Daxun is a 201 stainless steel sheet supplier from China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 201 stainless steel plates to the world.
- Grade: AISI 201/S20100
- Manufacture: cold rolled plate, hot rolled plate, forged plate
- Standard: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type: cold rolled thin plate and hot rolled thick plate
- Surface: 2B, NO.1, NO.4, HL, BA, 8K etc
- Comprimento: 2438mm3048mm6000mm pode ser personalizado
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong
Global leader in stainless steel sheet fabrication services
Daxun stocks 201 stainless steel plates (hot rolled and cold rolled). Because a portion of the nickel used in 300 series stainless steels (such as Type 304) is replaced with manganese, the 201 grade alloy is generally a high performance, lower cost, more stable austenitic stainless steel. In addition, the chemical composition of the 201 stainless steel provides better annealed mechanical properties than Type 304, which may provide further advantages in terms of weight reduction. Because the tensile strength of Type 201 is approximately 10% higher than that of Type 304, thinner gauges can be used, using less material overall. However, Type 201 stainless steel has lower chromium and nickel contents, so it is not as corrosion resistant as Type 304. 201 grade stainless steel is frequently used in domestic and commercial food service applications, construction applications, appliances, and other uses.
Corrosion Resistance: 201 stainless steel plate has excellent corrosion resistance suitable for both indoor and outdoor applications. Its excellent corrosion resistance. Stainless steel sheet has excellent resistance to atmospheric conditions, moisture and specific chemicals, thus guaranteeing long-lasting performance and durability. By providing excellent resistance to atmospheric conditions, moisture and specific chemicals, it guarantees long-lasting performance and durability.
High Strength: 201 stainless steel plate is able to withstand heavy weight and pressure due to its high tensile strength. Steel sheet is able to withstand large mass and pressure due to its high tensile strength. Parts and structural components that require extreme durability.
Steel sheet is a beautiful material that can add a touch of elegance to any project due to its smooth, polished surface. It is suitable for architectural elements, kitchen utensils and decorative applications due to its easy-to-clean and shiny surface. It is perfect for architectural elements, kitchen utensils and decorative applications due to its easy-to-clean and shiny surface.
It is a cost-effective solution compared to other grades of stainless steel without sacrificing quality. It is favored by budget-constrained projects due to its reliable performance and reasonable price. It is the choice of budget-constrained projects due to its reliable performance and reasonable price.
At Daxun, we offer high quality 201 Stainless Steel Plate at very competitive prices. We understand the importance of maintaining the superior quality of metal sheet products while keeping them affordable. Contact us today to secure the most competitive prices for SS 201 Stainless Steel Plate and experience the superior quality of our products. Contact us today to secure the most competitive prices for 201 Stainless Steel Plate and experience the superior quality of our products.
Dados técnicos
- Parâmetro
- Ingredients and properties
- PHYSICAL PROPERTIES:
- Propriedades mecânicas
| Product Parameters: 201/201LN Stainless Steel Sheet/Plate | |||
| Largura | 10mm~2500mm | ||
| Espessura | 0.2mm~100mm | Thickness tolerance | +/-0.03mm |
| Padrão | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| Superfície | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc | ||
| specification | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Mill Origin | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Certification | ISO, SGS, BV, TUV,CE etc | ||
| Padrão | Werkstoff Nr. | UNS | JIS | BS | GOST | AFNOR | PT | CN |
| SS 201 | 1.4372 | S20100 | SUS 201 | 904S13 | STS 317J5 | Z2 NCDU 25-20 | X1NiCrMoCu25-20-5 | 1Cr17Mn6Ni5N |
| Grau | C | Mn | Si | P | S | Cr | Ni | N |
| 201 | 0.25% | 5.5%-7.5% | 1% | 0.60% | 0.30% | 16%-18% | 3.5%-5.5% | 0.25% |
| Densidade (lb./in^2) @ RT | 0.283 | |
| Módulo de elasticidade em tensão (psi x 10^6) | 28.6 | |
| Calor específico (BTU/o F/lb.) | 32 a 212 oF | 0.12 |
| Condutividade térmica (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| Coeficiente médio de expansão térmica (pol. x 10^-6 por o F) | 32 a 212oF | 8.7 |
| 32 a 600oF | 9.7 | |
| 32 a 1.000oF | 10.2 | |
| Resistividade eléctrica (micro ohms - cm) | a 70oF | 69 |
| Gama de pontos de fusão (oF) | 2550/2650 | |
| Resistência à oxidação - Serviço contínuo (oF) | 1550 | |
| Resistência à oxidação - Serviço intermitente (oF) | 1500 |
| Resistência à tração | 99,400 PSI = 520MPa |
| Yield Strength | 42,400 PSI = 275MPa |
| Alongamento | 55 – 60% |
| Módulo de elasticidade | 29,000,000 psi = 203000MPa |
| Hardness Requirement | 183 n/was (MPa) |
| Densidade | .280 LBS /cubic inch(density 7.93g/cm3) |
Escolha a Daxun e deixe os seus clientes satisfeitos.

