{"id":17064,"date":"2025-06-05T16:12:23","date_gmt":"2025-06-05T08:12:23","guid":{"rendered":"https:\/\/daxuns.com\/?p=17064"},"modified":"2025-06-05T16:12:23","modified_gmt":"2025-06-05T08:12:23","slug":"what-you-need-to-know-about-grade-3-titanium","status":"publish","type":"post","link":"https:\/\/daxuns.com\/ru\/what-you-need-to-know-about-grade-3-titanium\/","title":{"rendered":"\u0427\u0442\u043e \u043d\u0443\u0436\u043d\u043e \u0437\u043d\u0430\u0442\u044c \u043e \u0442\u0438\u0442\u0430\u043d\u0435 \u043a\u043b\u0430\u0441\u0441\u0430 3"},"content":{"rendered":"<p>\u0422\u0438\u0442\u0430\u043d \u043c\u0430\u0440\u043a\u0438 CP 3 \u044f\u0432\u043b\u044f\u0435\u0442\u0441\u044f \u0445\u043e\u0440\u043e\u0448\u0438\u043c \u0432\u044b\u0431\u043e\u0440\u043e\u043c \u0434\u043b\u044f \u043c\u043d\u043e\u0433\u0438\u0445 \u043e\u0442\u0440\u0430\u0441\u043b\u0435\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438, \u043d\u043e \u043c\u043d\u043e\u0433\u043e \u043b\u0438 \u0432\u044b \u0437\u043d\u0430\u0435\u0442\u0435 \u043e \u043d\u0435\u043c? \u042d\u0442\u0430 \u0441\u0442\u0430\u0442\u044c\u044f \u0440\u0430\u0441\u0441\u043a\u0430\u0436\u0435\u0442 \u0432\u0430\u043c \u043e \u043d\u0435\u043a\u043e\u0442\u043e\u0440\u044b\u0445 \u0437\u043d\u0430\u043d\u0438\u044f\u0445, \u043a\u043e\u0442\u043e\u0440\u044b\u0435 \u0432\u044b \u0434\u043e\u043b\u0436\u043d\u044b \u0437\u043d\u0430\u0442\u044c \u043e \u0442\u0438\u0442\u0430\u043d\u0435 \u043c\u0430\u0440\u043a\u0438 3, \u0447\u0442\u043e\u0431\u044b \u043f\u043e\u043c\u043e\u0447\u044c \u0432\u0430\u043c \u043b\u0443\u0447\u0448\u0435 \u0432\u044b\u0431\u0440\u0430\u0442\u044c \u043f\u0440\u0430\u0432\u0438\u043b\u044c\u043d\u044b\u0439 \u0441\u043e\u0440\u0442 \u0442\u0438\u0442\u0430\u043d\u0430.<\/p>\n<h3><span style=\"color: #3366ff;\">\u041e\u0441\u043d\u043e\u0432\u043d\u043e\u0435 \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u0438\u0435<\/span><\/h3>\n<p>\u0422\u0438\u0442\u0430\u043d 3-\u0433\u043e \u043a\u043b\u0430\u0441\u0441\u0430 (\u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u044b\u0439 \u0447\u0438\u0441\u0442\u044b\u0439 \u0442\u0438\u0442\u0430\u043d 3-\u0433\u043e \u043a\u043b\u0430\u0441\u0441\u0430) - \u044d\u0442\u043e \u043c\u0435\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u0438\u0439 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b \u043d\u0430 \u043e\u0441\u043d\u043e\u0432\u0435 \u0442\u0438\u0442\u0430\u043d\u0430 \u0441 \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u0438\u0435\u043c \u043c\u0438\u043a\u0440\u043e\u043f\u0440\u0438\u043c\u0435\u0441\u0435\u0439 (\u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u0436\u0435\u043b\u0435\u0437\u043e, \u043a\u0438\u0441\u043b\u043e\u0440\u043e\u0434, \u0443\u0433\u043b\u0435\u0440\u043e\u0434 \u0438 \u0442.\u0434.). \u0421\u043e\u0433\u043b\u0430\u0441\u043d\u043e \u0441\u0442\u0430\u043d\u0434\u0430\u0440\u0442\u0443 ASTM \u0421\u0428\u0410, \u043e\u043d \u043e\u0442\u043d\u043e\u0441\u0438\u0442\u0441\u044f \u043a \u0442\u0440\u0435\u0442\u044c\u0435\u043c\u0443 \u0443\u0440\u043e\u0432\u043d\u044e \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0433\u043e \u0447\u0438\u0441\u0442\u043e\u0433\u043e \u0442\u0438\u0442\u0430\u043d\u0430 (CP Titanium), \u0441 \u0447\u0438\u0441\u0442\u043e\u0442\u043e\u0439 \u043e\u043a\u043e\u043b\u043e 99,5% \u0438 \u043e\u0431\u0449\u0438\u043c \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435\u043c \u043f\u0440\u0438\u043c\u0435\u0441\u0435\u0439 \u043c\u0435\u043d\u0435\u0435 0,5%. \u041f\u043e \u0441\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u044e \u0441 1 \u0438 2 \u043a\u043b\u0430\u0441\u0441\u0430\u043c\u0438, 3 \u043a\u043b\u0430\u0441\u0441 \u043e\u0431\u043b\u0430\u0434\u0430\u0435\u0442 \u0431\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c\u044e \u0438 \u043e\u0442\u043d\u043e\u0441\u0438\u0442\u0441\u044f \u043a \u043a\u0430\u0442\u0435\u0433\u043e\u0440\u0438\u0438 \u0441 \u043b\u0443\u0447\u0448\u0438\u043c\u0438 \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u043c\u0438 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430\u043c\u0438 \u0441\u0440\u0435\u0434\u0438 \u0447\u0438\u0441\u0442\u043e\u0433\u043e \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0433\u043e \u0442\u0438\u0442\u0430\u043d\u0430.