the world.
  • Grade: AISI 310S/310-S31008
  • Manufacturing: hot-rolled, cold-drawn, forged, welded
  • 規格ASM、ASME、GB、DIN、JIS、ISO、EN、BS
  • Type: general seamless steel pipe
  • Diameter: from small diameter to large diameter pipe
  • Thickness: thin-walled pipe and thick-walled pipe
  • Surface: pickled AP, polished, bright EP, annealed BA, etc.
  • Length: 3000mm, 6000mm, 9000mm, etc.

Global leader in stainless steel pipe and tube fabrication services

ASTM A312 / A358 Stainless Steel 310 Pipe Supplier, 310S Stainless Steel Seamless Pipe, Call us for ASME SA312 310 Stainless Steel Pipe.

310s grade stainless steel pipes are commercially used in various industries due to their high temperature operation and corrosion resistance in various environmental conditions. 310s grade stainless steel pipes are low carbon alloys that provide temporary operating values ​​up to 1050 degrees Celsius in intermittent services. Daxun Alloys is one of the leading producers, suppliers and stockists of 310s grade stainless steel pipes.

310S Stainless Steel Seamless Pipe | 310S Stainless Steel Seamless Pipe | 310S Stainless Steel ERW Pipe | 310S Stainless Steel EFW Pipe | 310S Stainless Steel Welded Pipe and Tube (Conforming to ASTM A213 / A312 / A269 / A358 Standards)

Type 310S is a low carbon austenitic stainless steel. Type 310S is a low carbon version of Type 310 and is noted for its ability to tolerate high temperature applications. The 310S alloy, like 309S, is best suited for high temperature applications. Both alloys function well in temperatures up to 2000°F, especially where oxidation resistance is necessary. 309 and 310S are the best high temperature performance of the typical stainless grades in our collection. 310S stainless steel has strong corrosion resistance and resists carburization, oxidation, and other conditions. It delivers good performance in industrial grade high temperature situations where great resistance to carburization and thermal cycling corrosion is required. It remains austenitic throughout the full temperature range and does not get embrittled. Its great strength and high temperature oxidation resistance make it valuable in commercial incinerators, kilns and food processing equipment.