Entrega rápida
Daxun provides customers with timely and fast delivery of 201 stainless steel plate products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Maquinação avançada
Daxun’s typical service of “more, faster, better and cheaper” for 201 stainless steel plate materials starts with Daxun’s stainless steel varieties, specifications and spot inventory. It has strategic resource support from many large steel mills at home and abroad to ensure a stable supply chain and meet customers’ personalized needs for specific materials. It can be called the “Wal-Mart” of the stainless steel industry. With more than 20 years of experience, it has established the brand image of “Look for Daxun for stainless steel plates” in the Chinese market.


Resposta rápida
- 201 stainless steel plate has high reliability
- Chemical composition of pure steel
- Easy to weld and excellent welding effect
- Optimal shape and excellent precision
- Long service life
- Relatively low cost
- Fácil de processar
201 stainless steel plate packaging
Daxun Alloy ensures the best quality of 201 stainless steel plate packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Caixas e caixotes
- Papel kraft + paletes de madeira
- Película retrátil
- Paletes de madeira sem fumigação
- Caixas de madeira sem fumigação


SS 201 Plate Surface Treatment
1D: A superfície é mate com uma forma de partícula descontínua.
2D: Branco com um tom prateado.
2B: Cinzento prateado com melhor brilho e nivelamento do que a superfície 2D.
Ba: Superfície próxima do espelho com excelente brilho e refletividade.
N.º 3: Bom brilho e superfície rugosa.
N.º 4: A superfície tem linhas finas e bom brilho.
HL: Cinzento prateado com cabelo dourado.
8K: Superfície espelhada.
201 Stainless Steel Sheet Processing:
- Processamento de gravura
- Processamento de soldadura
- Processamento de dobragem
- Processamento de relevo
- Processamento de jato de areia
- Processamento de polimento
- Processamento de perfuração
- Processamento de estampagem
- Processamento de corte

201 plate stainless steel Features
Daxun Deixe a sua marca melhorar rapidamente
- Galeria
- Outras séries de produtos
- Tolerância
- Estado de entrega
| Grau | Tipo | Espessura | Superfície |
| Austenítico | 304/304H/304L/304J1 | 0,25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrite ultra-puro | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Grau | Tipo | Espessura | Original |
| Aço resistente ao calor | 309S | 0,5-40mm | CHN |
| 310S | 0,5-40mm | CHN | |
| Aço duplex | 2101 | 1,5-50 mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0,5-60mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Aço superaustenítico | N08904 | 0,6-50mm | SWE / JPN / CHN |
| S31254 | 0,5-50mm | SWE / JPN / CHN | |
| N08926 | 0,5-50mm | SWE / JPN / CHN | |
| N08367 | 0,5-50mm | SWE / JPN / CHN | |
| Liga à base de níquel | N08031 | 1.0-50mm | EUA / JPN / GER |
| N08810/N08800 | 0,8-50mm | EUA / JPN / CHN | |
| N08028 | 1,0-20mm | EUA / GER / JPN | |
| N08020 | 1,0-20mm | EUA / GER / JPN | |
| N08825 | 0,8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50mm | EUA / GER / JPN | |
| N06022 | 1.0-50mm | EUA / GER / JPN | |
| N06625 | 0,8-20mm | EUA / GER / CHN | |
| N04400 | 1,0-20mm | EUA / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20mm | EUA / JPN | |
| Titânio | TA1/Gr1 | 0,5-50mm | JPN / CHN |
| TA2/Gr2 | 0,5-50mm | JPN / CHN | |
| Material de soldadura | ERNiCrMo-13 | 1.2、2.4mm | ALEMANHA |
| ERNiCrMo-3 | 2,4 mm | ALEMANHA | |
| ERNiCrMo-4 | 2,4 mm | EUA |
| Tolerância para chapa 2B | |||
| Tamanho | Classificação de tolerância | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Tolerância para chapa laminada a quente n.º 1 | |||
| Tamanho | Classificação de tolerância | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Entrega Estado Escolha | Estado da superfície |