<\/p>\n<h3><span style=\"color: #3366ff;\">\u041e\u0441\u043d\u043e\u0432\u043d\u044b\u0435 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a\u0438<\/span><\/h3>\n<p>1. \u0411\u0430\u043b\u0430\u043d\u0441 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u0438 \u0445\u043e\u0440\u043e\u0448\u0435\u0439 \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u0438<br \/>\n\u041f\u0440\u0435\u0434\u0435\u043b \u0442\u0435\u043a\u0443\u0447\u0435\u0441\u0442\u0438 (\u043e\u043a\u043e\u043b\u043e 250-350 \u041c\u041f\u0430) \u0438 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043d\u0430 \u0440\u0430\u0441\u0442\u044f\u0436\u0435\u043d\u0438\u0435 (\u043e\u043a\u043e\u043b\u043e 450-550 \u041c\u041f\u0430) \u0442\u0438\u0442\u0430\u043d\u0430 Grade 3 \u0437\u043d\u0430\u0447\u0438\u0442\u0435\u043b\u044c\u043d\u043e \u0432\u044b\u0448\u0435, \u0447\u0435\u043c \u0443 Grade 1 \u0438 Grade 2 (\u043e\u0431\u0430 \u0438\u043c\u0435\u044e\u0442 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043e\u043a\u043e\u043b\u043e 200-400 \u041c\u041f\u0430), \u0447\u0442\u043e \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u0441\u0446\u0435\u043d\u0430\u0440\u0438\u0435\u0432, \u0442\u0440\u0435\u0431\u0443\u044e\u0449\u0438\u0445 \u0431\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043d\u0435\u0441\u0443\u0449\u0435\u0439 \u0441\u043f\u043e\u0441\u043e\u0431\u043d\u043e\u0441\u0442\u0438 \u043f\u0440\u0438 \u0441\u043e\u0445\u0440\u0430\u043d\u0435\u043d\u0438\u0438 \u0445\u043e\u0440\u043e\u0448\u0435\u0439 \u0443\u0434\u0430\u0440\u043d\u043e\u0439 \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u0438.<\/p>\n<p>2. \u0423\u043c\u0435\u0440\u0435\u043d\u043d\u0430\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c<br \/>\n\u0418\u0437-\u0437\u0430 \u0432\u044b\u0441\u043e\u043a\u043e\u0433\u043e \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u044f \u043a\u0438\u0441\u043b\u043e\u0440\u043e\u0434\u0430 (\u043e\u0431\u044b\u0447\u043d\u043e \u22640,35%) \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u043a \u043a\u0438\u0441\u043b\u043e\u0442\u0430\u043c, \u0449\u0435\u043b\u043e\u0447\u0430\u043c \u0438 \u043c\u043e\u0440\u0441\u043a\u043e\u0439 \u0432\u043e\u0434\u0435 \u043d\u0435\u0441\u043a\u043e\u043b\u044c\u043a\u043e \u043d\u0438\u0436\u0435, \u0447\u0435\u043c \u0443 Grade 1 \u0438 Grade 2, \u043d\u043e \u043e\u043d\u0430 \u043f\u043e-\u043f\u0440\u0435\u0436\u043d\u0435\u043c\u0443 \u043d\u0430\u0434\u0435\u0436\u043d\u0430 \u0432 \u0431\u043e\u043b\u044c\u0448\u0438\u043d\u0441\u0442\u0432\u0435 \u043c\u044f\u0433\u043a\u0438\u0445 \u0441\u0440\u0435\u0434, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u0441\u0446\u0435\u043d\u0430\u0440\u0438\u0435\u0432 \u0443\u043c\u0435\u0440\u0435\u043d\u043d\u043e\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0441\u043e \u0441\u0442\u0440\u043e\u0433\u0438\u043c\u0438 \u0442\u0440\u0435\u0431\u043e\u0432\u0430\u043d\u0438\u044f\u043c\u0438 \u043a \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438.