続きを読む

データ

Stainless Steel 310 Specification Stainless Steel 310 / 310S, ASTM A312 Stainless Steel
SS UNS S31008 Pipe 310s Stainless Steel Pipe
ASTM A312 TP 310 – 310S SS Seamless Pipe Size 4 to 510mm W. T.: 0.5 to 50mm
WERKSTOFF NR. 1.4841 Welded Pipe Size 5.0 mm – 1219.2 mm
ASTM A312 TP 310 – 310S Stainless Steel EFW Pipe size 5.0 mm – 1219.2 mm
Stainless Steel WERKSTOFF NR. 1.4841 Pipe Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
310 – 310S Stainless Steel Pipe Schedule SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
SS UNS S31008 Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
310s Stainless Steel Tube wall thickness 0.020″ –0.220″, (special wall thicknesses available)
TP310 SS Length Single Random, Double Random, Standard & Cut length Pipe & Tube
ASTM A 358 SS 310 – 310S Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
ASTM A 312 SS 310 – 310S Form Round, Hydraulic, ‘U’ bent or Hollow,LSAW, Boiler, Straight Pipe, Clad Pipe, Rectangular, Square Pipe Etc
Stainless Steel 310 / 310S Type Welded, Seamless, ERW, EFW, Fabricated Pipe, ‘U’ bent or Hollow, Hydraulic, LSAW, Boiler, Straight Tube, Tube Coil, Round, Rectangular, Square Tube etc
TP310 SS End Plain End, Beveled End, Treaded Pipe
ASTM A312 TP 310 – 310S SS Marking All 310s Stainless Steel Pipe are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
SS TP310 – 310S Application Oil Pipe & Tube, Gas Pipe & Tube, Fluid Pipe & Tube, Boiler Pipe & Tube, Heat exchanger Tube
ASTM A312 Stainless Steel Value Added Service Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc.
マーキング All 310s Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
310s stainless steel tubing Testing & Inspection Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing
SS WERKSTOFF NR. 1.4841 Specialize in Alloy 310 / 310S Large Diameter Pipe
Stainless Steel 310 Capillary Tube
Stainless Steel 310S Heat Exchanger &
310 SS Condenser Tube
Stainless Steel 310S Test Certificate Manufacturer Test Certificate
Laboratory Test Certificate from Govt. Approved Lab.
Under Third Party Inspection
Manufacturers of 310 / 310S Stainless Steel Pipe TISCO stainless steel pipes
Baosteel stainless steel pipes
Qingshan stainless steel pipes
ATI stainless steel, USA
Tubacex Tubos Inoxidables S.A., Spain
Schoeller Bleckmann, Austria
Seah Steel Corporation, South Korea
(AS1449 / ASTM A240 – Flat Products)
グレード カーボン Manganese Silicon Phosphorus Sulphur Chromium Nickel
310 0.25 max 2.00 max 1.50 max 0.045 max 0.030 max 24.00 – 26.00 19.00 – 22.00
310S-S31008 0.08 max 2.00 max 1.50 max 0.045 max 0.030 max 24.00 – 26.00 19.00 – 22.00
引張強度 降伏強度
合金 UNS指定 Spec. psi MPa ksi psi MPa ksi Elongation in 2 inches (min.) % Grain Size Req. Maximum Hardness Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity(BTU-in/ft2-h-°F)
310S S31008 A249, A312 75,000 515 75 30,000 205 30 35 90 Rb 29 9.2 116
310H S31009 A249, A312 75,000 515 75 30,000 205 30 35 6 or coarser 90 Rb 29 9.2 116
プロパティ 価値 unit
密度 8,000 kg/m³
Melting Range 1400 – 1450 °C
弾性係数 20°C 200 GPa
せん断弾性率 20°C 77 GPa
ポアソン比 20°C 0.3
熱伝導率 100°C 14.2 W / m. °C
電気抵抗率 25°C 0.78 micro-ohm . m
Electrical Conductivity 25°C 1.25 % IACS
Specific Heat 500 J/kg. °C
Relative Magnetic Permeability 1.02
Coefficient of Expansion 0 – 100°C 15.9 /°C
0 – 315°C 16.2 /°C
0 – 540°C 17 /°C
グレード 中国 UNS No Old British Euronorm Swedish SS Japanese JIS GOST
BS En No 名称
310S 00Cr25Ni20 S31008 304S31 58E 1.4845 X5CrNi18-10 2332 SUS 310S 20Ch23N18
ASTM A312 TP310S Elliptical and Oval Tubes TP310S Pipe
ASTM A213 TP310S Condenser Tube A312 TP 310S pipe
ASTM A269 TP310S straight tube boiler Grade 310S stainless steel pipe
Schedule 10 Type 310S Stainless Steel Pipe Schedule 40 Type 310S Stainless Steel Pipe
SA312 TP310S Seamless Tubing Polished 310S Stainless Steel Tubing
310S Stainless Steel Threaded Pipe SAE 30310S Stainless Steel Rectangular Tube
JIS SUS310S Seamless Tubes 310S SS Round Tube
SS 310S Welded Tubes Seamless pipe 310s
ASTM A312 TP310S Coiled Tubing Stainless Steel Inox 310S Capillary Tubing
ASTM A312 gr TP 310S Aerospace tubes 310S Stainless Steel Pipe
SA213 TP 310S Sighting Tube Type 310S Stainless Steel Polished Pipes
ASTM A249 TP310S Mirror Tube 310S Stainless Steel Seamless Pipe
UNS S31008 Pitot Tube stockist Stainless Steel 310S Seamless Round Tubing
ASTM A358 TP310S Polished Tubing 310S Stainless Steel Ornamental Tube
Stainless Steel 310S Exhaust Pipe 310S Stainless Steel Spiral Pipe
ASME SA213 TP310S Perforated Tube WERKSTOFF NR. 1.4841/1.4845 Flexible Tube
SA 688 TP310S Finned Tube S31008 Stainless Steel Dom Tube
S31008 Stainless Steel U Shaped Tube 310S Stainless Steel Square Tube Mirror Finish
Din 1.4841/1.4845 Material Vacuum Tube WERKSTOFF NR. 1.4841/1.4845 Coaxial Tube
Schedule 40 Type 310S Stainless Steel Pipe SS 310S Needle Tube
310S Stainless Steel Rectangular Pipe 310S Stainless Steel Hypodermic Tubing for Medical Needle
Ultra-High Purity Electropolished Stainless Steel 310S Tube Thin Wall Stainless Steel 310S Tube
Din 1.4841/1.4845 Stainless Steel Annealed Tubing Type 310S Stainless Steel Coil Tubing Heat Exchanger
SAE J405 Uns S31008 Thin Wall Tubing 310S Stainless Steel Metric Tubing
310S Stainless Steel Seamless Square Tubing Large Diameter 310S Stainless Steel Tube
310S Stainless Steel Lined Pipe Corrugated 310S Stainless Steel Tube (CSST) for Gas
Z6 Cn 18.09 Woven Mesh Tube SS 2332 Sweden Stainless Steel Hollow Section
1.4841/1.4845 X 5 Crni 18 10 Instrument Tubing 310S Stainless Steel Square Tubing
High-pressure 310S Stainless Steel Water Pipe Stainless Steel 310S Hexagonal Pipe
Jis 310S Stainless Steel Coil Tubing JIS SUS310S Pipe
Din 1.4841/1.4845 AISI 310S Perforated Exhaust Tube Stainless Steel 310S Hypodermic Tubing
Din W.-Nr. 1.4841/1.4845 Aisi 310S Corrugated Tube SS 310S Box Pipe
Material 1.4841/1.4845 Aisi 310S Slotted Pipe SS 310S Thin Wall Tube
En 1.4841/1.4845 / Aisi 310S Thick Wall Tube 310S Stainless Steel Threaded Pipe
Stainless Steel 310S Ornamental Pipe Stainless Steel 310S Fin Tube / Finned Tube