| Laminados a frio | 2B |
| 2D | |
| BA | |
| Fio de cabelo | |
| N.º 3 | |
| N.º 4 | |
| 6K | |
| 8K | |
| Nota: | |
| 1. Se necessitar de um estado de entrega diferente do acima indicado, por favor confirme connosco. | |
| 2. Em caso de pedido de informação ou de encomenda, agradecemos que nos informe de qualquer requisito adicional não indicado aqui. | |
| Estado de entrega | |
| Entrega Estado Escolha | Estado da superfície |
| Laminados a quente | N.º 1 |
| N.º 3 | |
| N.º 4 | |
| 6K | |
| 8K | |
| Em conserva | |
| Nota: | |
| 1. Se necessitar de um estado de entrega diferente do acima indicado, por favor confirme connosco. | |
| 2. Em caso de pedido de informação ou de encomenda, agradecemos que nos informe de qualquer requisito adicional não indicado aqui. | |
The surface and shape of 201 stainless steel plate (7)
Informações disponíveis para consulta e descarregamento
Daxun é um fabricante confiável de chapa de aço inoxidável
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Produtos e projectos recentes de casos quentes
Produtos relacionados (13)
Daxun stainless steel plates are in high demand, have good quality, and are honest and trustworthy.
- A Daxun International está presente no mercado internacional há mais de dez anos. Em 2022, as suas receitas de exportação ultrapassaram os $100 milhões, e o seu volume de exportação situou-se entre as principais empresas chinesas de transformação de aço inoxidável. Para servir os mercados estrangeiros, construímos três instalações de serviços de exportação na China e colaborámos com organizações de engenharia, siderurgias e empresas de comércio internacional. Continuamos a melhorar as nossas capacidades de serviço, estabelecendo três bases de serviços de exportação na China e colaborando com empresas de engenharia, siderurgias e empresas de comércio internacional para crescer em novos mercados.
- A Daxun tem relações de longa data com dezenas de siderúrgicas conhecidas em todo o mundo, fornecendo 30.000 toneladas de chapas de aço inoxidável padrão e 20.000 toneladas de metais como aço duplex, ligas à base de níquel e aço resistente ao calor. Os materiais de aço inoxidável da Daxun são de qualidade consistente e nunca são contrafeitos. Os tipos, as especificações e os pesos de entrega cumprem rigorosamente as normas.
- A Daxun possui vários equipamentos de processamento de chapas de aço inoxidável, um centro profissional de testes físicos e químicos e linhas de produção de “corte, moagem, formação, chanfradura, soldadura, tratamento térmico, maquinagem e pulverização”. Os serviços são prestados em cerca de 30 sectores, incluindo veículos, electrodomésticos, elevadores, novas energias, semicondutores de vácuo, alimentos e bebidas/biofermentação, petroquímica e equipamento energético. Colaborar com siderurgias, institutos de investigação e outras organizações para oferecer serviços abrangentes que vão desde a conceção de projectos e desenvolvimento de materiais até à otimização de processos de processamento e fabrico.
Stainless steel materials “more, faster, better, and cheaper” customised services
- First, it refers to Daxun’s stainless steel plate kinds and specifications, as well as its spot inventories.Daxun has strategic resource assistance from many large steel mills at home and abroad, ensuring the stability of the stainless steel plate supply chain and meeting clients’ individualised needs on specific materials.
- Em segundo lugar, a tecnologia de transformação da Daxun é diversificada.
processes, including stainless steel plate cutting, grinding, cutting, forming, welding, and machining, to provide customers with “one-stop” service.
A Daxun presta serviços a um grande número de consumidores em diversos sectores.
