x
أرسل استفسارك اليوم
اقتباس سريع

Grade 12 Ti-0.3Mo-0.8Ni Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Grade 12 - UNS R53400
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 12 titanium is approximately 4.51 g/cm3
  • Standards:ASTM B338、ASTM B861
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 12 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 12 Titanium Pipe to Customers Around The World
Grade 12 titanium pipe is a specialized tubing made from Ti-0.3Mo-0.8Ni titanium alloy, which belongs to a specific grade in the titanium alloy pipe family. This material is created by adding 0.3% molybdenum and 0.8% nickel to pure titanium, significantly enhancing its corrosion resistance, particularly in acidic environments and chloride media. Grade 12 titanium pipe complies with international standards such as ASTM B338 or ASTM B861, featuring a density of approximately 4.51 g/cm³, tensile strength of about 483 MPa, and yield strength of around 345 MPa, while maintaining the lightweight characteristics typical of titanium materials.

Where is Grade 12 titanium pipe used?
Compared to pure titanium, Grade 12 titanium pipe offers superior resistance to crevice corrosion and stress corrosion cracking, making it particularly suitable for chemical processing equipment, heat exchangers, oil and gas industries, and seawater treatment systems. This material provides longer service life and lower maintenance costs while maintaining excellent mechanical properties, making it highly favored in high-end industrial applications and an ideal choice for handling corrosive fluids.
Chemical processing plants utilize it for heat exchangers, reactor vessels, and piping systems handling aggressive acids and chlorides. Marine and offshore installations employ it in seawater cooling systems, desalination equipment, and subsea components, leveraging its exceptional resistance to saltwater corrosion and biofouling. In the oil and gas sector, it serves in downhole tubing, Christmas tree components, and production equipment exposed to sour environments with H₂S and CO₂. Power generation facilities specify Grade 12 titanium for condenser tubes and heat exchangers in cooling systems, while industrial pollution control systems incorporate it in scrubbers and flue gas desulfurization units that handle corrosive gases and acidic condensates.

Key Performance

Strength-Ductility Balance:

  • Tensile Strength: 483 MPa (annealed state) – Matches Grade 2 but with superior corrosion resistance.
  • Yield Strength: 345 MPa (min) – Exceeds Grade 2 (275 MPa), suitable for pressure-containing components.
  • Elongation: 18% (min) – Exceptional ductility for cold forming, flaring, and high fatigue resistance.
  • Density: 4.51 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Core Mechanism: Synergistic effect of Molybdenum (0.3%) and Nickel (0.8%) stabilizes the passive oxide layer.
  • Pitting/Crevice Corrosion Resistance:
    • Outstanding performance in seawater, chloride solutions (e.g., NaCl, MgCl₂), and sour gas (H₂S) environments.
    • Resists reducing acids (e.g., H₂SO₄, HCl) where stainless steels fail.
  • Advantages vs. Other Grades:
    • Outperforms Grade 2 in reducing acids and chlorides.
    • Superior to Grade 9 in high-temperature acidic media (e.g., chemical processing).
    • Immune to corrosion in oxidizing media (e.g., HNO₃) and aggressive chemical environments.
  • Optimal Heat Treatment: Annealed at 595°C to maximize corrosion resistance and ductility.
قراءة المزيد

البيانات

العنصر Minimum (%) Maximum (%)
Titanium (Ti) الرصيد الرصيد
الموليبدينوم (Mo) 0.25 0.40
النيكل (ني) 0.60 0.90
الحديد (Fe) 0.30
Oxygen (O) 0.25
Carbon © 0.08
النيتروجين (N) 0.03
Hydrogen (H) 0.015
عناصر أخرى 0.40 (total)
الممتلكات Value/Range Unit
الكثافة 4.48 g/cm³
نقطة الانصهار 1650 ± 20 °C
التوصيل الحراري 7.2 (at 25°C) W/m·K
Specific Heat 560 (at 25°C) J/kg·K
المقاوماتية الكهربائية 1.7 μΩ·m
Magnetic Susceptibility Paramagnetic
الممتلكات Minimum Requirement Typical Value Unit Test Method
قوة الشد 483 520–620 MPa ASTM E8/E8M
قوة الخضوع (إزاحة 0.2%) 345 380–480 MPa ASTM E8/E8M
الاستطالة 18 22–30 % ASTM E8/E8M
الصلابة ≤ 200 (HV) 150–180 (HV) Vickers ASTM E10
Impact Toughness Not specified 40–60 J ASTM E23

Elevated Temperature Performance

Temperature (°C) قوة الشد (ميجا باسكال) Yield Strength (MPa) الاستطالة (%)
100 450–500 320–370 20–25
200 400–450 280–330 18–23
300 350–400 240–290 15–20

 

اختر Daxun لمساعدة مشروعك على الانطلاق.

