CP Grade 3 Titanium Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:R50550 / CP TI50A
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Standards:ASTM B338
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

CP Grade 3 Titanium Pipe Manufacturer

CP Grade 3 titanium pipe is a commercially pure titanium product known for its balanced combination of moderate strength and excellent corrosion resistance. With titanium content of approximately 99.1% and controlled oxygen levels between 0.10-0.27%, Grade 3 offers higher mechanical properties than Grades 1 and 2. This specific oxygen content is the key differentiator, providing increased strength while retaining the inherent corrosion resistance of pure titanium.

In terms of mechanical performance, CP Grade 3 features a tensile strength around 450-485 MPa and a yield strength of 380-415 MPa, all while maintaining good ductility with 20-30% elongation. This makes it stronger than Grade 1 and Grade 2 but less strong than Grade 4 or titanium alloys like Grade 5, positioning it as a versatile “middle-strength” option within the commercially pure titanium series.

Applications of CP Grade 3 titanium

CP Grade 3 titanium pipes find extensive applications across various industries due to their excellent corrosion resistance and moderate strength. In the chemical processing industry, they are widely used for heat exchangers, condensers, and piping systems that handle corrosive chemicals and chlorides. The marine sector relies on these pipes for seawater cooling systems, desalination plants, and offshore platform components where resistance to saltwater corrosion is critical.

The oil and gas industry utilizes CP Grade 3 pipes for downhole tubing and surface equipment exposed to harsh environments. In power generation, particularly in geothermal and coastal plants, these pipes serve in condensers and heat transfer systems. The aerospace industry employs them for hydraulic systems and fuel lines where weight savings and corrosion resistance are priorities.

Medical applications include surgical implants and medical devices that benefit from titanium’s biocompatibility. Additionally, the food processing and pharmaceutical industries use CP Grade 3 pipes for equipment requiring sanitary conditions and resistance to cleaning chemicals. Their combination of weldability, formability, and durability makes them suitable for custom fabrication across these diverse applications.

Comparison of Grade 3 titanium pipes with other pure titanium grades

CP Grade 3 titanium pipe sits in a practical middle ground within the commercially pure titanium series. Think of it as a balance between strength and formability.

Grade 1 is the softest and most easily formed, perfect for complex deep-drawing applications, but it has the lowest strength. Grade 2 is the workhorse of the titanium industry—it’s slightly stronger than Grade 1 while still offering excellent corrosion resistance and weldability, which is why it’s the most commonly used grade.

This is where CP Grade 3 comes in. With a higher oxygen content, it provides significantly more strength than Grade 2, making it suitable for pressure vessels and piping systems where Grade 2 might not be robust enough. However, this extra strength means it’s slightly less formable than the lower grades.

Grade 4 is the strongest of all the commercially pure grades, but it sacrifices much of the ductility that makes the other grades easy to work with.

For most piping applications, the choice often comes down to Grade 2 versus Grade 3. If your project demands higher pressure ratings and mechanical strength, Grade 3 is the superior choice. If you need maximum formability for complex shapes, Grade 2 might be more suitable. Essentially, you choose Grade 3 when strength is a higher priority than ease of fabrication.

قراءة المزيد

البيانات

العنصر Content (%)
Titanium (Ti)
Balance (~99.1%)
Oxygen (O) 0.10 – 0.27
الحديد (Fe) ≤ 0.30
Carbon © ≤ 0.10
النيتروجين (N) ≤ 0.05
Hydrogen (H) ≤ 0.015
الممتلكات القيمة
الكثافة ~4.51 g/cm³
نقطة الانصهار
~1660–1670 °C
معامل المرونة
~103–107 GPa
التوصيل الحراري
~21.9 W/m·K (at 25°C)
المقاوماتية الكهربائية ~420 nΩ·m
الممتلكات القيمة
قوة الشد
~450–485 MPa
قوة المردود
~380–415 MPa
الاستطالة ~20–30%
الصلابة (برينل)
~200–240 HB

اختر Daxun لمساعدة مشروعك على الانطلاق.

اتصل بـ Daxun الآن

Advanced Production:Titanium seamless pipe

  • CP Grade 3 titanium pipes are typically manufactured according to major international standards such as ASTM B338, ASME SB338, ASTM B861 (for seamless pipes), and ASTM B862 (for welded pipes). They are readily available in a variety of sizes, with diameters ranging from 3.35mm to 152mm and wall thicknesses from 0.020″ to 0.220″, accommodating diverse project requirements.
اتصل بـ Daxun الآن

CP Grade 3 Titanium Tube Features

  • Balanced Properties: As a commercially pure titanium, it offers a great balance of moderate strength and excellent corrosion resistance, stronger than Grade 1 and 2.
  • Superior Corrosion Resistance: Exceptionally resistant to chloride and seawater environments, making it ideal for marine and chemical processing applications.
  • Good Fabricability: It is well-suited for forming, welding, and machining, allowing for easy manufacturing of complex components.
  • Biocompatible: Safe for use in medical implants and food processing equipment due to its non-toxic and hypoallergenic nature.
  • Cost-Effective: Provides better performance than lower grades without the high cost of titanium alloys, offering a practical solution for many industrial uses.
اتصل بـ Daxun الآن

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

اتصل بـ Daxun الآن

تقارير الاختبار

The test reports we provide include: Factory test certificate for CP Grade 3 titanium welded pipe and CP Grade 3 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

اتصل بـ Daxun الآن

Applications and standards

CP Grade 3 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
اتصل بـ Daxun الآن

