Daxun is an excellent manufacturer of grade 12 (Ti-0.3Mo-0.8Ni) titanium rods and bars.

  • Titanium bar grade: Grade 12-Ti / UNS R53400
  • Tipos de barras de titânio: barras laminadas, barras trefiladas, barras de titânio forjadas
  • Titanium bar density: The density of grade 12 titanium is 4.51 g/cm³
  • Principais normas: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.

O líder mundial em serviços de fabrico de barras de titânio comercialmente puro

Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 12 titanium alloy rods.

Grade 12 titanium bar (Ti Grade 12 / UNS R53400) is a nickel-molybdenum-enhanced, commercially pure (CP) titanium alloy specifically engineered for superior corrosion resistance in aggressive environments. It consists of titanium (≥99%) with strategic additions of 0.6–0.9% nickel (Ni) and 0.2–0.4% molybdenum (Mo), which significantly enhances its electrochemical properties. This nickel-molybdenum modification substantially improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice corrosion—conditions where standard CP grades like Grade 2 would exhibit accelerated degradation. While maintaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 12 offers enhanced performance at elevated temperatures (up to ~315°C/600°F) and in moderately reducing or acidic environments. Its passive oxide layer, reinforced by the nickel-molybdenum combination, provides exceptional protection against chemical attack, making it one of the most cost-effective corrosion-resistant metallic materials available.

Where is Grade 12 titanium bar used?

Grade 12 titanium bar is widely utilized in chemical processing for essential components such as heat exchangers, piping systems, vessel linings, and agitators handling acids, chlorides, or organic compounds. In marine and offshore applications, it serves in seawater desalination plants, condenser tubing, and offshore platform components exposed to high-salinity conditions. The alloy also performs exceptionally well in oil and gas production equipment, pulp and paper processing machinery, and power generation systems due to its durability and corrosion resistance. Despite its moderate premium over standard grades—justified by its alloying elements—Grade 12 delivers outstanding lifecycle value by reducing maintenance requirements, extending service intervals, and minimizing replacement costs in corrosive service. Its reliability in preventing premature failures ensures operational continuity and cost efficiency in applications ranging from chemical processing plants to marine infrastructure, establishing it as an optimal solution for demanding corrosion challenges where budget constraints exist.

Daxun é a sua empresa de produção de barras de liga de titânio de confiança. Daxun produz todos os tipos de ligas de titânio, incluindo titânio comercialmente puro série CP, série de liga de titânio, liga de níquel de titânio, etc. Têm um desempenho fiável e proporcionam um elevado desempenho para as suas aplicações críticas. Em várias indústrias e aplicações, pode confiar nas barras de liga de titânio da Daxun para alta resistência, alta temperatura e ambientes corrosivos. Durante décadas, a Daxun Metals tem-se empenhado em produzir soluções de liga de titânio de alta engenharia para enfrentar os desafios mais severos.

Ler mais

Dados

Especificação Detalhes
Material Titanium rod and bar Grade 12 (UNS R53400)
Padrão ASTM B348, ASTM SB348, AMS 4921, AMS 4902
Dimensões EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
Gama de diâmetros 0.125″ – 14″ (3.175mm – 355.6mm), custom
Comprimento Intervalo Up to 240″ (6096mm), custom
Acabamento Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black
Acabamento da superfície Estirado a frio, rectificado sem centros, polido ou torneado em bruto, preto, acabamento NO.4, acabamento BA, acabamento mate, etc.
Estado Endurecido e temperado, recozido
Tolerância Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
Formulário Barras quadradas de titânio, lingotes de titânio, barras redondas de titânio, barras rectangulares de titânio, barras triangulares de titânio, barras forjadas de titânio, barras hexagonais de titânio, etc.
Elemento Minimum (%)
Maximum (%)
Titanium (Ti) Equilíbrio Equilíbrio
Molibdénio (Mo) 0.25 0.4
Níquel (Ni) 0.6 0.9
Ferro (Fe) 0.3
Oxygen (O) 0.25
Carbon © 0.08
Azoto (N) 0.03
Hydrogen (H) 0.015
Outros elementos 0.40 (total)

 

Imóveis Minimum Requirement Typical Value Unit Test Method
Resistência à tração 483 520–620 MPa
ASTM E8/E8M
Resistência ao escoamento (0,2% offset) 345 380–480 MPa
ASTM E8/E8M
Alongamento 18 22–30 %
ASTM E8/E8M
Dureza ≤ 200 (HV) 150–180 (HV) Vickers ASTM E10
Impact Toughness Not specified 40–60 J ASTM E23

Elevated Temperature Performance

Temperature (°C)
Resistência à tração (MPa) Yield Strength (MPa)
Alongamento (%)
100 450–500 320–370 20–25
200 400–450 280–330 18–23
300 350–400 240–290 15–20
Imóveis Value/Range Unit
Densidade 4.48 g/cm³
Ponto de fusão 1650 ± 20 °C
Condutividade térmica 7.2 (at 25°C) W/m·K
Specific Heat 560 (at 25°C) J/kg·K
Resistividade eléctrica 1.7 μΩ·m
Suscetibilidade magnética Paramagnetic

Escolha a Daxun para ajudar o seu projeto a arrancar.