<\/p>\n<p>3. \u041f\u0440\u043e\u0441\u0442\u043e\u0442\u0430 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438<br \/>\n\u041e\u043d \u043c\u043e\u0436\u0435\u0442 \u0431\u044b\u0442\u044c \u0441\u0444\u043e\u0440\u043c\u0438\u0440\u043e\u0432\u0430\u043d \u0441 \u043f\u043e\u043c\u043e\u0449\u044c\u044e \u043e\u0431\u044b\u0447\u043d\u044b\u0445 \u043f\u0440\u043e\u0446\u0435\u0441\u0441\u043e\u0432 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438 \u043c\u0435\u0442\u0430\u043b\u043b\u0430 (\u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u043a\u043e\u0432\u043a\u0430, \u0448\u0442\u0430\u043c\u043f\u043e\u0432\u043a\u0430, \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430), \u0430 \u044d\u0444\u0444\u0435\u043a\u0442 \u0442\u0435\u0440\u043c\u043e\u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438 \u043e\u0433\u0440\u0430\u043d\u0438\u0447\u0435\u043d. \u041e\u0431\u044b\u0447\u043d\u043e \u043e\u043d \u0443\u043f\u0440\u043e\u0447\u043d\u044f\u0435\u0442\u0441\u044f \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u043e\u0439.<br \/>\n4. \u0412\u044b\u0441\u043e\u043a\u0430\u044f \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430 \u043f\u043b\u0430\u0432\u043b\u0435\u043d\u0438\u044f \u0438 \u043d\u0438\u0437\u043a\u0430\u044f \u0442\u0435\u043f\u043b\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u043d\u043e\u0441\u0442\u044c<br \/>\n\u0422\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430 \u043f\u043b\u0430\u0432\u043b\u0435\u043d\u0438\u044f \u0441\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0435\u0442 \u043e\u043a\u043e\u043b\u043e 1660\u2103, \u0430 \u0442\u0435\u043f\u043b\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u043d\u043e\u0441\u0442\u044c - \u043e\u043a\u043e\u043b\u043e 17 \u0412\u0442\/(\u043c-\u041a), \u0447\u0442\u043e \u043d\u0438\u0436\u0435, \u0447\u0435\u043c \u0443 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438 (\u043e\u043a\u043e\u043b\u043e 15-50 \u0412\u0442\/(\u043c-\u041a)). \u0421\u043b\u0435\u0434\u0443\u0435\u0442 \u043e\u0431\u0440\u0430\u0442\u0438\u0442\u044c \u0432\u043d\u0438\u043c\u0430\u043d\u0438\u0435 \u043d\u0430 \u043a\u043e\u043d\u0442\u0440\u043e\u043b\u044c \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u044b \u0432\u043e \u0432\u0440\u0435\u043c\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438.<\/p>\n<h3><span style=\"color: #3366ff;\">\u0422\u0438\u043f\u0438\u0447\u043d\u044b\u0435 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f<\/span><\/h3>\n<p><strong>1. \u0410\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/strong><br \/>\n\u041d\u0430 \u043f\u0435\u0440\u0432\u044b\u0445 \u043f\u043e\u0440\u0430\u0445 \u043e\u043d \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043b\u0441\u044f \u0434\u043b\u044f \u0438\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0442\u0438\u0432\u043d\u044b\u0445 \u0434\u0435\u0442\u0430\u043b\u0435\u0439 \u0441\u0430\u043c\u043e\u043b\u0435\u0442\u043e\u0432 (\u043d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, \u043a\u0440\u043e\u043d\u0448\u0442\u0435\u0439\u043d\u043e\u0432 \u0438 \u0441\u043e\u0435\u0434\u0438\u043d\u0438\u0442\u0435\u043b\u0435\u0439). \u041f\u043e\u0437\u0436\u0435, \u0432 \u0441\u0432\u044f\u0437\u0438 \u0441 \u043f\u043e\u043f\u0443\u043b\u044f\u0440\u043d\u043e\u0441\u0442\u044c\u044e \u0431\u043e\u043b\u0435\u0435 \u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0445 \u0442\u0438\u0442\u0430\u043d\u043e\u0432\u044b\u0445 \u0441\u043f\u043b\u0430\u0432\u043e\u0432, \u0435\u0433\u043e \u043f\u043e\u0441\u0442\u0435\u043f\u0435\u043d\u043d\u043e \u0441\u0442\u0430\u043b\u0438 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u0442\u044c \u0434\u043b\u044f \u0434\u0435\u0442\u0430\u043b\u0435\u0439 \u0441 \u0447\u0443\u0442\u044c \u0431\u043e\u043b\u0435\u0435 \u043d\u0438\u0437\u043a\u0438\u043c\u0438 \u0442\u0440\u0435\u0431\u043e\u0432\u0430\u043d\u0438\u044f\u043c\u0438 \u043a \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0438\u0442\u0435\u043b\u044c\u043d\u043e\u0441\u0442\u0438, \u043d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, \u0434\u043b\u044f \u043a\u043e\u0440\u043f\u0443\u0441\u043e\u0432 \u043d\u0435\u043a\u043e\u0442\u043e\u0440\u044b\u0445 \u0433\u0438\u0434\u0440\u0430\u0432\u043b\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u0441\u0438\u0441\u0442\u0435\u043c.