Daxun is an excellent manufacturer of grade 12 (Ti-0.3Mo-0.8Ni) titanium rods and bars.
- Titanium bar grade: Grade 12-Ti / UNS R53400
- أنواع قضبان التيتانيوم: القضبان المدرفلة، القضبان المسحوبة، قضبان التيتانيوم المطروقة
- Titanium bar density: The density of grade 12 titanium is 4.51 g/cm³
- المعايير الرئيسية: ASTM ASME GB GB GJB EN JIS DIN ISO ATP BS، إلخ.
- High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.
الشركة الرائدة عالمياً في خدمات تصنيع قضبان التيتانيوم النقي تجارياً
Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 12 titanium alloy rods.
Grade 12 titanium bar (Ti Grade 12 / UNS R53400) is a nickel-molybdenum-enhanced, commercially pure (CP) titanium alloy specifically engineered for superior corrosion resistance in aggressive environments. It consists of titanium (≥99%) with strategic additions of 0.6–0.9% nickel (Ni) and 0.2–0.4% molybdenum (Mo), which significantly enhances its electrochemical properties. This nickel-molybdenum modification substantially improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice corrosion—conditions where standard CP grades like Grade 2 would exhibit accelerated degradation. While maintaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 12 offers enhanced performance at elevated temperatures (up to ~315°C/600°F) and in moderately reducing or acidic environments. Its passive oxide layer, reinforced by the nickel-molybdenum combination, provides exceptional protection against chemical attack, making it one of the most cost-effective corrosion-resistant metallic materials available.
Where is Grade 12 titanium bar used?
Grade 12 titanium bar is widely utilized in chemical processing for essential components such as heat exchangers, piping systems, vessel linings, and agitators handling acids, chlorides, or organic compounds. In marine and offshore applications, it serves in seawater desalination plants, condenser tubing, and offshore platform components exposed to high-salinity conditions. The alloy also performs exceptionally well in oil and gas production equipment, pulp and paper processing machinery, and power generation systems due to its durability and corrosion resistance. Despite its moderate premium over standard grades—justified by its alloying elements—Grade 12 delivers outstanding lifecycle value by reducing maintenance requirements, extending service intervals, and minimizing replacement costs in corrosive service. Its reliability in preventing premature failures ensures operational continuity and cost efficiency in applications ranging from chemical processing plants to marine infrastructure, establishing it as an optimal solution for demanding corrosion challenges where budget constraints exist.
داكسون هي شركة إنتاج قضبان سبائك التيتانيوم الموثوق بها. تنتج شركة Daxun جميع درجات سبائك التيتانيوم، بما في ذلك سلسلة التيتانيوم النقي تجاريًا CP، وسلسلة سبائك التيتانيوم، وسبائك التيتانيوم والنيكل، وما إلى ذلك. إنها تتمتع بأداء موثوق به وتوفر أداءً عاليًا لتطبيقاتك الحرجة. في مختلف الصناعات والتطبيقات، يمكنك الاعتماد على قضبان سبائك التيتانيوم من Daxun لقوة عالية ودرجة حرارة عالية وبيئات تآكل. على مدى عقود، تلتزم شركة Daxun Metals بإنتاج حلول سبائك التيتانيوم عالية الهندسة لمواجهة أشد التحديات.