Contactar a Daxun agora

DAXUN® Grade 12 Titanium Rod Features

O DAXUN® Ti Grau 5 é uma barra de liga de titânio (6al-4v) que apresenta:

  • Boa conformabilidade e soldabilidade a quente;
  • A resistência à tração pode atingir 1000MPa;
  • Trabalho dimensional a alta temperatura
  • Insensível à água do mar ou à água do mar;
  • Não é afetado por vários meios corrosivos;
  • Elevada resistência e boa tenacidade;
  • Resistir ao início e à propagação de fissuras.
Contactar a Daxun agora

Vantagens da fábrica Daxun

O conceito de “Gestão de Excelência de Desempenho” da Daxun promove o modelo de gestão “PDCA + Lean”. O cartão de visita da empresa diz “Daxun = Qualidade fiável”. A Daxun utiliza o sistema ERP para alcançar a rastreabilidade total da variedade, especificação e origem de cada barra de titânio, e defende e incentiva a anti-falsificação da indústria. A Daxun confia na tecnologia para processamento e personalização, e a alta precisão e a alta qualidade são as referências da indústria; em termos de serviço, promove a gestão do ciclo de vida do produto, fornece soluções profissionais de seleção e processamento de materiais antes das vendas, monitoriza rigorosamente durante as vendas e fornece garantias de serviço sem preocupações após as vendas.

Contactar a Daxun agora

Grade 12 Titanium Rod Production Method

A Daxun produz barras de titânio de alta qualidade com alto desempenho, e também pode fabricar de acordo com o acordo do cliente:

  • Os lingotes de titânio têm de passar por tratamento térmico e maquinagem, testes ultra-sónicos de imersão, testes de propriedades mecânicas, inspeção estrutural macroscópica e microscópica e outros processos. Processo de produção: barras de titânio laminadas a quente - alta eficiência, desempenho estável, barras de titânio forjadas - tamanho flexível, forjamento multi-fogo, melhorar o desempenho abrangente de barras de titânio, barras de titânio estiradas a frio - geralmente pequenas barras de titânio de alta precisão; as barras de titânio acima são todas entregues com superfície brilhante.
Contactar a Daxun agora

Relatórios de ensaio

Os relatórios de teste que fornecemos incluem: Haste de titânio de grau 2 e barra redonda de titânio de grau 2 Certificado de teste de fábrica, EN 10204 3.1, relatório químico, relatório mecânico, relatório de teste PMI, relatório de inspeção visual, relatório de inspeção de terceiros, relatório de laboratório aprovado pela NABL, relatório de teste destrutivo, relatório de teste não destrutivo. (Daxun fornecerá de acordo com os requisitos do cliente)

Contactar a Daxun agora

Grade 12 Rods Applications and Standards

Grade 12 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Indústria aeroespacial, construção naval, indústria do petróleo e do gás, engenharia naval, fábricas de produtos químicos, maquinaria industrial, indústria eléctrica, indústria do papel e da pasta de papel, indústria de transformação de alimentos, refinarias, indústria militar, equipamento farmacêutico e de transformação de alimentos, etc.
  • Especificações: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
  • Normas: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Contactar a Daxun agora

Qualidade, entrega, inspeção

A Daxun realiza vários testes de garantia de qualidade, estes testes incluem testes mecânicos como a área de tração, análise química, identificação positiva de material - teste PMI, testes micro e macro, teste de corrosão intergranular (IGC), teste de deteção de falhas por ultra-sons, teste de resistência e pitting, teste de dureza, identificação positiva de material, teste de expansão, etc. Todos estes testes garantem que o material da barra de titânio de grau 2 e da barra redonda de titânio de grau 2 é adequado para a aplicação pretendida. Durante o processo de produção, medimos o diâmetro, a espessura e a superfície do produto.

