Duplex 2507 stainless steel plate, born for extreme environments
As China’s leading stainless steel plate supplier and exporter, Daxun provides 2507 stainless steel plates to the world.
- DGrade: AISI 2507-S32750
- 特徴:高い強度と信頼性
- 製造:冷延板、熱延板、鍛造板
- 規格ASM、ASME、GB、DIN、JIS、ISO、EN、BS
- 種類:冷間圧延薄板、熱間圧延厚板
- 表面: 2B、NO.1、NO.4、HL、BA、8K、等。.
- 長さ: 2438mm3048mm6000mm はカスタマイズすることができます
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong, ATI,
2507/S32750Global leader in stainless steel sheet fabrication services
At Daxun, we are pleased to provide customers with high-quality super duplex 2507 stainless steel plates, which are a 50/50 mixture of austenite and ferrite, stronger than pure austenite or iron alloys. Since its birth in the United States in the 1940s, it has developed to the third generation, and its main feature is that the yield strength can reach 400-550MPa, which is twice that of ordinary stainless steel, so the duplex plate can save materials and reduce equipment manufacturing costs. In terms of corrosion resistance, especially in media environments (such as seawater, high chloride ion content), the resistance to pitting, crevice corrosion, stress corrosion, and corrosion fatigue of duplex stainless steel is better than that of ordinary austenitic stainless steel, and is comparable to high-alloy austenitic stainless steel. Daxun Alloys provides duplex 2507 stainless steel in a variety of forms and sizes, all of which comply with industry and international standards such as ASTM, ASME, EURONORM and AFNOR.
Daxun’s inventory now includes Duplex 2507 stainless steel plate, an excellent super duplex stainless steel containing 25% chromium, 4% molybdenum and 7% nickel. This plate is designed for applications requiring excellent strength and corrosion resistance; such as applications in the chemical processing industry, petrochemical and seawater equipment industries. This grade of plate has excellent resistance to chloride stress corrosion cracking, high thermal conductivity and low thermal expansion coefficient. The high chromium, molybdenum and nickel content provides excellent resistance to pitting, crevice corrosion and general corrosion. Ask Daxun today.
技術データ
- パラメータ
- 化学組成
- 機械的性質
- 物理的性質
- スタンダード
| ASTM Specification | ASM A240 / ASME SA240 |
| スタンダード | MSRR, AMS, BS, ASTM A240 / ASME SA240 |
| Length& Sizes Duplex 2507 board | 1000 mm x 2000 mm, 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm, 2m, 2.44m, 3m, 36″ X 120″ or 48″ X 144″, 4′ x 8′, Cut to size available |
| 厚さ | 0.1mm~100mm Thk |
| 幅 | 10-2500mm |
| Hardness Duplex 2507 board | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
| Temper | Annealed |
| コンディション | Polished on both sides |
| Finish Duplex 2507 board | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Stock in form of Duplex 2507 board | Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate |
| Value Added Service | Cladding, Heat Treatment, Annealed, Pickling, Polish, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc. |
| Dealers & Distributor of | ATI, POSCO, JISCO, TISCO, LISCO, BAOSTEELESSAR, JINDAL, BHUSHAN, IMPORTED material |
| Test Report Duplex 2507 board | Raw Materials Certificate |
| EN 10204/3.1B | |
| 100% Radiography Test Report | |
| High special strength, high melt point | |
| Third Party Inspection Report, etc | |
| Excellent corrosive resistance, good thermal resistance | |
| Customer support after-sales service | |
| Strict Control from Raw Material to Finished | |
| Profiling Duplex 2507 board | To provide a full profiling service we use numerous profiling methods including: |
| Plasma Plate Cutting | |
| Laser Plate Cutting | |
| Oxy-propane Flame Cutting | |
| Specialized in Duplex 2507 board | material under 3/16 ” [5.00 mm] in thickness and 24″ [600 mm] and over in width |