البيانات
- المعلمة
- المكونات
- الخواص الميكانيكية
- الخصائص الفيزيائية
| المواصفات | التفاصيل |
|---|---|
| المواد | Titanium rod and bar Grade 12 (UNS R53400) |
| قياسي | astm b348، astm sb348، ams 4921، ams 4902 |
| الأبعاد | EN، ASTM، JIS، JIS، ASME، BMS، AISI، GB، GJB، DIN |
| نطاق القطر | 0.125 ″ - 14 ″ (3.175 مم - 355.6 مم)، مخصص |
| نطاق الطول | ما يصل إلى 240 بوصة (6096 مم)، حسب الطلب |
| الإنهاء | مسحوب على البارد (ساطع)، ومطحون بدون مركز، ومدرفل على الساخن، ومدرفل على الساخن، ومدرفل على الساخن ومطحون على الساخن، ومطحون على الساخن، ومطحون على الساخن، ومطحون على الساخن، ومطحون على البارد، ومطحون بدون مركز، ومطحون على الساخن، ومطحون على الساخن، ومطحون على الساخن، ومطحون على الساخن، ومطحون على الساخن، ومطحون على الساخن |
| تشطيب السطح | مسحوب على البارد، أو مسحوب على البارد، أو أرضي بدون مركز، أو مصقول، أو خشن، أو أسود، أو تشطيب رقم 4، أو تشطيب BA، أو تشطيب غير لامع، إلخ. |
| الحالة | Hardened & tempered, annealed |
| التسامح | تفاوت القطر: +/- 0.005″ (0.127 مم)، تفاوت الطول: +/- 0.125″ (3.175 مم) |
| الاستمارة | قضبان التيتانيوم المربعة، وسبائك التيتانيوم، وقضبان التيتانيوم المستديرة، وقضبان التيتانيوم المستطيلة، وقضبان التيتانيوم المثلثة، وقضبان التيتانيوم المطروقة، وقضبان التيتانيوم السداسية الشكل، إلخ. |
| العنصر | Minimum (%) |
Maximum (%)
|
| Titanium (Ti) | الرصيد | الرصيد |
| الموليبدينوم (Mo) | 0.25 | 0.4 |
| النيكل (ني) | 0.6 | 0.9 |
| الحديد (Fe) | — | 0.3 |
| Oxygen (O) | — | 0.25 |
| Carbon © | — | 0.08 |
| النيتروجين (N) | — | 0.03 |
| Hydrogen (H) | — | 0.015 |
| عناصر أخرى | — | 0.40 (total) |
| الممتلكات | Minimum Requirement | Typical Value | Unit | Test Method |
| قوة الشد | 483 | 520–620 | MPa |
ASTM E8/E8M
|
| قوة الخضوع (إزاحة 0.2%) | 345 | 380–480 | MPa |
ASTM E8/E8M
|
| الاستطالة | 18 | 22–30 | % |
ASTM E8/E8M
|
| الصلابة | ≤ 200 (HV) | 150–180 (HV) | Vickers | ASTM E10 |
| Impact Toughness | Not specified | 40–60 | J | ASTM E23 |
Elevated Temperature Performance
|
Temperature (°C)
|
قوة الشد (ميجا باسكال) | Yield Strength (MPa) |
الاستطالة (%)
|
| 100 | 450–500 | 320–370 | 20–25 |
| 200 | 400–450 | 280–330 | 18–23 |
| 300 | 350–400 | 240–290 | 15–20 |
| الممتلكات | Value/Range | Unit |
| الكثافة | 4.48 | g/cm³ |
| نقطة الانصهار | 1650 ± 20 | °C |
| التوصيل الحراري | 7.2 (at 25°C) | W/m·K |
| Specific Heat | 560 (at 25°C) | J/kg·K |
| المقاوماتية الكهربائية | 1.7 | μΩ·m |
| Magnetic Susceptibility | Paramagnetic | — |
اختر Daxun لمساعدة مشروعك على الانطلاق.
DAXUN® Grade 12 Titanium Rod Features
DAXUN® Ti الصف 5 عبارة عن قضيب من سبائك التيتانيوم (6al-4v) يتميز بـ
- قابلية تشكيل ولحام جيدة على الساخن;
- يمكن أن تصل قوة الشد إلى 1000 ميجا باسكال;
- عمل الأبعاد في درجة حرارة عالية
- غير حساس لمياه البحر أو مياه البحر;
- لا تتأثر بمختلف الوسائط المسببة للتآكل;
- قوة عالية وصلابة جيدة;
- مقاومة بدء التشقق وانتشار الشقوق.
مزايا مصنع داكسن
يروج مفهوم “إدارة التميز في الأداء” في داكسون لنموذج إدارة “PDCA + اللين”. وتقول بطاقة أعمال الشركة “Daxun = جودة موثوقة”. تستخدم Daxun نظام تخطيط موارد المؤسسات لتحقيق إمكانية التتبع الكامل للصنف والمواصفات ومنشأ كل قضيب تيتانيوم، وتدعو وتشجع على مكافحة التزييف في الصناعة. وتعتمد Daxun على التكنولوجيا في المعالجة والتخصيص، والدقة العالية والجودة العالية هي معايير الصناعة؛ وفيما يتعلق بالخدمة، فإنها تعزز إدارة دورة حياة المنتج، وتوفر حلولاً احترافية لاختيار المواد والمعالجة قبل البيع، وتراقب بدقة أثناء البيع، وتوفر ضمانات خدمة خالية من القلق بعد البيع.