اتصل بـ Daxun الآن

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
اتصل بـ Daxun الآن

Grade 12 Titanium Tube Features

Grade 12 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
اتصل بـ Daxun الآن

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

اتصل بـ Daxun الآن

تقارير الاختبار

The test reports we provide include: Factory test certificate for Grade 12 titanium welded pipe and Grade 12 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

اتصل بـ Daxun الآن

Applications and standards

Titanium Grade 12 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
اتصل بـ Daxun الآن

الجودة والتسليم والتفتيش

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 12 Titanium Welded Pipe and Grade 12 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • وقت التسليم لدينا يتوافق تمامًا مع العقد.
  • دعم الوكالات الخارجية للعملاء للذهاب إلى المصنع للفحص
  • دعم العينات المجانية لاختبار العملاء
  • دعم الفحص الموقعي أو فحص المصنع بالفيديو
اتصل بـ Daxun الآن

التعبئة والتغليف

تضمن شركة Daxun Alloy أفضل جودة للتغليف لأنها تلعب دورًا مهمًا في الشحن الدولي حيث تمر البضائع عبر قنوات مختلفة للوصول إلى الوجهة النهائية، لذلك نولي اهتمامًا خاصًا بالتغليف. نقوم بتغليف بضائعنا بعدة طرق حسب المنتج. نقوم بتغليف منتجاتنا بعدة طرق مثل:
- الصناديق والصناديق
- الغلاف المنكمش
- منصات خشبية
- صناديق خشبية

اتصل بـ Daxun الآن

الدعم الفني

إذا كنت بحاجة إلى أي مساعدة فنية إضافية، فسيكون من دواعي سرور أخصائي المعادن المقيم لدينا وموظفينا المطلعين تقديم المساعدة. بالإضافة إلى ذلك، تفتخر Daxun بوجود مختبر اختبار معتمد - وهو الأول من نوعه في صناعة مخزون المعادن المتعددة والبلاستيك. وهذا، في رأينا، يدل على تفانينا الثابت للجودة وفلسفتنا كمورد متكامل الخدمات.

Daxun Grade 12 Titanium TUBE Let your brand improve rapidly

Grade 12 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

أحدث مشاريع ومنتجات الحالة الساخنة

ما هي درجة التيتانيوم الأفضل؟

تعتمد درجة سبيكة التيتانيوم التي تحتاجها على المشروع الذي تعمل عليه، حيث أن لكل درجة فوائد مختلفة.

إنّ جميع درجات سبائك التيتانيوم قوية للغاية ومقاومة للتآكل، مما يعني أنها ستستمر في العمل بشكل جيد في أقسى الظروف.

إن الدرجات الأعلى من سبائك التيتانيوم (5-12) هي سبائك مصممة لفوائد محددة. على سبيل المثال، تتميز سبائك التيتانيوم من الدرجة 12 بمقاومة ممتازة للحرارة، مما يجعلها خياراً مثالياً للمبادلات الحرارية الصدفية والأنبوبية والأنابيب الهيدروليكية ومعدات الصناعة الكيميائية.

الدرجات من 1-4 هي سبائك التيتانيوم النقي، وهي خيار مثالي إذا كنت بحاجة إلى مادة قابلة للحام وقابلة للسحب لأنظمة الأنابيب والأنابيب. ستجد درجات أقل تستخدم في الصناعات البحرية والصناعية.

إذا كنت تبدأ مشروعاً ولست متأكداً من درجة سبيكة التيتانيوم الأفضل لك، اتصل بنا اليوم؛ فنحن سعداء للغاية بمساعدتك.

كيف تختلف الدرجات الأعلى من التيتانيوم عن الدرجات الأدنى؟

نقدم في DAXUN مجموعة واسعة من درجات سبائك التيتانيوم من الدرجة 1 إلى الدرجة 12.

الدرجات من 1 إلى 4 هي التيتانيوم النقي، بينما الدرجات الأعلى هي السبائك.