- Daxun’s stainless steel company focuses on the key sectors of equipment manufacture. far, it has served over 30,000 customers, including over 10,000 active customers from more than 30 industries and a big number of major businesses. This demonstrates Daxun’s extensive service experience, as well as its widespread consumer recognition across industries.
Customers with urgent needs can rest assured that we will supply stainless steel plate products on time and quickly.
- Por detrás da velocidade está o apoio do sistema, incluindo o fluxo de informação, a logística e o fluxo de capital. Por exemplo, em termos de fluxo de informação, os dados das encomendas da Daxun são enviados para o sistema de logística em tempo real, com uma ligação perfeita; em termos de logística, o centro de processamento está perto de portos, rios e mares, com uma programação razoável, resposta rápida, ligação de armazenamento e transporte e carregamento eficiente para garantir que a tarefa é concluída a tempo.
Oferecemos uma excelente qualidade e serviços de alta qualidade.
- Quality is belief, and integrity is a business card. Daxun pioneered the concept of “excellent performance management” and promoted the “PDCA+Lean” management model, making “Daxun = assured quality” the company’s business card. In terms of materials, Daxun Stainless Steel has achieved full traceability of each steel plate from the ERP system, including varieties, specifications, and origins, and advocated and encouraged industry anti-counterfeiting.
- Daxun Stainless Steel relies on technology for processing, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, closely monitors during sales, and provides worry-free service guarantees after sales.
Poupamos tempo, materiais e energia aos nossos clientes e, em última análise, poupamos-lhes dinheiro.
As vantagens profissionais da Daxun permitem-nos fornecer as recomendações de materiais mais rentáveis com base nas necessidades do cliente e minimizar os custos para os clientes através de métodos como o processamento contínuo e o processamento de nesting.
Os nossos métodos inovadores de processamento de encaixe optimizam a utilização do material e do corte.
Simultaneamente, a Daxun consegue uma redução contínua dos custos e uma melhoria da eficiência através da promoção de actividades de melhoria optimizada e da transferência dos benefícios para os clientes. A Daxun também possui um sistema completo de rastreabilidade de produtos e um tratamento atempado de objecções de qualidade, o que alivia as preocupações dos clientes.
Leading Stainless Steel Sheet Suppliers in China
Contact the top suppliers in China for stainless steel sheets (steel plates) in a variety of finishes. You need no other stainless steel sheet supplier than Daxun Alloys, who offer free cutting services and delivery times as short as 5-7 days.
201 Stainless Steel Plate in a Variety of Finishes
Our stainless steel sheets (sometimes called steel sheets) are available in a range of beautiful finishes: brushed finish, 2B smooth finish or 8K mirror finish.
The finished side of each stainless steel sheet we supply is coated with a film. This film is easily peeled off after fabrication or installation and protects the surface of the material from wear and marks. The back side is unfinished.
201 Stainless Steel Plate is the most commonly used variety. It is easily weldable, formable, and has good corrosion resistance.
We can assist in providing stainless steel sheets in any required size.
To meet your specific requirements, our stainless steel sheets are available in three finishes and a variety of sizes. We can readily provide any custom size you may need with our free unlimited cutting service.
Temos capacidade para satisfazer qualquer necessidade de tamanho entre 0,3 e 30 mm de espessura e entre 50 x 50 mm e 2500 x 1250 mm de tamanho. Além disso, fornecemos corte ilimitado gratuito em cada encomenda, utilizando uma máquina de corte de última geração para satisfazer com precisão os seus requisitos.
Order Stainless Steel Sheets by Phone or Online.
There has never been an easier way to get stainless steel sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email [email protected].
O nosso prazo de entrega é de apenas um a dois dias.
Caraterísticas:
Este tipo é mais resistente à corrosão e à corrosão por pite do que o 304 e oferece maior resistência a temperaturas elevadas. Além disso, o 316L é uma variação de carbono extra baixo que ajuda a evitar a precipitação de carbonetos devido à soldadura.
Nota de segurança importante:
The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any stainless steel sheet. We remind users to use, install and handle these devices with care.
Podemos fornecer amostras de chapas de aço inoxidável para que possa verificar a qualidade. A amostra é grátis e o cliente só paga o frete.
Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.
O nosso MOQ é de 1 tonelada para chapas de aço inoxidável.
As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.