| material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width | |
| cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width | |
| Free Quote, Inquiry answered within 24 hours | |
| We offer a comprehensive services designed to add value to your project: plasma cutting, waterjet cutting, laser cutting, bending and mechanical processing, edge preparation, welding, sawing and shearing. | |
| 名称 | 2507/S32750 |
| 国連 | S32750; S39275 |
| エン・ノー. | 1.441 |
| C(最大) | 0.03 |
| ムン | 1.2 |
| Si | 0.8 |
| Cr | 24.0-26.0 |
| ニー | 6.0-8.0 |
| モ | 3.0-5.0 |
| N | 0.24-0.32 |
| 銅 | 0.5 |
| その他 | S 最大0.020;P 最大0.035 |
| PREN | 40-43 |
| プロパティ | 価値 |
| 密度(g/cm3) | 7.8 |
| 0.2% Offset Yield Strength | 80 ksi |
| Ultimate Tensile Strength | 116 ksi |
| 0.1% Offset Yield Strength 0.2% | 91 ksi |
| Elongation in 2 inches, % | 15% |
| Hardness Rockwell C | 32 |
| Impact Energy | 74 ft.-lbs |
| 密度 | 0.28 lb per inch3 |
| 弾性係数 | 28 x 10(6) psi |
| 熱膨張係数 | 7.2 x 10(-6) per of at 68 to 212 of |
| 熱伝導率 | 8.7 Btu/hr ftoF |
| Heat capacity | 0.12 Btu/ lb oF |
| Electrical resistivity | 31.5 x10(-6) ohm-inch |
| Interval | Thermal | °C | 抵抗率 | Thermal | Specific | Young | Shear |
| Temper | expansion | conductivity | heat | modulus | modulus | ||
| °C | ax10M-bK-1 | (μ_ cm) | (W.m-1.K-1) | (J.kg-1.K-1 | E | G | |
| (GPa) | (GPa) | ||||||
| 20-100 | 13 | 20 | 80 | 17 | 450 | 200 | 75 |
| 20-100 | 13 | 100 | 92 | 18 | 500 | 190 | 73 |
| 20-200 | 13.5 | 200 | 100 | 19 | 530 | 180 | 70 |
| 20-300 | 14 | 300 | 105 | 20 | 560 | 170 | 67 |
| グレード | 国連 | Industry Specifications |
| 2507 Duplex Stainless Steel | UNS S32750 | ASTM A182 F53, A240, A276, A479, A789, A790, A815, A928, A988 |
| UNS S32760 | ASTM A182 F55, A240, A276, A314, A473, A479, A789, A790, A815, A928, A988 | |
| SAE J405 |
Daxunを選択し、顧客を満足させる。.

迅速な配達
We provide timely and fast delivery of 2507 stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
2507 stainless steel plate advantages:
- 2507 stainless steel plate has high resistance to pitting corrosion, with a PREN value of up to 43, and has excellent corrosion resistance. Duplex 2507 steel plate also exhibits excellent resistance to other forms of corrosion, including stress corrosion cracking (SCC), crevice corrosion, and general corrosion. These combined corrosion resistance properties make duplex 2507 a versatile and reliable choice for a wide range of applications in harsh environments.
- 2507 has a yield strength that is twice that of 300 series stainless steel. This strength advantage allows the use of thinner steel sections under the same load conditions and reduces the material cost of the equipment.
- It has a yield strength and tensile strength that is twice that of ordinary stainless steel. This significantly improves wear resistance.

Stainless Steel 2507 Applications
- 海水淡水化。.
- Oil and gas industry equipment, including offshore platforms, pipelines, and well casings.
- Chemical processing equipment, especially for handling corrosive chemicals.
- Pulp and paper industry, particularly bleaching process equipment.
- Petrochemical industry applications, including PVC strippers.
- 海水淡水化プラント。.
- Power industry equipment, such as flue gas desulfurization (FGD) systems.
- Marine components, including ship propellers and shafts.
- Pollution control equipment such as scrubbers.
- Fittings are crucial components for connecting and controlling the flow of fluids in pipelines and systems. This includes elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples, among others.
品質、納期、検査
- Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
当社の納期は、契約に厳密に従います。. - 顧客の第三者機関が工場に検査に行くのをサポートする。
- テスト用の無料サンプルを顧客に提供
- 現場検査またはビデオ工場検査をサポート
テクニカルサポート
さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.