تحظى درجات السبائك بشعبية كبيرة بسبب نسبة قوتها إلى وزنها العالية.

درجة سبائك التيتانيوم الأكثر استخداماً لدينا هي الدرجة 5. وعلى الرغم من أنها لا تزال تحتوي على نسبة عالية من التيتانيوم، إلا أن هذه الدرجة هي الأكثر موثوقية لأنها تتحمل درجات حرارة تصل إلى 600 درجة فهرنهايت وتتحمل الظروف القاسية.

وتفضل الصناعات مثل صناعات الطيران والصناعات البحرية الدرجات الأعلى لمقاومتها للتآكل والتآكل.

وعلى العكس من ذلك، تُستخدم الدرجات الأقل في المقام الأول في اللحام نظرًا لانخفاض قوتها.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

هل تؤثر درجة التيتانيوم على التكلفة؟

على الرغم من أن درجة التيتانيوم تزيد من التكلفة قليلاً، إلا أن التكلفة الإجمالية تتحدد في المقام الأول حسب شكل وشكل التيتانيوم الذي تحتاجه.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

لسوء الحظ، من الصعب التوصل إلى سعر عبر الإنترنت دون معرفة الكثير عن مشروعك وما سيُستخدم التيتانيوم من أجله.

لحسن الحظ، فريق خبرائنا موجود دائماً لمساعدتك وتقديم المشورة لك بشأن احتياجاتك من التيتانيوم. من خلال إرسال بريد إلكتروني إلى [email protected]، سنكون قادرين على الرد عليك ببعض النصائح وعرض أسعار دقيق.

احرص على تضمين أكبر قدر ممكن من المعلومات حول درجة وشكل وكمية التيتانيوم التي تحتاجها للحصول على فهم أفضل لاحتياجاتك.

أين يمكنني معرفة المزيد عن درجات التيتانيوم؟

يتمتع فريق العمل في DAXUN بالخبرة والمعرفة والود. وبفضل سنوات خبرتهم الطويلة في هذا المجال، فهم يعرفون كل شيء عن التيتانيوم، بما في ذلك استخداماته وفوائده ودرجاته.

للحصول على تحديثات منتظمة عن التيتانيوم واستخداماته وتطبيقاته في مختلف الصناعات، احرص على الاطلاع على مدونتنا. لقد كتب خبراؤنا أدلة سهلة المتابعة يمكنك الرجوع إليها دائماً عندما تكون لديك أسئلة.

إذا كنت لا تزال تواجه مشكلة، فلا تتردد في الاتصال بنا؛ يسعدنا تقديم المساعدة.

من خلال إرسال بريد إلكتروني إلى [email protected]، ستتلقى رداً سريعاً. تأكد من تضمين أكبر قدر ممكن من التفاصيل في سؤالك حتى نتمكن من التوصية بالحل المناسب.

كيف تحصل على عرض أسعار أو تفهم معلومات السوق في أسرع وقت ممكن؟

يُرجى ملء النموذج الموجود في صفحة “اتصل بنا”، أو الاتصال بمدير المبيعات لدينا على “+86 13382898899”، وسوف نتصل بك في أقرب وقت ممكن. واتسابنا على الإنترنت، وسيتم التحقق من البريد الإلكتروني ([email protected]) في غضون 6 ساعات. سيتم الرد على كل استفسار أو رسالة على الفور. بالإضافة إلى ذلك، نشارك معلومات السوق مع عملائنا كل أسبوع

هل يمكنني الحصول على بعض العينات؟

يمكننا تقديم عينات من صفائح الفولاذ المقاوم للصدأ لك للتحقق من الجودة. العينة مجانية وما عليك سوى دفع أجرة الشحن.

ما هي الدول التي قمت بتصديرها بالفعل؟

لقد قمنا بالتصدير إلى أكثر من 42 دولة، مثل كندا، وتشيلي، والكويت، وألمانيا، وكوريا الجنوبية، والمملكة العربية السعودية، وسنغافورة، وغيرها.

ما هو موك الخاص بك؟

موك لدينا هو 1 طن لصفائح الفولاذ المقاوم للصدأ.

ما هي مدة التوصيل؟

يمكن تسليم الطلبات التجريبية في غضون أسبوع. بالنسبة للطلبات العادية، يستغرق الأمر أسبوعين تقريباً.

أرسل استفسارك اليوم