Daxunを選択し、顧客を満足させる。.

今すぐDaxunに連絡する

310S Stainless Steel pipe Quick response

  • Improved resistance to cyclic oxidation
  • Improved resistance to sulfidation
  • Better high temperature strength
  • Improved resistance to intergranular corrosion
  • Good resistance to aqueous corrosion
  • Not susceptible to thermal fatigue and cyclic heating
  • Good strength up to 2100°
今すぐDaxunに連絡する

310S Stainless Steel pipe Daxun Advantages

  • Variety: From small to large diameter stainless steel pipe, we offer a wide range of sizes and grades, including 304L, 316L, 317L ,321,310S,347,2205and more.
  • Flexibility: Whether you need seamless or welded steel pipe, our stainless steel pipe lengths are designed to meet your specific project requirements.
    品質
  • Standards: Our stainless steel pipes meet stringent standards such as ISO9001, ABS, NSF/ANSI Standard 61, and NACE MR0175 to ensure reliability and performance.
  • Custom Orders: Looking for special size stainless steel pipes? We offer a variety of stainless steel pipe custom options at competitive prices and convenient online ordering.
今すぐDaxunに連絡する

Steel tube packaging

  1. Woven bag bale cargo (hexagonal)
  2. Special crates for U-bend pipes, (steel/wood) divided
  3. Each bale is wrapped in plastic to protect against wind and rain.
  4. SS 310S seamless pipes are protected by plastic covers.
  5. Plastic strips are used to secure the bale.
  6. Export-specific fumigation-free wooden crate packaging.
  7. Laminated packing slip attached to the bale or crate.
  8. Customized packaging as per customer needs.
今すぐDaxunに連絡する

310S Stainless Steel pipe Ordering Information

310S stainless steel pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.