<\/p>\n<p><strong>2. \u041c\u0435\u0434\u0438\u0446\u0438\u043d\u0441\u043a\u0430\u044f \u0441\u0444\u0435\u0440\u0430<\/strong><br \/>\n\u0418\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0434\u043b\u044f \u0438\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u0438\u043c\u043f\u043b\u0430\u043d\u0442\u0430\u0442\u043e\u0432, \u043d\u0435 \u043d\u0435\u0441\u0443\u0449\u0438\u0445 \u043d\u0430\u0433\u0440\u0443\u0437\u043a\u0438 (\u043d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, \u043e\u0441\u043d\u043e\u0432\u0430\u043d\u0438\u0439 \u0437\u0443\u0431\u043d\u044b\u0445 \u0438\u043c\u043f\u043b\u0430\u043d\u0442\u0430\u0442\u043e\u0432 \u0438 \u0445\u0438\u0440\u0443\u0440\u0433\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432). \u0425\u043e\u0442\u044f \u0435\u0433\u043e \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0432\u044b\u0448\u0435, \u0447\u0435\u043c \u0443 \u0447\u0438\u0441\u0442\u043e\u0433\u043e \u0442\u0438\u0442\u0430\u043d\u0430, \u0435\u0433\u043e \u0431\u0438\u043e\u0441\u043e\u0432\u043c\u0435\u0441\u0442\u0438\u043c\u043e\u0441\u0442\u044c \u043d\u0435 \u0431\u044b\u043b\u0430 \u0437\u043d\u0430\u0447\u0438\u0442\u0435\u043b\u044c\u043d\u043e \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u0430. \u0412 \u043d\u0430\u0441\u0442\u043e\u044f\u0449\u0435\u0435 \u0432\u0440\u0435\u043c\u044f \u0432 \u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0435 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u0445 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u043e\u0432 \u0434\u043b\u044f \u0438\u043c\u043f\u043b\u0430\u043d\u0442\u0430\u0442\u043e\u0432 \u0447\u0430\u0449\u0435 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u044e\u0442\u0441\u044f \u0442\u0438\u0442\u0430\u043d\u043e\u0432\u044b\u0435 \u0441\u043f\u043b\u0430\u0432\u044b (\u043d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, Ti-6Al-4V).<\/p>\n<p><strong>3. \u0425\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435<\/strong><br \/>\n\u0424\u0443\u0442\u0435\u0440\u043e\u0432\u043a\u0438 \u0438 \u0441\u043e\u0435\u0434\u0438\u043d\u0438\u0442\u0435\u043b\u044c\u043d\u044b\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b \u0442\u0440\u0443\u0431 \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u0440\u0435\u0430\u043a\u0442\u043e\u0440\u043e\u0432, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u0443\u043c\u0435\u0440\u0435\u043d\u043d\u043e \u0430\u0433\u0440\u0435\u0441\u0441\u0438\u0432\u043d\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445, \u0433\u0434\u0435 \u0442\u0440\u0435\u0431\u0443\u0435\u0442\u0441\u044f \u0431\u0430\u043b\u0430\u043d\u0441 \u043c\u0435\u0436\u0434\u0443 \u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c\u044e \u0438 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c\u044e, \u043a\u043b\u0430\u0441\u0441 3 \u044f\u0432\u043b\u044f\u0435\u0442\u0441\u044f \u044d\u043a\u043e\u043d\u043e\u043c\u0438\u0447\u043d\u044b\u043c \u0432\u044b\u0431\u043e\u0440\u043e\u043c.<\/p>\n<p><strong>4. \u0410\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/strong><br \/>\n\u0412\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u0445\u043d\u043e\u043b\u043e\u0433\u0438\u0447\u043d\u044b\u0435 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0445 \u0432\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0445 \u0441\u0438\u0441\u0442\u0435\u043c, \u043e\u0431\u043b\u0430\u0434\u0430\u044e\u0449\u0438\u0435 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e \u0438 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e, \u043d\u043e \u043c\u0430\u0441\u0448\u0442\u0430\u0431\u043d\u043e\u0435 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0435 \u043e\u0433\u0440\u0430\u043d\u0438\u0447\u0435\u043d\u043e (\u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c \u0432\u044b\u0448\u0435, \u0447\u0435\u043c \u0443 \u043e\u0431\u044b\u0447\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438).