高度な機械加工
Daxun Stainless Steel uses the ERP system to achieve full traceability of the type, specification, and origin of each stainless steel plate, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and its high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

2507 plate stainless steel Features
Daxun ブランドを急速に向上させる
- ギャラリー
- 寛容
- 配送状態
- その他の製品シリーズ
| 2Bシートの公差 | |||
| サイズ | 寛容度ランク | ||
| グループ1 | グループ2 | グループ3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| No.1熱延板の公差 | |||
| サイズ | 寛容度ランク | ||
| グループ1 | グループ2 | グループ3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| デリバリー・ステートの選択 | 表面状態 |
| 冷間圧延 | 2B |
| 2D | |
| 文学士 | |
| ヘアライン | |
| 第3位 | |
| 第4位 | |
| 6K | |
| 8K | |
| 注: | |
| 1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。. | |
| 2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。. | |
| 配信状態 | |
| デリバリー・ステートの選択 | 表面状態 |
| 熱間圧延 | 第1位 |
| 第3位 | |
| 第4位 | |
| 6K | |
| 8K | |
| ピクルス | |
| 注: | |
| 1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。. | |
| 2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。. | |
| グレード | タイプ | 厚さ | 表面 |
| オーステナイト系 | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/4番/8K/SB/HL/1番 |
| 321 | 0.4-80mm | 2B/BA/4番/8K/SB/HL/1番 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/4番/8K/SB/HL/1番 | |
| フェライト | 430 | 0.4-3.0mm | 2b/ba/no.4/8k/sb/hl |
| 超高純度フェライト | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
| 409L | 0.4-2.5mm | 2B、2D | |
| グレード | タイプ | 厚さ | オリジナル |
| 耐熱鋼 | 309S | 0.5-40mm | 中国 |
| 310S | 0.5-40mm | 中国 | |
| 二相鋼 | 2101 | 1.5-50mm | 中国 |
| 2304 | 3.0-50mm | 中国 | |
| 2205 | 0.5-60mm | 中国 | |
| 2507 | 1.0-60mm | スイス/日本/中国 | |
| スーパーオーステナイト鋼 | N08904 | 0.6-50mm | スイス/日本/中国 |
| S31254 | 0.5-50mm | スイス/日本/中国 | |
| N08926 | 0.5-50mm | スイス/日本/中国 | |
| N08367 | 0.5-50mm | スイス/日本/中国 | |
| ニッケル基合金 | N08031 | 1.0-50mm | アメリカ / 日本 / ドイツ |
| N08810/N08800 | 0.8-50mm | アメリカ / 日本 / 中国 | |
| N08028 | 1.0-20mm | アメリカ / ドイツ / 日本 | |
| N08020 | 1.0-20mm | アメリカ / ドイツ / 日本 | |
| N08825 | 0.8-40mm | アメリカ / ドイツ / スイス / 日本 / 中国 | |
| N10276 | 0.5-50mm | アメリカ / ドイツ / 日本 | |
| N06022 | 1.0-50mm | アメリカ / ドイツ / 日本 | |
| N06625 | 0.8-20mm | アメリカ / ドイツ / 中国 | |
| N04400 | 1.0-20mm | アメリカ / ドイツ / 日本 | |
| N06600 | 1.0-50mm | アメリカ / ドイツ / 日本 / 中国 | |
| N02201 | 0.5-20mm | アメリカ / 日本 | |
| チタン | TA1/Gr1 | 0.5-50mm | 日本 / 中国 |
| TA2/Gr2 | 0.5-50mm | 日本 / 中国 | |
| 溶接材料 | ERNiCrMo-13 | 1.2、2.4mm | ドイツ |
| ERNiCrMo-3 | 2.4mm | ドイツ | |
| ERNiCrMo-4 | 2.4mm | 米国 |
The surface and shape of 2507 stainless steel plate (7)
参照およびダウンロード可能な情報
Daxunは信頼できるステンレス鋼板メーカーです。
Daxunは専門メーカーとして、生産するすべての製品が高品質であることを保証します。そのため、すべてのステンレス鋼板はISO9001、SGS、CE、OQCなどの国際品質規格の認証を取得しています。また、ステンレス鋼板の欠陥が少ないことを保証するために、厳格な品質管理を行っています。Daxunでは、すべての製品は、耐久性、高品質、高性能であることをご安心ください。.
関連商品 (13)
Yes. Duplex 2507 stainless steel has good weldability and can be joined to itself and other materials using a variety of welding methods, including SMAW (shielded metal arc welding), PAW (plasma arc welding), GTAW (gas tungsten arc welding), FCW (flux cored wire) and SAW (submerged arc welding). When welding 2507, it is best to use 2507/P100 filler metal.
Yes. Although duplex 2507 stainless steel is very corrosion resistant, it can still rust in extreme situations. It is, nevertheless, less likely to rust than other varieties of stainless steel. The high quantities of chromium and molybdenum in 2507 make it extremely resistant to uniform corrosion caused by organic acids like formic and acetic acid. The exceptional corrosion resistance of 2507 steel makes it suited for use in corrosive conditions such as seawater, acids, and chemicals, where it retains its integrity and does not rust or corrode quickly.
Yes, the presence of ferritic grains within its composition renders 2507 duplex stainless steel a magnetic material.
Yes, duplex 2507 is an expensive metal. This is primarily due to its high alloying content, but it comes with the added benefit of exceptional corrosion resistance in extreme environments.
私達は質を点検するためにあなたのためのステンレス鋼板のサンプルを提供してもいいです。サンプルは無料で、お客様は運賃を支払うだけです。.
カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.
私達の MOQ はステンレス鋼シートのための 1 トンです。.
トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.