Grade 12 Titanium Rod Production Method
تنتج Daxun قضبان التيتانيوم عالية الجودة ذات الأداء العالي، ويمكنها أيضًا تصنيعها وفقًا لاتفاق العميل:
- تحتاج سبائك التيتانيوم إلى الخضوع للمعالجة الحرارية والتشغيل الآلي، والاختبار بالموجات فوق الصوتية بالغمر، واختبار الخواص الميكانيكية، والفحص الهيكلي العياني والمجهري وغيرها من العمليات. عملية الإنتاج: قضبان التيتانيوم المدرفلة على الساخن - كفاءة عالية، وأداء مستقر، قضبان التيتانيوم المطروقة - حجم مرن، تزوير متعدد النيران، تحسين الأداء الشامل لقضبان التيتانيوم، قضبان التيتانيوم المسحوبة على البارد - عادةً ما تكون قضبان التيتانيوم صغيرة الحجم وعالية الدقة؛ يتم تسليم جميع قضبان التيتانيوم المذكورة أعلاه بسطح لامع.
تقارير الاختبار
تشمل تقارير الاختبار التي نقدمها ما يلي: قضيب التيتانيوم من الدرجة 2 وقضيب التيتانيوم المستدير من الدرجة 2 شهادة اختبار المصنع، EN 10204 3.1، التقرير الكيميائي، التقرير الميكانيكي، تقرير اختبار PMI، تقرير الفحص البصري، تقرير فحص الطرف الثالث، تقرير مختبر NABL المعتمد، تقرير الاختبار المدمر، تقرير الاختبار غير المدمر، تقرير الاختبار غير المدمر. (ستقدم Daxun وفقًا لمتطلبات العملاء)
Grade 12 Rods Applications and Standards
Grade 12 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- الفضاء، وبناء السفن، وصناعة السفن، وصناعة النفط والغاز، والهندسة البحرية، والمصانع الكيميائية، والآلات الصناعية، وصناعة الطاقة، وصناعة الورق ولب الورق، وصناعة تجهيز الأغذية، والمصافي، والصناعات العسكرية، ومعدات تجهيز الأدوية والأغذية، إلخ.
- المواصفات: Ams 4928,ams 4928,ams 4967,ams 4965,ams 6931,astm b 348
- المعايير: Astm, asme, asme, en, jis, din, gb, gjb, gjb, api
الجودة والتسليم والتفتيش
تقوم Daxun بإجراء العديد من اختبارات ضمان الجودة، وتشمل هذه الاختبارات الاختبارات الاختبارات الميكانيكية مثل اختبارات الشد المساحي، والتحليل الكيميائي، والتحليل الكيميائي، والتحديد الإيجابي للمواد - اختبار PMI، والاختبارات الدقيقة والكليّة، واختبار التآكل بين الخلايا الحبيبية (IGC)، واختبار الكشف عن الخلل بالموجات فوق الصوتية، واختبار التنقر والمقاومة، واختبار الصلابة، والتحديد الإيجابي للمواد، واختبار التمدد وما إلى ذلك. تضمن جميع هذه الاختبارات أن قضيب التيتانيوم من الدرجة 2 وقضيب التيتانيوم المستدير من الدرجة 2 مناسب للتطبيق المطلوب. أثناء عملية الإنتاج، نقوم بقياس قطر وسمك وسطح المنتج.
- وقت التسليم لدينا يتوافق تمامًا مع العقد.
- دعم الوكالات الخارجية للعملاء للذهاب إلى المصنع للفحص
- دعم العينات المجانية لاختبار العملاء
- دعم الفحص الموقعي أو فحص المصنع بالفيديو
التعبئة والتغليف
تضمن شركة Daxun Alloy أفضل جودة للتغليف لأنها تلعب دورًا مهمًا في الشحن الدولي حيث تمر البضائع عبر قنوات مختلفة للوصول إلى الوجهة النهائية، لذلك نولي اهتمامًا خاصًا بالتغليف. نقوم بتغليف بضائعنا بعدة طرق حسب المنتج. نقوم بتغليف منتجاتنا بعدة طرق مثل:
- الصناديق والصناديق
- الغلاف المنكمش
- منصات خشبية
- صناديق خشبية
الدعم الفني
إذا كنت بحاجة إلى أي مساعدة فنية إضافية، فسيكون من دواعي سرور أخصائي المعادن المقيم لدينا وموظفينا المطلعين تقديم المساعدة. بالإضافة إلى ذلك، تفتخر Daxun بوجود مختبر اختبار معتمد - وهو الأول من نوعه في صناعة مخزون المعادن المتعددة والبلاستيك. وهذا، في رأينا، يدل على تفانينا الثابت للجودة وفلسفتنا كمورد متكامل الخدمات.