<\/p>\n<h3><span style=\"color: #3366ff;\">\u041c\u0435\u0440\u044b \u043f\u0440\u0435\u0434\u043e\u0441\u0442\u043e\u0440\u043e\u0436\u043d\u043e\u0441\u0442\u0438 \u043f\u0440\u0438 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0435 \u0438 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u0438<\/span><\/h3>\n<p><strong>1. \u0425\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a\u0438 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438<\/strong><br \/>\n&#8211; Cold processing is easy to harden, and it needs to be carried out in stages and interspersed with annealing treatment (annealing temperature is about 700-800\u2103);<br \/>\n&#8211; Welding requires inert gas protection (such as argon) to avoid oxidation and performance degradation.<\/p>\n<p><strong>2. \u0417\u0430\u0449\u0438\u0442\u0430 \u043e\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438<\/strong><br \/>\n&#8211; Performance is limited in strong acid (such as hydrochloric acid, sulfuric acid) or high-temperature chloride environments. It is recommended to apply anti-corrosion coating or use titanium alloy instead;<br \/>\n&#8211; Long-term exposure to seawater environment may cause local pitting corrosion, which requires regular inspection.<\/p>\n<p><strong>3. \u041a\u043e\u043d\u0442\u0440\u043e\u043b\u044c \u0437\u0430\u0442\u0440\u0430\u0442<\/strong><br \/>\n\u0426\u0435\u043d\u0430 \u043d\u0430\u0445\u043e\u0434\u0438\u0442\u0441\u044f \u043c\u0435\u0436\u0434\u0443 \u0447\u0438\u0441\u0442\u044b\u043c \u0442\u0438\u0442\u0430\u043d\u043e\u043c \u0438 \u0442\u0438\u0442\u0430\u043d\u043e\u0432\u044b\u043c \u0441\u043f\u043b\u0430\u0432\u043e\u043c, \u043f\u0440\u0438\u043c\u0435\u0440\u043d\u043e \u0432 1,2-1,5 \u0440\u0430\u0437\u0430 \u0432\u044b\u0448\u0435, \u0447\u0435\u043c \u0443 Grade 2, \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439, \u0433\u0434\u0435 \u0432\u0430\u0436\u043d\u0430 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u043d\u043e \u0431\u044e\u0434\u0436\u0435\u0442 \u043e\u0433\u0440\u0430\u043d\u0438\u0447\u0435\u043d.<\/p>\n<h3><span style=\"color: #3366ff;\">\u0421\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u0435 \u0441 \u0434\u0440\u0443\u0433\u0438\u043c\u0438 \u043c\u0430\u0440\u043a\u0430\u043c\u0438 \u0442\u0438\u0442\u0430\u043d\u0430 CP<\/span><\/h3>\n<table style=\"border-collapse: collapse; width: 691px; height: 281px;\" border=\"0\" width=\"445\" cellspacing=\"0\" cellpadding=\"0\">\n<tbody>\n<tr style=\"height: 13.50pt;\">\n<td style=\"height: 13.50pt; width: 109.50pt;\" width=\"146\" height=\"18\">\u041d\u0435\u0434\u0432\u0438\u0436\u0438\u043c\u043e\u0441\u0442\u044c<\/td>\n<td style=\"width: 62.25pt;\" width=\"83\">1 \u043a\u043b\u0430\u0441\u0441<\/td>\n<td style=\"width: 54.00pt;\" width=\"72\">2 \u043a\u043b\u0430\u0441\u0441<\/td>\n<td style=\"width: 54.00pt;\" width=\"72\">3 \u043a\u043b\u0430\u0441\u0441<\/td>\n<td style=\"width: 54.00pt;\" width=\"72\">4 \u043a\u043b\u0430\u0441\u0441<\/td>\n<\/tr>\n<tr style=\"height: 13.50pt;\">\n<td style=\"height: 13.50pt;\" height=\"18\">\u041f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043d\u0430 \u0440\u0430\u0437\u0440\u044b\u0432<\/td>\n<td>400 \u041c\u041f\u0430<\/td>\n<td>500 \u041c\u041f\u0430<\/td>\n<td>550 \u041c\u041f\u0430<\/td>\n<td>700 \u041c\u041f\u0430<\/td>\n<\/tr>\n<tr style=\"height: 13.50pt;\">\n<td