  • O nosso prazo de entrega está estritamente de acordo com o contrato.
  • Apoio a agências terceiras do cliente para se deslocarem à fábrica para inspeção
  • Apoio a amostras gratuitas para teste do cliente
  • Apoio à inspeção de fábrica no local ou por vídeo
Contactar a Daxun agora

Embalagem

A Daxun Alloy assegura a melhor qualidade de embalagem, uma vez que esta desempenha um papel importante no transporte internacional de mercadorias, onde as mercadorias passam por vários canais para chegar ao destino final, pelo que prestamos especial atenção à embalagem. Embalamos os nossos produtos de várias formas, consoante o produto. Embalamos os nossos produtos de várias formas, tais como:
- Caixas e caixotes
- Película retrátil
- Paletes de madeira
- Caixas de madeira

Contactar a Daxun agora

Apoio técnico

Se necessitar de qualquer assistência técnica adicional, o nosso metalúrgico residente e a nossa equipa experiente terão todo o prazer em ajudar. Além disso, a Daxun possui um laboratório de testes certificado - o primeiro na indústria de inventário de multi-metal e plástico. Isto, na nossa opinião, demonstra a nossa dedicação inabalável à qualidade e a nossa filosofia como um fornecedor de serviço completo.

Daxun Grade 12 Titanium Rods help your brand improve quickly

TAMANHO NOMINAL h5 h6 h7 h8 h9 H10 H11 h12
DIÂMETRO mm
~ a 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
de 3 a 6 anos +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
mais de 6 a 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
mais de 10 a 18 anos +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
mais de 18 a 30 anos +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
mais de 30 a 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
mais de 50 a 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
mais de 80 a 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
mais de 120 a 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
mais de 180 a 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

Haste de titânio

Produtos e projectos recentes de casos quentes

Grade 7 Titanium rod and bar
Varão e barra de titânio
Varão e barra de titânio
Varão e barra de titânio
Varão e barra de titânio
Varão e barra de titânio
Titanium Alloy Bar, Titanium Bar Grade 12/UNS 53400

Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 12 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.


ESPECIFICAÇÕES

ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4924 – Titanium Alloy Bars and Billets, Grade 12


TRATAMENTO TÉRMICO

When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).

DAXUN Grade 12 alloy can be heat treated in a variety of ways:

  1. Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
  2. Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool

DUREZA

Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.


Forgeability / Formability

Grade 12 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.

Grade 12 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).


Maquinabilidade

Grade 12 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The nickel-molybdenum content does not significantly affect machinability compared to other CP titanium grades.


Soldabilidade

Grade 12 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The nickel-molybdenum addition enhances weld integrity in corrosive environments.


Considerações especiais

Grade 12 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The nickel-molybdenum content provides additional protection against corrosion in contaminated conditions.


Size Range

Grade 12 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 - 400 mm (laminados a quente, pelados)
Tolerances: h11–h5 (ISO 286-2)
Tolerâncias mais apertadas ou diferentes disponíveis a pedido
Comprimentos até 9.000 mm, consoante o diâmetro
Para diâmetros maiores, podem ser acordados outros comprimentos de barra e tolerâncias mediante pedido


Availability Grade 7 Titanium Rods

Processing options include:

  • Desenhar, endireitar
  • Desenho, endireitamento, polimento
  • Desenho, retificação, polimento
  • Estiramento, endireitamento, retificação, polimento
  • Estiramento, recozimento, endireitamento
  • Trefilagem, recozimento, polimento
  • Estiramento, recozimento, retificação, polimento
  • Trefilagem, recozimento, endireitamento, retificação, polimento

Produzimos barras de acordo com as suas necessidades.
Excelente superfície e retidão, arredondamento perfeito e tolerâncias de diâmetro mais apertadas (de acordo com a norma ISO 286-2 até h5). Disponível em estado rectificado, esmerilado e polido.


Serrar

  • Serras de fita (até Ø510 mm)
  • Bench band saws (up to 6,000 x 3,000 x 400 mm)
  • Máquinas de serrar de alto desempenho para serrar com precisão

Titanium Bar End Machining

  • Uma ou duas faces
  • Chanfro 90° (45°)
  • Ponto 60° (30°)
  • Extremidade plana
  • Centrado

Delivery Form

  • ASTM American Society for Testing and Materials Standards
  • AMS American Aerospace Materials Standards
  • NACE American Association of Corrosion Engineers International Standards
  • ASME American Society of Mechanical Engineers Standards
  • GB Chinese National Standards
  • GJB Chinese National Military Standards
  • ISO International Standards
  • DIN German Standards
  • PT European Standards
  • API American Petroleum Institute Standards

Detection Method

Ensaios não destrutivos > Ensaios 100%
Testing methods:

  • Eddy current testing / eddy current crack testing
  • Superfície sem defeitos (nível 4)
  • Diâmetro do furo de fundo plano 0,7 mm e 0,4 mm
  • Blind area can be cut off according to fixed length > Test to the end of the bar
  • Ensaio ultrassónico de diâmetro total

Os nossos serviços de material de barras de titânio

As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.