今すぐDaxunに連絡する

品質、納期、検査

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • テスト用の無料サンプルを顧客に提供
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

310/310S Stainless Steel pipe and tube Features

高強度
耐食性
耐熱性
低温耐性
環境保護
溶接性能

大順合金 あなたのブランドを急速に向上させる

NPS Outside Diameter Wall Thickness 重量 重量
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
SS 310s Pipe Pressure Rating (psig)
310s Pipe Size(inches) 310s Pipe Schedule Temperature(F)
100 200 300 400 500 600 650 700 750
1″ 40 3048 2629 2362 2171 2019 1924 1867 1824 1810
80 4213 3634 3265 3002 2791 2659 2580 2528 2501
160 6140 5296 4759 4375 4068 3876 3761 3684 3646
1 1/2″ 40 2257 1947 1750 1608 1496 1425 1383 1354 1340
80 3182 2744 2466 2267 2108 2009 1949 1909 1889
160 4619 3984 3580 3291 3060 2916 2829 2772 2743
2″ 40 1902 1640 1474 1355 1260 1201 1165 1141 1129
80 2747 2369 2129 1957 1820 1734 1682 1648 1631
160 4499 3880 3486 3205 2980 2840 2755 2699 2671
3″ 40 1806 1558 1400 1287 1196 1140 1106 1084 1072
80 2553 2202 1979 1819 1691 1612 1564 1532 1516
160 3840 3312 2976 2736 2544 2424 2352 2304 2280
4″ 40 1531 1321 1187 1091 1014 967 938 919 909
80 2213 1909 1715 1577 1466 1397 1355 1328 1314
160 3601 3106 2791 2566 2386 2273 2206 2161 2138
5″ 40 1342 1158 1040 956 889 847 822 805 797
80 1981 1709 1535 1411 1312 1250 1213 1189 1176
160 3414 2945 2646 2433 2262 2155 2091 2049 2027
6 40 1219 1052 945 869 808 770 747 732 724
80 1913 1650 1483 1363 1267 1208 1172 1148 1136
160 3289 2836 2549 2343 2179 2076 2014 1973 1953
8″ 40 1073 926 832 765 711 678 657 644 637
80 1692 1459 1311 1205 1121 1068 1036 1015 1005
160 3175 2738 2460 2262 2103 2004 1944 1905 1885
10″ 40 974 840 755 694 645 615 596 584 578
80 1609 1388 1247 1147 1066 1016 986 966 56
160 3147 2714 2439 2242 2085 1986 1927 1880 1868
1 psi (lb/in2) = 6,894.8 Pa (N/m2) = 6.895×10-2 bar
Notes:
Maximum safe working pressure is calculated per ASME B 31.3-2012, paragraph 304.1.2 (formula 3a). Calculations assume maximum allowable O.D. and minimum allowable wall thickness (worst case scenario).
Temperature Range = -20°F to +300F, -28.8°C to 148.9°C
種類 Out diameter サイズ 長さ
NB Sizes (in stock) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc Cut to length
Stainless Steel 310/310S Seamless Tube (Custom Sizes) 6.35 mm OD To 508 mm OD As per requirement Cut to length
Stainless Steel 310/310S Welded Tube (ERW Tube) (in Stock + Custom Sizes) 6.35 mm OD To 1219 mm OD As per requirement Cut to length
表面仕上げ Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
文学士 Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of 310/310S stainless steel tube (6)

Daxun is a trustworthy stainless steel pipe and tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 310S stainless steel pipe have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

最近の注目プロジェクトと製品

310/310S stainless steel pipe
ステンレス鋼シームレスパイプ
310/310S stainless steel pipe
large diameter stainless steel pipe
ステンレス鋼研磨チューブ
310/310S seamless pipe
BA stainless steel pipe
ステンレス管
Stainless steel tube / pipe
Stainless steel welded pipe
310/310S stainless pipe
Stainless steel precision tube
サンプルをいただけますか?

私達は質を点検するためにあなたのためのステンレス鋼板のサンプルを提供してもいいです。サンプルは無料で、お客様は運賃を支払うだけです。.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

私達の MOQ はステンレス鋼シートのための 1 トンです。.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ
クイック見積もり