style=\"height: 13.50pt;\" height=\"18\">\u041f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c<\/td>\n<td>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e<\/td>\n<td>\u0425\u043e\u0440\u043e\u0448\u043e<\/td>\n<td>\u0421\u0440\u0435\u0434\u043d\u0438\u0439<\/td>\n<td>\u0411\u0435\u0434\u043d\u044b\u0439<\/td>\n<\/tr>\n<tr style=\"height: 13.50pt;\">\n<td style=\"height: 13.50pt;\" height=\"18\">\u0423\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438<\/td>\n<td>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e<\/td>\n<td>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e<\/td>\n<td>\u0423\u043c\u0435\u0440\u0435\u043d\u043d\u044b\u0439<\/td>\n<td>\u0423\u043c\u0435\u0440\u0435\u043d\u043d\u044b\u0439<\/td>\n<\/tr>\n<tr style=\"height: 13.50pt;\">\n<td style=\"height: 13.50pt;\" height=\"18\">\u0421\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c<\/td>\n<td>\u0421\u0430\u043c\u044b\u0439 \u043d\u0438\u0437\u043a\u0438\u0439<\/td>\n<td>\u0421\u0440\u0435\u0434\u043d\u0438\u0439<\/td>\n<td>\u0412\u044b\u0448\u0435<\/td>\n<td>\u0421\u0430\u043c\u044b\u0439 \u0432\u044b\u0441\u043e\u043a\u0438\u0439<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3><span style=\"color: #3366ff;\">\u0420\u0435\u0437\u044e\u043c\u0435<\/span><\/h3>\n<p>Grade 3 titanium is still an important material in some industrial fields due to its characteristics of &#8220;upgraded strength and moderate cost&#8221;. However, with the development of titanium alloy technology, its share in high-demand scenarios (such as aerospace load-bearing parts and medical implants) has gradually decreased, and it has turned to focus on specific market segments &#8211; such as parts that need to balance strength and medium corrosion protection, or mid-range applications that are more sensitive to cost. When choosing Grade 3, it is necessary to give priority to evaluating the actual needs of specific working conditions for strength and corrosion resistance, avoiding cost waste caused by over-design, and preventing hidden dangers caused by insufficient performance.<\/p>\n<p><em><strong>Daxun Alloy Co., Ltd.<\/strong> \u043f\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0435\u0442 \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0435 \u0441\u043e\u0440\u0442\u0430 \u043c\u0435\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u043e\u0433\u043e \u0442\u0438\u0442\u0430\u043d\u0430 \u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u0442\u0435\u043b\u044f\u043c \u043f\u043e \u0432\u0441\u0435\u043c\u0443 \u043c\u0438\u0440\u0443. \u041e\u043d \u043e\u0442\u043b\u0438\u0447\u0430\u0435\u0442\u0441\u044f \u0445\u043e\u0440\u043e\u0448\u0438\u043c \u043a\u0430\u0447\u0435\u0441\u0442\u0432\u043e\u043c \u0438 \u043d\u0438\u0437\u043a\u043e\u0439 \u0446\u0435\u043d\u043e\u0439, \u0430 \u0442\u0430\u043a\u0436\u0435 \u0432\u044b\u0441\u043e\u043a\u0438\u043c \u043f\u0440\u043e\u0446\u0435\u043d\u0442\u043e\u043c \u0432\u043e\u0437\u0432\u0440\u0430\u0442\u0430 \u043a\u043b\u0438\u0435\u043d\u0442\u043e\u0432. \u0415\u0441\u043b\u0438 \u0432\u0430\u0448 \u043f\u0440\u043e\u0435\u043a\u0442 \u0442\u0440\u0435\u0431\u0443\u0435\u0442 \u043f\u043e\u0434\u0434\u0435\u0440\u0436\u043a\u0438 \u0442\u0438\u0442\u0430\u043d\u043e\u0432\u043e\u0433\u043e \u043c\u0435\u0442\u0430\u043b\u043b\u0430, Daxun Alloy \u0431\u0443\u0434\u0435\u0442 \u0432\u0430\u0448\u0438\u043c \u043b\u0443\u0447\u0448\u0438\u043c \u0432\u044b\u0431\u043e\u0440\u043e\u043c. <a href=\"https:\/\/daxuns.com\/ru\/contact-us\/\" target=\"_blank\" rel=\"noopener\">\u0421\u0432\u044f\u0436\u0438\u0442\u0435\u0441\u044c \u0441 \u043d\u0430\u043c\u0438<\/a> \u0441\u0435\u0439\u0447\u0430\u0441 \u0438 \u043f\u043e\u0437\u0432\u043e\u043b\u044c\u0442\u0435 \u043d\u0430\u043c \u043f\u0440\u0435\u0434\u043e\u0441\u0442\u0430\u0432\u0438\u0442\u044c \u0432\u0430\u043c \u043b\u0443\u0447\u0448\u0438\u0439 \u0441\u0435\u0440\u0432\u0438\u0441 \u043f\u0440\u043e\u0434\u0430\u0436.