Daxun Grade 12 Titanium Rods help your brand improve quickly
- Tolerances for Grade 12 Titanium Round Bars (BS EN ISO 286-2)
| الحجم الاسمي | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| القطر مم | ||||||||
| ~ إلى 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| أكثر من 3 إلى 6 | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| أكثر من 6 إلى 10 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| فوق 10 إلى 18 سنة | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| فوق 18 إلى 30 سنة | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| أكثر من 30 إلى 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| أكثر من 50 إلى 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| أكثر من 80 إلى 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| أكثر من 120 إلى 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| أكثر من 180 إلى 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Grade 12 Titanium Rods (3)
قضيب تيتانيوم
أحدث مشاريع ومنتجات الحالة الساخنة
المنتجات ذات الصلة (8)
Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 12 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
المواصفات
ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4924 – Titanium Alloy Bars and Billets, Grade 12
المعالجة الحرارية
When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).
DAXUN Grade 12 alloy can be heat treated in a variety of ways:
- Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
- Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool
الصلابة
Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.
قابلية التزوير/قابلية التشكيل
Grade 12 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.
Grade 12 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).
قابلية التصنيع
Grade 12 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The nickel-molybdenum content does not significantly affect machinability compared to other CP titanium grades.
قابلية اللحام
Grade 12 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The nickel-molybdenum addition enhances weld integrity in corrosive environments.
Special Considerations
Grade 12 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The nickel-molybdenum content provides additional protection against corrosion in contaminated conditions.
نطاق الحجم
Grade 12 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 – 400 mm (hot rolled, peeled)
Tolerances: h11–h5 (ISO 286-2)
Tighter or different tolerances available on request
Lengths up to 9,000 mm long, depending on diameter
For larger diameters, other bar lengths and tolerances can be agreed upon request
Availability Grade 7 Titanium Rods
تتضمن خيارات المعالجة ما يلي:
- Drawing, straightening
- Drawing, straightening, polishing
- Drawing, grinding, polishing
- الرسم، والتقويم، والطحن، والتلميع، والصقل
- Drawing, annealing, straightening
- Drawing, annealing, polishing
- Drawing, annealing, grinding, polishing
- Drawing, annealing, straightening, grinding, polishing
We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.
Sawing
- Band saws (up to Ø510 mm)
- Bench band saws (up to 6,000 x 3,000 x 400 mm)
- High-performance sawing machines for precise sawing
Titanium Bar End Machining
- Single or double sided
- Chamfer 90° (45°)
- Point 60° (30°)
- Flat end
- Centered
Delivery Form
- ASTM American Society for Testing and Materials Standards
- AMS American Aerospace Materials Standards
- NACE American Association of Corrosion Engineers International Standards
- ASME American Society of Mechanical Engineers Standards
- GB Chinese National Standards
- GJB Chinese National Military Standards
- ISO International Standards
- DIN German Standards
- EN European Standards
- API American Petroleum Institute Standards
Detection Method
Non-destructive testing > 100% testing
Testing methods:
- Eddy current testing / eddy current crack testing
- Defect-free surface (level 4)
- Flat bottom hole diameter 0.7 mm and 0.4 mm
- Blind area can be cut off according to fixed length > Test to the end of the bar
- Full diameter ultrasonic testing
Our Titanium Bar Material Services
As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.
If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 12 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
معلومات الطلب
Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact داكسون now, we will reply to your email as soon as possible.
تعتمد درجة سبيكة التيتانيوم التي تحتاجها على المشروع الذي تعمل عليه، حيث أن لكل درجة فوائد مختلفة.
إنّ جميع درجات سبائك التيتانيوم قوية للغاية ومقاومة للتآكل، مما يعني أنها ستستمر في العمل بشكل جيد في أقسى الظروف.
إن الدرجات الأعلى من سبائك التيتانيوم (5-12) هي سبائك مصممة لفوائد محددة. على سبيل المثال، تتميز سبائك التيتانيوم من الدرجة 12 بمقاومة ممتازة للحرارة، مما يجعلها خياراً مثالياً للمبادلات الحرارية الصدفية والأنبوبية والأنابيب الهيدروليكية ومعدات الصناعة الكيميائية.
الدرجات من 1-4 هي سبائك التيتانيوم النقي، وهي خيار مثالي إذا كنت بحاجة إلى مادة قابلة للحام وقابلة للسحب لأنظمة الأنابيب والأنابيب. ستجد درجات أقل تستخدم في الصناعات البحرية والصناعية.