We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.

Se tiver um compromisso de fornecimento a longo prazo, pode estabelecer um acordo-quadro com a Daxun. Garantimos preços e quantidades durante um determinado período.

Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 12 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.


Informações para encomenda

Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.

Qual é o melhor grau de titânio?

O tipo de liga de titânio de que necessita depende do projeto em que está a trabalhar, uma vez que cada tipo tem benefícios diferentes.

Todos os graus de liga de titânio são extremamente fortes e resistentes à corrosão, o que significa que continuarão a funcionar bem nas condições mais adversas.

Os graus mais elevados de liga de titânio (5-12) são ligas concebidas para benefícios específicos. Por exemplo, a liga de titânio de grau 12 tem uma excelente resistência ao calor, o que a torna uma escolha perfeita para permutadores de calor de casco e tubo, tubagens hidráulicas e equipamento da indústria química.

Os graus 1-4 são ligas de titânio puro e são a escolha perfeita se precisar de um material soldável e dúctil para sistemas de tubagem e tubos. Encontrará graus inferiores utilizados nas indústrias marinha e industrial.

Se está a iniciar um projeto e não tem a certeza de qual o melhor tipo de liga de titânio para si, contacte-nos hoje mesmo; teremos todo o gosto em ajudá-lo.

Em que é que os graus superiores de titânio são diferentes dos graus inferiores?

Na DAXUN, oferecemos uma vasta gama de graus de liga de titânio, do grau 1 ao grau 12.

Os graus 1-4 são titânio puro, enquanto os graus superiores são ligas.

Os tipos de liga são populares pela sua elevada relação resistência/peso.

O grau de liga de titânio mais utilizado que encontramos é o grau 5. Embora continue a ser rica em titânio, esta classe é uma das mais fiáveis porque pode suportar temperaturas até 600°F e resistir a condições extremas.

As qualidades superiores são preferidas por indústrias como a aeroespacial e a marítima devido à sua resistência ao desgaste e à corrosão.

Por outro lado, os graus inferiores são utilizados principalmente para soldadura devido à sua menor resistência.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

O grau do titânio afecta o custo?

Embora o grau de titânio aumente ligeiramente o custo, o custo total é determinado principalmente pela forma e pelo formato do titânio que pretende.

Na DAXUN, oferecemos uma vasta gama de produtos de titânio, incluindo placas, tubos, bobinas e barras. O comprimento, a largura e a quantidade de cada artigo que pretende afectam o montante a pagar no momento do pagamento.

Infelizmente, é difícil apresentar um preço online sem saber muito sobre o seu projeto e para que será utilizado o titânio.

Felizmente, a nossa equipa de especialistas está sempre aqui para o ajudar e aconselhar nas suas necessidades de titânio. Ao enviar um e-mail para [email protected], poderemos responder-lhe com alguns conselhos e um orçamento exato.

Certifique-se de que inclui o máximo de informação possível sobre o grau, a forma e a quantidade de titânio de que necessita para compreender melhor as suas necessidades.

Onde posso obter mais informações sobre os tipos de titânio?

A equipa da DAXUN é experiente, conhecedora e simpática. Com anos de experiência no sector, sabem tudo sobre o titânio, incluindo as suas utilizações, benefícios e graus.

Para obter actualizações regulares sobre o titânio, as suas utilizações e as suas aplicações em todas as indústrias, não deixe de consultar o nosso blogue. Os nossos especialistas escreveram guias fáceis de seguir que pode consultar sempre que tiver dúvidas.

Se continuar a ter problemas, não hesite em contactar-nos; teremos todo o gosto em ajudar.

Ao enviar uma mensagem de correio eletrónico para [email protected], receberá uma resposta rápida. Certifique-se de que inclui o máximo de pormenores possível na sua pergunta para que possamos recomendar uma solução adequada.

Como obter uma cotação OU compreender a informação de mercado o mais rapidamente possível?

Preencha o formulário na página “Contacte-nos” ou ligue para o nosso gestor de vendas através do número “+86 13382898899” e entraremos em contacto consigo o mais rapidamente possível. O nosso WhatsApp está online e o e-mail ([email protected]) será verificado no prazo de 6 horas. Todas as perguntas ou mensagens serão respondidas prontamente. Além disso, todas as semanas partilhamos informações de mercado com os nossos clientes

Podem dar-me algumas amostras?

Nós podemos fornecer amostras de haste de titânio para você verificar a qualidade. A amostra é grátis e você só paga o frete.

Para que países já exportou?

Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.

Qual é o vosso MOQ?

Our MOQ is 300 Kg for titanium rod.

Qual é o prazo de entrega?

As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.

Envie hoje o seu pedido de informação
Orçamento rápido