<\/em><\/p>","protected":false},"excerpt":{"rendered":"<p>CP grade 3 titanium is a good choice for many industries, so how much do you know about it? This article tells you some knowledge you must know about grade 3 titanium to help you better choose the right titanium grade. Basic definition Grade 3 titanium (industrial pure titanium Grade [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"default","adv-header-id-meta":"","stick-header-meta":"default","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[1],"tags":[],"class_list":["post-17064","post","type-post","status-publish","format-standard","hentry","category-blog"],"acf":[],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v28.7 - https:\/\/yoast.com\/product\/yoast-seo-wordpress\/ -->\n<title>What You Need to Know About Grade 3 Titanium - Daxun Alloy Alloy<\/title>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/daxuns.com\/ru\/what-you-need-to-know-about-grade-3-titanium\/\" \/>\n<meta property=\"og:locale\" content=\"ru_RU\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"What You Need to Know About Grade 3 Titanium - Daxun Alloy Alloy\" \/>\n<meta property=\"og:description\" content=\"CP grade 3 titanium is a good choice for many industries, so how much do you know about it? This article tells you some knowledge you must know about grade 3 titanium to help you better choose the right titanium grade. Basic definition Grade 3 titanium (industrial pure titanium Grade [&hellip;]\" \/>\n<meta property=\"og:url\" content=\"https:\/\/daxuns.com\/ru\/what-you-need-to-know-about-grade-3-titanium\/\" \/>\n<meta property=\"og:site_name\" content=\"Daxun Alloy\" \/>\n<meta property=\"article:published_time\" content=\"2025-06-05T08:12:23+00:00\" \/>\n<meta name=\"author\" content=\"\u5927\u62a5\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"\u041d\u0430\u043f\u0438\u0441\u0430\u043d\u043e \u0430\u0432\u0442\u043e\u0440\u043e\u043c\" \/>\n\t<meta name=\"twitter:data1\" content=\"\u5927\u62a5\" \/>\n\t<meta name=\"twitter:label2\" content=\"\u041f\u0440\u0438\u043c\u0435\u0440\u043d\u043e\u0435 \u0432\u0440\u0435\u043c\u044f \u0434\u043b\u044f \u0447\u0442\u0435\u043d\u0438\u044f\" \/>\n\t<meta name=\"twitter:data2\" content=\"4 \u043c\u0438\u043d\u0443\u0442\u044b\" \/>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"What You Need to Know About Grade 3 Titanium - Daxun Alloy Alloy","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/daxuns.com\/ru\/what-you-need-to-know-about-grade-3-titanium\/","og_locale":"ru_RU","og_type":"article","og_title":"What You Need to Know About Grade 3 Titanium - Daxun Alloy Alloy","og_description":"CP grade 3 titanium is a good choice for many industries, so how much do you know about it? This article tells you some knowledge you must know about grade 3 titanium to help you better choose the right titanium grade. Basic definition Grade 3 titanium (industrial pure titanium Grade [&hellip;]","og_url":"https:\/\/daxuns.com\/ru\/what-you-need-to-know-about-grade-3-titanium\/","og_site_name":"Daxun Alloy","article_published_time":"2025-06-05T08:12:23+00:00","author":"\u5927\u62a5","twitter_card":"summary_large_image","twitter_misc":{"\u041d\u0430\u043f\u0438\u0441\u0430\u043d\u043e \u0430\u0432\u0442\u043e\u0440\u043e\u043c":"\u5927\u62a5","\u041f\u0440\u0438\u043c\u0435\u0440\u043d\u043e\u0435 \u0432\u0440\u0435\u043c\u044f \u0434\u043b\u044f \u0447\u0442\u0435\u043d\u0438\u044f":"4 \u043c\u0438\u043d\u0443\u0442\u044b"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/#article","isPartOf":{"@id":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/"},"author":{"name":"\u5927\u62a5","@id":"https:\/\/daxuns.com\/#\/schema\/person\/de54877afc2565a9ca1fbbfc7f40eeab"},"headline":"What