إذا كنت تبدأ مشروعاً ولست متأكداً من درجة سبيكة التيتانيوم الأفضل لك، اتصل بنا اليوم؛ فنحن سعداء للغاية بمساعدتك.
نقدم في DAXUN مجموعة واسعة من درجات سبائك التيتانيوم من الدرجة 1 إلى الدرجة 12.
الدرجات من 1 إلى 4 هي التيتانيوم النقي، بينما الدرجات الأعلى هي السبائك.
تحظى درجات السبائك بشعبية كبيرة بسبب نسبة قوتها إلى وزنها العالية.
درجة سبائك التيتانيوم الأكثر استخداماً لدينا هي الدرجة 5. وعلى الرغم من أنها لا تزال تحتوي على نسبة عالية من التيتانيوم، إلا أن هذه الدرجة هي الأكثر موثوقية لأنها تتحمل درجات حرارة تصل إلى 600 درجة فهرنهايت وتتحمل الظروف القاسية.
وتفضل الصناعات مثل صناعات الطيران والصناعات البحرية الدرجات الأعلى لمقاومتها للتآكل والتآكل.
وعلى العكس من ذلك، تُستخدم الدرجات الأقل في المقام الأول في اللحام نظرًا لانخفاض قوتها.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
على الرغم من أن درجة التيتانيوم تزيد من التكلفة قليلاً، إلا أن التكلفة الإجمالية تتحدد في المقام الأول حسب شكل وشكل التيتانيوم الذي تحتاجه.
في DAXUN، نقدم مجموعة كبيرة من منتجات التيتانيوم، بما في ذلك الألواح والأنابيب والملفات والقضبان. سيؤثر طول وعرض وكمية كل صنف تطلبه على المبلغ الذي ستدفعه عند الدفع.
لسوء الحظ، من الصعب التوصل إلى سعر عبر الإنترنت دون معرفة الكثير عن مشروعك وما سيُستخدم التيتانيوم من أجله.
لحسن الحظ، فريق خبرائنا موجود دائماً لمساعدتك وتقديم المشورة لك بشأن احتياجاتك من التيتانيوم. من خلال إرسال بريد إلكتروني إلى [email protected]، سنكون قادرين على الرد عليك ببعض النصائح وعرض أسعار دقيق.
احرص على تضمين أكبر قدر ممكن من المعلومات حول درجة وشكل وكمية التيتانيوم التي تحتاجها للحصول على فهم أفضل لاحتياجاتك.
يتمتع فريق العمل في DAXUN بالخبرة والمعرفة والود. وبفضل سنوات خبرتهم الطويلة في هذا المجال، فهم يعرفون كل شيء عن التيتانيوم، بما في ذلك استخداماته وفوائده ودرجاته.
للحصول على تحديثات منتظمة عن التيتانيوم واستخداماته وتطبيقاته في مختلف الصناعات، احرص على الاطلاع على مدونتنا. لقد كتب خبراؤنا أدلة سهلة المتابعة يمكنك الرجوع إليها دائماً عندما تكون لديك أسئلة.
إذا كنت لا تزال تواجه مشكلة، فلا تتردد في الاتصال بنا؛ يسعدنا تقديم المساعدة.
من خلال إرسال بريد إلكتروني إلى [email protected]، ستتلقى رداً سريعاً. تأكد من تضمين أكبر قدر ممكن من التفاصيل في سؤالك حتى نتمكن من التوصية بالحل المناسب.
يُرجى ملء النموذج الموجود في صفحة “اتصل بنا”، أو الاتصال بمدير المبيعات لدينا على “+86 13382898899”، وسوف نتصل بك في أقرب وقت ممكن. واتسابنا على الإنترنت، وسيتم التحقق من البريد الإلكتروني ([email protected]) في غضون 6 ساعات. سيتم الرد على كل استفسار أو رسالة على الفور. بالإضافة إلى ذلك، نشارك معلومات السوق مع عملائنا كل أسبوع
يمكننا تقديم عينات من قضبان التيتانيوم لك للتحقق من الجودة. العينة مجانية وما عليك سوى دفع أجرة الشحن.
لقد قمنا بالتصدير إلى أكثر من 42 دولة، مثل كندا، وتشيلي، والكويت، وألمانيا، وكوريا الجنوبية، والمملكة العربية السعودية، وسنغافورة، وغيرها.
موك لدينا هو 300 كجم لقضيب التيتانيوم.
يمكن تسليم الطلبات التجريبية في غضون أسبوع. بالنسبة للطلبات العادية، يستغرق الأمر أسبوعين تقريباً.