الجودة والتسليم والتفتيش

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Titanium Welded Pipe and  Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • وقت التسليم لدينا يتوافق تمامًا مع العقد.
  • دعم الوكالات الخارجية للعملاء للذهاب إلى المصنع للفحص
  • دعم العينات المجانية لاختبار العملاء
  • دعم الفحص الموقعي أو فحص المصنع بالفيديو
اتصل بـ Daxun الآن

التعبئة والتغليف

تضمن شركة Daxun Alloy أفضل جودة للتغليف لأنها تلعب دورًا مهمًا في الشحن الدولي حيث تمر البضائع عبر قنوات مختلفة للوصول إلى الوجهة النهائية، لذلك نولي اهتمامًا خاصًا بالتغليف. نقوم بتغليف بضائعنا بعدة طرق حسب المنتج. نقوم بتغليف منتجاتنا بعدة طرق مثل:
- الصناديق والصناديق
- الغلاف المنكمش
- منصات خشبية
- صناديق خشبية

اتصل بـ Daxun الآن

الدعم الفني

إذا كنت بحاجة إلى أي مساعدة فنية إضافية، فسيكون من دواعي سرور أخصائي المعادن المقيم لدينا وموظفينا المطلعين تقديم المساعدة. بالإضافة إلى ذلك، تفتخر Daxun بوجود مختبر اختبار معتمد - وهو الأول من نوعه في صناعة مخزون المعادن المتعددة والبلاستيك. وهذا، في رأينا، يدل على تفانينا الثابت للجودة وفلسفتنا كمورد متكامل الخدمات.

Daxun CP Grade 3 Titanium TUBE Let your brand improve rapidly

CP Grade 3 titanium tube form (4)

أحدث مشاريع ومنتجات الحالة الساخنة

CP Grade 3 Titanium pipe and tube
CP Grade 3 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
What is the main difference between CP Grade 3 and CP Grade 2 titanium pipe?

The primary difference is the oxygen content, which directly impacts strength. CP Grade 3 has a higher oxygen content (0.10-0.27%) than Grade 2, giving it approximately 20-30% higher tensile and yield strength. This makes Grade 3 suitable for applications requiring more robust pressure handling and mechanical performance, while Grade 2 is often chosen for its superior formability.

Is CP Grade 3 titanium pipe weldable?

Yes, CP Grade 3 has excellent weldability using standard titanium welding procedures, most commonly TIG (GTAW) and MIG (GMAW) welding. It requires proper inert gas shielding (argon or helium) to prevent contamination of the weld pool, but it can be reliably welded to itself or other CP titanium grades.

When should I choose CP Grade 3 over a titanium alloy like Grade 5 (Ti-6Al-4V)?

You should choose CP Grade 3 when excellent corrosion resistance is your primary concern and the mechanical demands are moderate. Titanium alloys like Grade 5 offer much higher strength and are better for high-stress structural applications. CP Grade 3 is more cost-effective than titanium alloys and provides superior corrosion resistance in many environments, making it the ideal choice for piping, heat exchangers, and chemical processing equipment.

How does CP Grade 3 titanium compare to 316L stainless steel?

CP Grade 3 offers vastly superior corrosion resistance, especially in chloride environments like seawater, where 316L is prone to pitting and crevice corrosion. Titanium is also about 40% lighter than steel and has a much longer service life in aggressive environments. However, 316L has a lower initial material cost. The choice depends on whether long-term durability and corrosion resistance outweigh upfront cost.

هل تؤثر درجة التيتانيوم على التكلفة؟

على الرغم من أن درجة التيتانيوم تزيد من التكلفة قليلاً، إلا أن التكلفة الإجمالية تتحدد في المقام الأول حسب شكل وشكل التيتانيوم الذي تحتاجه.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

لسوء الحظ، من الصعب التوصل إلى سعر عبر الإنترنت دون معرفة الكثير عن مشروعك وما سيُستخدم التيتانيوم من أجله.

لحسن الحظ، فريق خبرائنا موجود دائماً لمساعدتك وتقديم المشورة لك بشأن احتياجاتك من التيتانيوم. من خلال إرسال بريد إلكتروني إلى [email protected]، سنكون قادرين على الرد عليك ببعض النصائح وعرض أسعار دقيق.

احرص على تضمين أكبر قدر ممكن من المعلومات حول درجة وشكل وكمية التيتانيوم التي تحتاجها للحصول على فهم أفضل لاحتياجاتك.

كيف تحصل على عرض أسعار أو تفهم معلومات السوق في أسرع وقت ممكن؟

يُرجى ملء النموذج الموجود في صفحة “اتصل بنا”، أو الاتصال بمدير المبيعات لدينا على “+86 13382898899”، وسوف نتصل بك في أقرب وقت ممكن. واتسابنا على الإنترنت، وسيتم التحقق من البريد الإلكتروني ([email protected]) في غضون 6 ساعات. سيتم الرد على كل استفسار أو رسالة على الفور. بالإضافة إلى ذلك، نشارك معلومات السوق مع عملائنا كل أسبوع

هل يمكنني الحصول على بعض العينات؟

يمكننا تقديم عينات من صفائح الفولاذ المقاوم للصدأ لك للتحقق من الجودة. العينة مجانية وما عليك سوى دفع أجرة الشحن.

ما هي الدول التي قمت بتصديرها بالفعل؟

لقد قمنا بالتصدير إلى أكثر من 42 دولة، مثل كندا، وتشيلي، والكويت، وألمانيا، وكوريا الجنوبية، والمملكة العربية السعودية، وسنغافورة، وغيرها.

ما هي مدة التوصيل؟

يمكن تسليم الطلبات التجريبية في غضون أسبوع. بالنسبة للطلبات العادية، يستغرق الأمر أسبوعين تقريباً.

أرسل استفسارك اليوم
اقتباس سريع