You Need to Know About Grade 3 Titanium","datePublished":"2025-06-05T08:12:23+00:00","mainEntityOfPage":{"@id":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/"},"wordCount":768,"publisher":{"@id":"https:\/\/daxuns.com\/#organization"},"articleSection":["Blog"],"inLanguage":"ru-RU"},{"@type":"WebPage","@id":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/","url":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/","name":"What You Need to Know About Grade 3 Titanium - Daxun Alloy Alloy","isPartOf":{"@id":"https:\/\/daxuns.com\/#website"},"datePublished":"2025-06-05T08:12:23+00:00","breadcrumb":{"@id":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/#breadcrumb"},"inLanguage":"ru-RU","potentialAction":[{"@type":"ReadAction","target":["https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/daxuns.com\/what-you-need-to-know-about-grade-3-titanium\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/daxuns.com\/"},{"@type":"ListItem","position":2,"name":"What You Need to Know About Grade 3 Titanium"}]},{"@type":"WebSite","@id":"https:\/\/daxuns.com\/#website","url":"https:\/\/daxuns.com\/","name":"Daxun Alloy, \u043f\u0440\u043e\u0444\u0435\u0441\u0441\u0438\u043e\u043d\u0430\u043b\u044c\u043d\u044b\u0439 \u043f\u043e\u0441\u0442\u0430\u0432\u0449\u0438\u043a \u043c\u0435\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u043e\u0432.","description":"Titanium, Stainless Steel &amp; Nickel Alloy Supplier","publisher":{"@id":"https:\/\/daxuns.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/daxuns.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ru-RU"},{"@type":"Organization","@id":"https:\/\/daxuns.com\/#organization","name":"Daxun Alloy, \u043f\u0440\u043e\u0444\u0435\u0441\u0441\u0438\u043e\u043d\u0430\u043b\u044c\u043d\u044b\u0439 \u043f\u043e\u0441\u0442\u0430\u0432\u0449\u0438\u043a \u043c\u0435\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u043e\u0432.","url":"https:\/\/daxuns.com\/","logo":{"@type":"ImageObject","inLanguage":"ru-RU","@id":"https:\/\/daxuns.com\/#\/schema\/logo\/image\/","url":"https:\/\/daxuns.com\/wp-content\/uploads\/2026\/05\/cropped-\u9875\u7709-\u84dd\u8272-1.png","contentUrl":"https:\/\/daxuns.com\/wp-content\/uploads\/2026\/05\/cropped-\u9875\u7709-\u84dd\u8272-1.png","width":500,"height":104,"caption":"Daxun Alloy, a professional supplier of metal materials."},"image":{"@id":"https:\/\/daxuns.com\/#\/schema\/logo\/image\/"}},{"@type":"Person","@id":"https:\/\/daxuns.com\/#\/schema\/person\/de54877afc2565a9ca1fbbfc7f40eeab","name":"\u5927\u62a5","image":{"@type":"ImageObject","inLanguage":"ru-RU","@id":"https:\/\/secure.gravatar.com\/avatar\/8fed9561b22851cfe97194d727ccd325c4a6ce00dee641e4de57ee184b3e431c?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8fed9561b22851cfe97194d727ccd325c4a6ce00dee641e4de57ee184b3e431c?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8fed9561b22851cfe97194d727ccd325c4a6ce00dee641e4de57ee184b3e431c?s=96&d=mm&r=g","caption":"\u5927\u62a5"},"url":"https:\/\/daxuns.com\/ru\/author\/dp_admin\/"}]}},"_links":{"self":[{"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/posts\/17064","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/comments?post=17064"}],"version-history":[{"count":4,"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/posts\/17064\/revisions"}],"predecessor-version":[{"id":17068,"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/posts\/17064\/revisions\/17068"}],"wp:attachment":[{"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/media?parent=17064"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/categories?post=17064"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/daxuns.com\/ru\/wp-json\/wp\/v2\/tags?post=17064"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}